LM (Coating) Compacted Wire Rope GB6x36 (14/7+7/7/1) IWRC
Request a Quote
Please feel freely to contact with us for new price .
Product Details
6x36 wire rope is available with FC (fiber core) or IWRC (independent wire rope core), and is a general-purpose flexible engineering wire rope. This wire rope offers superior breaking load capacity and good fatigue resistance, with a long service life and wide application.
Surface finish: bright or galvanized
Standard: GB/T 20118-2006

Engineering Applications
General engineering applications
Grab bucket crane ropes
Wire rope slings
Crane ropes
Slings
Winch ropes
Lifeboat ropes
Mooring ropes
Search ropes
Luffing ropes
Traction ropes
Breaking load
|
|
Minimum breaking load |
Minimum breaking load |
Minimum breaking load |
|---|---|---|---|---|
Diameter | Weight |
(1770Mpa)
|
(1960Mpa) |
(2160Mpa)
|
mm | kg/m | KN |
KN | KN |
| 12 | 0.68 | 112 | 124 | 131 |
| 13 | 0.79 | 131 | 147 | 157 |
| 14 | 0.93 | 153 | 169 | 183 |
| 15 | 1.06 | 176 | 194 | 208 |
| 16 | 1.19 | 198 | 219 | 237 |
| 18 | 1.52 | 250 | 277 | 298 |
| 19 | 1.68 | 275 | 305 | 329 |
| 20 | 1.85 | 307 | 340 | 368 |
| 22 | 2.26 | 370 | 410 | 441 |
| 24 | 2.74 | 447 | 492 | 540 |
| 25 | 2.93 | 481 | 532 | 576 |
| 26 | 3.14 | 520 | 581 | 622 |
| 28 | 3.68 | 604 | 663 | 722 |
| 30 | 4.21 | 689 | 763 | 831 |
| 32 | 4.75 | 777 | 861 | 949 |
| 34 | 5.45 | 891 | 980 | 1070 |
| 35 | 5.71 | 933 | 1033 | 1131 |
| 36 | 6.09 | 992 | 1099 | 1192 |
General-purpose engineering wire rope
Greenlogy TEC specializes in supplying multi-strand bright or galvanized wire rope. Our products range in diameter from 0.5 mm to 64 mm, including 1X19, 7X7, 6X19, 7X19, 6X36, 8X19, 8X36, 19X7 and 35X7 specifications with fiber core and steel core (IWRC). In addition to these standard wire ropes, we can also supply premium special wire ropes.
Most wire ropes operate under demanding conditions and must resist crushing, bending fatigue and wear. All our wire ropes are designed to achieve high performance levels to maximize service life and thereby improve end-user productivity. We therefore ensure that all materials are produced in accordance with wire rope industry standards. Each wire rope can be supplied with fittings such as thimbles, swaged terminals and wedge sockets, as well as many other assembly components. We also offer customization services, and our engineering team can manufacture wire ropes to your required specifications. All materials are certified, traceable and compliant with ISO9001.。
Selection Guide
This product is an LM (plastic-coated) compacted strand wire rope with GB6x36 (14/7+7/7/1) IWRC construction. The compacted strand process makes the outer strands fit more tightly against the rope core, making it suitable for general lifting, sling and traction scenarios that require a combination of flexibility and wear resistance. During selection, please match it according to the diameter requirements of the actual working conditions, strength grades (such as 1770/1960/2160 MPa), surface treatment (bright or galvanized) and plastic coating requirements; you are welcome to contact us for detailed specifications and quotations, and we will assist you in confirming the suitable model.
Product Advantages
This wire rope adopts a 6x36 flexible structure with an independent wire rope core (IWRC), offering good fatigue resistance and breaking load capacity. With the plastic coating (LM) treatment, the surface wear resistance is further improved, making it suitable for frequent bending and wear conditions. Compared with ordinary fiber core (FC) construction, IWRC performs more stably under pressure and extrusion resistance, making it suitable for grab cranes, winches, mooring and other scenarios; specific performance can be further discussed based on your actual usage conditions.
Inquiry Guide
If you need to know the detailed specifications, available diameter range, surface treatment options and commercial terms of LM (plastic-coated) compacted strand wire rope GB6x36 (14/7+7/7/1) IWRC, you are welcome to contact us for detailed specifications and quotations. Please provide information such as the required diameter, strength grade, plastic coating requirements and usage scenario, and we will provide you with a targeted solution and technical support as soon as possible.
Operating Environment
- Designed for general engineering applications in both indoor and outdoor environments.
- Suitable for use in humid or moist conditions, including marine and offshore settings, as part of general engineering applications.
- Can be used in industrial atmospheres where moderate corrosion may be present, such as in crane ropes and winch ropes.
- For use in applications involving exposure to abrasive or dirty environments, typical of grab bucket crane ropes and mooring ropes.