LM Fiber Core(FC) Wire Rope GB7X7 (6/1)
Please feel freely to contact with us for new price .
Production Details
When supplied with a WSC(wire strand core) the rope is more commonly referred to as 7x7. 0.5mm to 2mm is most popular diameter ,and it is flexible .
Surface treatment:Galvanised or Marine Grade Stainless Steel
Standard:GB/T 20118-2006

Applications
General engineering applications
Small diameter wire rope slings
Stay wires
Fencing rope
Catenary wire
Garage door cables
Standing rigging
Hanging signs
Ski-lifts
Breaking Loads
|
|
Min Breaking Loads |
Min Breaking Loads |
Diameter | Weight |
(1770Mpa) |
(1770Mpa) |
mm | kg/m | KN | Kg |
| 1 | 0.004 | 0.76 | 78 |
| 2 | 0.015 | 2.75 | 280 |
| 3 | 0.035 | 6.18 | 630 |
| 4 | 0.06 | 11 | 1120 |
| 5 | 0.1 | 17.2 | 1751 |
| 6 | 0.14 | 24.7 | 2521 |
| 7 | 0.19 | 33.7 | 3432 |
| 8 | 0.25 | 44 | 4483 |
| 9 | 0.31 | 55.6 | 5674 |
| 10 | 0.38 | 68.7 | 7004 |
| 11 | 0.47 | 83.1 | 8475 |
| 12 | 0.55 | 98.9 | 10087 |
| 13 | 0.65 | 116 | 11838 |
| 14 | 0.75 | 135 | 13729 |
| 16 | 0.98 | 176 | 17932 |
| 18 | 1.24 | 223 | 22696 |
| 20 | 1.54 | 275 | 28019 |
| 22 | 1.86 | 332 | 33903 |
| 24 | 2.21 | 396 | 40348 |
| 26 | 2.6 | 464 | 47353 |
| 28 | 3.01 | 538 | 54918 |
| 30 | 3.46 | 618 | 63044 |
General Engineering Ropes
GREENLOGY TEC(LM) specializes in supplying multiple strands of ungalvanised and galvanized steel wire ropes. Our products range from 0.5mm to 64mm, including 1X19, 7X7, 6X19, 7X19, 6X36, 8X19, 8X36, 19X7 and 35X7 with both Fibre Core and Steel Cores. In addition to these conventional steel wire ropes, we can also provide high-quality special steel wire ropes.
Most wire ropes are used in harsh conditions and must have resistance to extrusion, bending fatigue and abrasion. All of our wire ropes are guaranteed to achieve the highest level , maximizing the service life to increase the productivity of end users. We ensure that all materials are produced in accordance with the best standards in the wire rope industry. Each wire rope can be supplied with a thimble eyes, swaged ends and wedge sockets ,as well as many other assembly components.In addition, we also provide customized services, our team of engineers can manufacture wire ropes of your required specifications. All materials are certified, traceable, and comply with ISO9001 standards.
选型指导
请根据实际使用场景确认所需绳径、绳芯结构(如7X7或6/1)、表面处理方式(镀锌钢或316不锈钢),以及是否需要按国标GB/T 20118-2006执行。若对破断荷载、柔韧性或耐腐蚀性有特定要求,欢迎联系我们说明工况,由技术人员协助匹配规格。
产品优势
该产品采用钢丝绳芯结构,直径0.5mm至2mm范围内整体柔软,便于弯曲与打结,适用于吊索、支索、击剑绳、车库门绳等多种场合。表面可选镀锌钢或316航海级不锈钢,兼顾强度与耐蚀需求,工程适应性强。
询盘引导
如需了解具体直径的重量、最小破断荷载、包装方式或供货周期,欢迎联系我们获取详细规格与报价。请提供所需绳径、材质、表面处理及订购数量,我们将尽快回复。
简体中文
English