LM (Coating) Fiber Core Wire Rope GB6X37 FC
Please feel freely to contact with us for new price .
Product Details
6x37 is a cross laid construction used for general engineering applications. 6x37 is also available with IWRC (independent wire rope core). In the UK 6x36 is a far more popular construction, whilst on the European mainland, vast quantities of 6x37 are used for a variety of applications.。
Surface treatment:Ungalv or Galvanized
Standard:GB/T 20118-2006

Applications
General engineering applications
Crane ropes
Hoist rope
Breaking Loads
|
|
Min Breaking Loads |
Min Breaking Loads |
Min Breaking Loads | Min Breaking Loads |
Diameter | Weight |
(1770Mpa) |
(1770Mpa) |
(1960Mpa) |
(1960Mpa) |
mm | kg/m | KN | Kg | KN | Kg |
| 12 | 0.5 | 75.2 | 7669 | 83.3 | 8492 |
| 13 | 0.59 | 88.2 | 9000 | 97.7 | 9967 |
| 14 | 0.68 | 102 | 10438 | 113 | 11559 |
| 16 | 0.89 | 134 | 13634 | 148 | 15098 |
| 18 | 1.12 | 169 | 17256 | 187 | 19108 |
| 20 | 1.38 | 209 | 21303 | 231 | 23590 |
| 22 | 1.68 | 253 | 25777 | 280 | 28544 |
| 24 | 1.99 | 301 | 30677 | 333 | 33970 |
| 26 | 2.34 | 353 | 36003 | 391 | 39868 |
| 28 | 2.71 | 409 | 41755 | 453 | 46237 |
| 30 | 3.11 | 470 | 47933 | 520 | 53078 |
| 32 | 3.54 | 535 | 54537 | 592 | 60391 |
| 34 | 4 | 604 | 61567 | 668 | 68176 |
| 36 | 4.48 | 677 | 69024 | 749 | 76433 |
| 38 | 5 | 754 | 76906 | 835 | 85161 |
| 40 | 5.54 | 835 | 85214 | 925 | 94362 |
| 42 | 6.1 | 921 | 93949 | 1020 | 104034 |
| 44 | 6.7 | 1011 | 103110 | 1119 | 114178 |
| 46 | 7.32 | 1105 | 112696 | 1224 | 124794 |
| 48 | 7.97 | 1203 | 122709 | 1332 | 135881 |
General Engineering Ropes
GREENLOGY TEC(LM) specializes in supplying multiple strands of ungalvanised and galvanized steel wire ropes. Our products range from 0.5mm to 64mm, including 1X19, 7X7, 6X19, 7X19, 6X36, 8X19, 8X36, 19X7 and 35X7 with both Fibre Core and Steel Cores. In addition to these conventional steel wire ropes, we can also provide high-quality special steel wire ropes.
Most wire ropes are used in harsh conditions and must have resistance to extrusion, bending fatigue and abrasion. All of our wire ropes are guaranteed to achieve the highest level , maximizing the service life to increase the productivity of end users. We ensure that all materials are produced in accordance with the best standards in the wire rope industry. Each wire rope can be supplied with a thimble eyes, swaged ends and wedge sockets ,as well as many other assembly components.In addition, we also provide customized services, our team of engineers can manufacture wire ropes of your required specifications. All materials are certified, traceable, and comply with ISO9001 standards.
选型指导
选型时请结合工况的载荷要求、轮槽直径、运行频率与环境腐蚀条件,确认所需直径、表面处理(光面或镀锌)及绳芯类型。LM(涂层)纤维芯钢丝绳适用于通用工程、起重与吊索等场景,若需更高承载可选IWRC结构,具体规格欢迎联系我们获取详细参数与选型建议。
产品优势
LM涂层纤维芯钢丝绳采用6x37结构,柔韧性好,便于交叉铺设与穿绕,纤维芯有助于提升绳索的缓冲与弯曲性能。表面可提供光面或镀锌处理,以适应不同防锈需求,产品按GB/T 20118-2006标准生产,适合通用工程、起重机及吊索等应用。
询盘引导
如需了解LM(涂层)纤维芯钢丝绳的详细规格、断裂荷载数据、表面处理选项及供货方案,欢迎联系我们获取详细报价与技术资料。请提供所需直径、绳芯类型、表面处理与使用工况,我们将据此为您推荐合适的产品与商务条件。