LM (Coating) Comp. Rotation Resistant Wire Rope GB35X7 (6/1)

LM (Coating) Comp. Rotation Resistant Wire Rope GB35X7 (6/1)

Engineering tool Wire rope selector

Price on request

Get a quote
Request a Quote


Please feel freely to contact with us for new price .

Product Details

35X7 (coated) compacted wire rope is available in galvanized and non-galvanized versions, and also in 32X7 and 37X7 specifications. To meet your requirements for higher breaking loads and better wear characteristics, we can apply surface treatment, lubrication, plastic coating and compaction.

Surface treatment: bright or galvanized

Standard: GB/T 20118-2006

Greenlogy TEC GB (Coated) Compacted Rotation-Resistant Wire Rope 35X7 (6/1)

Engineering Applications

  • Offshore crane wire rope

  • Deck crane wire rope

  • Column crane wire rope

  • Lifting slings

  • Main hoist wire rope

  • Slings

Breaking load

Minimum breaking load

Minimum breaking load

Minimum breaking load

Minimum breaking load


Diameter

Weight

(1770Mpa)

(1770Mpa)

(1960Mpa)

(1960Mpa)

mm

kg/m

KN

Kg

KN

Kg

120.71151169912712961
130.821351373014915212
140.951561592417317642
151.091791828019920252
161.242042079822623043
181.572582632328629163
201.943193249735336004
222.353863932242743565
242.794594679650851846
263.285385492159760847
283.86246369569270568
304.377177311979481009

General engineering wire rope

   Greenlogy TEC (LM) specializes in supplying multi-strand bright or galvanized wire rope. Our products range in diameter from 0.5mm to 64mm, including 1X19, 7X7, 6X19, 7X19, 6X36, 8X19, 8X36, 19X7 and 35X7 specifications with fiber core and steel core. In addition to these conventional wire ropes, we can also supply high-quality special wire ropes.

Most wire ropes work under demanding conditions and must be resistant to crushing, bending fatigue and wear. All our wire ropes are designed to achieve a high performance level to extend service life and thereby improve end-user productivity. We therefore ensure that all materials are produced according to wire rope industry standards. Each wire rope can be supplied with thimble eyes, swaged ends, wedge sockets and many other assembly components. We also offer customization services; our engineering team can manufacture wire rope to your required specifications. All materials are certified, traceable and compliant with ISO9001.


Selection Guide

35X7 (coated) compacted wire rope is suitable for engineering applications such as offshore cranes, deck cranes, column cranes, lifting slings, main hoist wire rope and slings. When selecting, factors such as working load, frequency of use, environmental corrosion conditions and matching requirements of sheaves and drums should be considered comprehensively. We can supply 32X7, 37X7 and other specifications, as well as options including galvanized or non-galvanized, surface treatment, lubrication, plastic coating and compaction. Please contact us for detailed specifications and selection support.

Product Advantages

This wire rope features a compacted structure, providing a higher breaking load and good wear resistance, making it suitable for heavy-duty and frequent lifting operations. The surface can be bright or galvanized, and lubrication or plastic coating can be applied as required to enhance corrosion resistance and service life. For specific performance data, please refer to the technical parameter table or contact us for detailed information.

Inquiry Guide

For information on MOQ, pricing, delivery times, or customized solutions, please feel free to contact us. Please provide the required diameter, specifications, surface treatment requirements, and quantity, and we will provide you with a professional quotation and technical support as soon as possible.

Operating Environment

  • This 35X7 compacted rotation resistant wire rope is typically deployed in outdoor marine and industrial environments, where galvanized versions resist atmospheric moisture and non-galvanized versions are chosen for dry or lubricated service conditions.
  • Its plastic coating and compaction help seal the strand gaps and limit the ingress of water, salt spray and airborne contaminants in offshore crane, deck crane and column crane applications.
  • For lifting slings and main hoist wire rope used in humid or chemically exposed plants, the rope can be supplied with surface treatment and lubrication suited to the prevailing corrosive media as specified by the user.
  • Indoor workshop and yard duties are also common; in all cases storage and operation should follow the GB/T 20118-2006 standard conditions to maintain rope performance.