LM Wire Rope GB 6X37 IWRC
Request a Quote
Please feel freely to contact with us for new price .
Product Details
6x37 Specifications Generally used for cross laying in engineering, also available with IWRC (Independent Wire Rope Core). 6x36 is more popular in the UK; while in continental Europe,6x37 is generally used.
Surface treatment: bright or galvanized
Standard: GB/T 20118-2006
.jpg?access_token=3cc09a22-9720-43d1-b58a-87a5548f102a)
Engineering Applications
General Engineering Wire Rope
Crane Wire Rope
Sling
Breaking Load
|
|
Minimum Breaking Load |
Minimum Breaking Load |
Minimum Breaking Load | Minimum Breaking Load |
|---|---|---|---|---|---|
Diameter | Weight |
(1770Mpa) |
(1770Mpa) |
(1960Mpa) |
(1960Mpa) |
mm | kg/m | KN | Kg | KN | Kg |
| 12 | 0.55 | 81.3 | 8293 | 90 | 9183 |
| 13 | 0.64 | 95.4 | 9733 | 106 | 10777 |
| 14 | 0.75 | 111 | 11288 | 123 | 12499 |
| 16 | 0.98 | 145 | 14743 | 160 | 16326 |
| 18 | 1.23 | 183 | 18659 | 203 | 20662 |
| 20 | 1.52 | 226 | 23036 | 250 | 25509 |
| 22 | 1.84 | 273 | 27874 | 302 | 30866 |
| 24 | 2.2 | 325 | 33173 | 360 | 36734 |
| 26 | 2.58 | 382 | 38932 | 423 | 43111 |
| 28 | 2.99 | 443 | 45152 | 490 | 49999 |
| 30 | 3.43 | 508 | 51833 | 563 | 57397 |
| 32 | 3.9 | 578 | 58974 | 640 | 65305 |
| 34 | 4.4 | 653 | 66576 | 723 | 73723 |
| 36 | 4.94 | 732 | 74639 | 810 | 82651 |
| 38 | 5.5 | 815 | 83163 | 903 | 92090 |
| 40 | 6.1 | 903 | 92147 | 1000 | 102039 |
| 42 | 6.72 | 996 | 101592 | 1103 | 112498 |
| 44 | 7.38 | 1093 | 111498 | 1211 | 123467 |
| 46 | 8.06 | 1195 | 121865 | 1323 | 134946 |
| 48 | 8.78 | 1301 | 132692 | 1441 | 146936 |
General Engineering Wire Rope
Greenlogy TEC LM specializes in supplying multi-strand bright or galvanized wire rope. Our products range in diameter from 0.5mm to 64mm, including 1X19, 7X7, 6X19, 7X19, 6X36, 8X19, 8X36, 19X7 and 35X7 specifications with fiber core and steel core. In addition to these conventional wire ropes, we can also provide premium special wire ropes.
Most wire ropes work under harsh conditions and must have resistance to crushing, bending fatigue and wear. All our wire ropes strive to achieve a high performance level to extend service life, thereby improving end-user productivity. We therefore ensure that all materials are produced in accordance with wire rope industry standards. Each wire rope can be supplied with fittings such as thimble eyes, swaged ends and wedge sockets as well as many other assembly components. In addition, we offer customization services; our engineering team can manufacture wire ropes to the specifications you require. All materials are certified, traceable and compliant with ISO9001.
Selection Guide
Please confirm the required diameter, surface treatment (bright or galvanized), core structure (such as IWRC independent wire rope core) and breaking load grade according to actual working conditions, and make your selection taking into account the regional usage habits of specifications such as 6x37 and 6x36. Different applications such as engineering cross laying, lifting and slings have different requirements for flexibility and wear resistance. You are welcome to contact us for selection advice and detailed specifications for your project.
Product Advantages
Greenlogy TEC LM Wire Rope GB 6X37 IWRC is produced to national standard GB/T 20118-2006, available in bright or galvanized surface treatment. The 6x37 structure is suitable for engineering cross laying, with optional IWRC independent wire rope core to improve structural stability. The product covers application scenarios including general engineering wire rope, crane wire rope and slings. You are welcome to contact us for detailed specifications and quotations.
Inquiry Guide
To confirm technical parameters such as diameter, surface treatment, core type and breaking load, or to obtain pricing and delivery information, please contact us. Kindly provide your application scenario and required quantity, and we will arrange a dedicated contact to supply detailed specifications and commercial terms.
Operating Environment
- LM Wire Rope GB 6X37 IWRC is suitable for general engineering applications in both indoor and outdoor environments, where the bright or galvanized surface treatment provides basic protection against atmospheric conditions.
- For outdoor or humid environments, the galvanized version offers enhanced corrosion resistance compared to the bright finish, making it appropriate for applications where moisture exposure is a concern.
- This wire rope is not intended for continuous immersion in corrosive media or for service in highly acidic or alkaline atmospheres; in such cases, additional protective measures or alternative materials should be considered.
- Typical operating temperatures for general engineering wire ropes of this construction fall within a moderate range; however, for extreme temperature applications, consult the manufacturer for specific recommendations.
Cut to Length
Need rope in fixed lengths? We cut wire rope to your required segment lengths before delivery (e.g. 5 m x 4 pcs + 10 m x 2 pcs), with end treatment per your needs. Request cut-to-length rope.