LM Wire Rope GB 6X36 FC

LM Wire Rope GB 6X36 FC

¥ 1.00 1.0 CNY

¥ 1.00

Add To Cart


Please feel freely to contact with us for new price .

 Product Details

6x36 wire rope is a flexible general engineering wire rope available with either FC (fibre core) or IWRC (independent wire rope core). The wire rope has a superior breaking load and a good fatigue life. This wire rope can be used for a wide range of applications.

Surface treatment:Ungalv, Galvanized or Marine Grade Stainless Steel.

Standard:GB/T 20118-2006

LM Wire Rope GB 6x36 FC

Applications

  • General engineering

  • Ropes for grab cranes

  • Wire rope slings

  • Crane ropes

  • Hoist rope

  • Winch ropes 


  • Lifeboat falls

  • Mooring ropes

  • Pursing wires

  • Luffing ropes

  • Tow ropes


Breaking Loads 

   Min Breaking Loads

Min Breaking Loads

   Min Breaking Loads

Min Breaking Loads


Diameter

Weight 

          (1770Mpa)

(1770Mpa)

(1960Mpa)

(1960Mpa)

mm

kg/m

KN

Kg

KN

Kg

80.2437.4381341.44222
90.347.3482552.45343
100.3758.4595764.76597
110.4470.7720978.37982
120.5384.1857993.19500
130.6298.71006810911149
140.721151167712712930
150.831311340514614844
160.941501525216616889
181.191891930321021375
191.332112150723423816
201.472342383125926389
221.782832883531331931
242.113363431737338000
262.483954027443744598
282.884584670950751723
303.35265362058259376
323.765986100866267557
344.246756887274876265
364.767577721383885501
385.38438603093495265
405.87935953251035105557
426.4710301050951141116377
447.1111311153431252127724
467.7712361260671369139600
488.4613461372681490152003

General Engineering Ropes

   GREENLOGY TEC(LM) specializes in supplying multiple strands of  ungalvanised and galvanized steel wire ropes. Our products range from 0.5mm to 64mm, including 1X19, 7X7, 6X19, 7X19, 6X36, 8X19, 8X36, 19X7 and 35X7 with both Fibre Core and Steel Cores. In addition to these conventional steel wire ropes, we can also provide high-quality special steel wire ropes.

    Most wire ropes are used in harsh conditions and must have resistance to extrusion, bending fatigue and abrasion. All of our wire ropes are guaranteed to achieve the highest level , maximizing the service life to increase the productivity of end users. We ensure that all materials are produced in accordance with the best standards in the wire rope industry. Each wire rope can be supplied with a thimble eyes, swaged ends and wedge sockets ,as well as many other assembly components.In addition, we also provide customized services, our team of engineers can manufacture wire ropes of your required specifications. All materials are certified, traceable, and comply with ISO9001 standards.


选型指导

6x36钢丝绳按国标GB/T 20118-2006生产,具柔性好、抗疲劳性能佳的特点,适合抓斗起重机、吊索、绞车及系泊等通用场景。选型时请结合所需直径、芯型(FC纤维芯或IWRC独立钢丝绳芯)、表面处理(光面、镀锌、316不锈钢)及实际断裂荷载需求综合确定。如对规格匹配有疑问,欢迎联系我们获取详细规格与报价。

产品优势

该钢丝绳结构兼顾柔韧性与承载能力,断裂荷载表现优良,使用寿命较长,适用于频繁弯曲与反复受力的工况。提供纤维芯与钢芯两种选择,并有光面、镀锌及316航海级不锈钢表面,可适应室内外、潮湿及腐蚀性环境。具体性能与配置请以实际询盘确认。

询盘引导

如您需要特定直径、芯型、表面处理或长度规格,欢迎联系我们获取详细规格与报价。我们可依据您的应用场景提供选型参考与技术支持,商业条款与交期以正式沟通为准。

Free,easy click for support

7*24 professional team support. Within 24 Hours, our team will give you the feedback.

Send   
 Website Visitor