37X7 is available in both galvanised and ungalvanised finish depending upon your requirement for higher breaking load or better wear characteristics, these wire ropes are available in different finishes and lubrications as well as being available with plastic impregnated or in compacted constructions.
Surface treatment:Ungalv or Galvanized
Standard:GB/T 20118-2006

Applications
Offshore crane rope
Deck crane rope
Pillar crane rope
Whip hoist rope
Main hoist rope
Crane rope
Breaking Loads
|
|
Min Breaking Loads |
Min Breaking Loads |
Min Breaking Loads | Min Breaking Loads |
Weight | Weight |
(1770Mpa) |
(1770Mpa) |
(1960Mpa) |
(1960Mpa) |
mm | kg/m | KN | Kg | KN | Kg |
| 14 | 0.95 | 154 | 15708 | 171 | 17442 |
| 15 | 1.09 | 177 | 18054 | 196 | 19992 |
| 16 | 1.25 | 203 | 20706 | 225 | 22950 |
| 18 | 1.58 | 257 | 26214 | 285 | 29070 |
| 19 | 1.78 | 290 | 29580 | 321 | 32742 |
| 20 | 1.95 | 318 | 32436 | 352 | 35904 |
| 21 | 2.15 | 349 | 35598 | 387 | 39474 |
| 22 | 2.37 | 385 | 39270 | 426 | 43452 |
| 23 | 2.56 | 416 | 42432 | 461 | 47022 |
| 24 | 2.81 | 457 | 46601 | 506 | 51612 |
| 25 | 3.1 | 504 | 51510 | 558 | 56916 |
| 26 | 3.3 | 537 | 54774 | 595 | 60690 |
| 28 | 3.8 | 618 | 63036 | 685 | 69870 |
| 29 | 4.1 | 667 | 68034 | 738 | 75276 |
| 30 | 4.45 | 724 | 73848 | 802 | 81804 |
| 32 | 4.96 | 806 | 82212 | 892 | 90984 |
General Engineering Ropes
绿盟(LM)专门供应多股光面或镀锌钢丝绳。我们的产品直径从0.5mm到64mm不等,包括带纤维芯和钢芯的1X19、7X7、6X19、7X19、6X36、8X19、8X36、19X7和35X7各种规格。除这些常规钢丝绳外,我们还可以提供优质的特种钢丝绳。
Most wire ropes are used in harsh conditions and must have resistance to extrusion, bending fatigue and abrasion. All of our wire ropes are guaranteed to achieve the highest level , maximizing the service life to increase the productivity of end users. We ensure that all materials are produced in accordance with the best standards in the wire rope industry. Each wire rope can be supplied with a thimble eyes, swaged ends and wedge sockets ,as well as many other assembly components.In addition, we also provide customized services, our team of engineers can manufacture wire ropes of your required specifications. All materials are certified, traceable, and comply with ISO9001 standards.
选型指导
本产品为LM(涂层)压实非旋转钢丝绳,结构为GB37X7(6/1),适用于对非旋转性能和耐磨性有要求的起重与吊装场景。选型时请结合工况的额定载荷、滑轮与卷筒直径、使用频率及腐蚀环境,确认所需直径与表面处理方式(光面或镀锌)。由于本页未列出完整规格覆盖范围,欢迎联系我们获取详细规格与选型建议。
产品优势
该结构具有非旋转特性,配合涂层可改善耐磨与防腐蚀表现,并可按需求进行表面处理、润滑、包塑或压实等工艺调整。镀锌与非镀锌两种选择便于匹配不同腐蚀等级的使用环境,适用于海上起重机、甲板起重、立柱吊车、起重吊索与主提升等应用。具体性能表现随直径、结构与工艺不同而变化,欢迎联系我们获取详细技术资料与报价。
询盘引导
如需确认适配直径、表面处理方式、涂层或包塑要求,以及批量供货与交期安排,请提供您的工况参数与需求数量。欢迎联系我们获取详细规格、样品与报价,我们将根据您的应用场景提供针对性建议。
简体中文
English