FRP Molded Grating 38*38H30 (OFR-25)
Request a Quote
Please feel freely to contact with us for new price .
Greenlogy TEC
FRP molded grating is a panel with a certain open area, made with unsaturated polyester resin (including isophthalic, orthophthalic, phenolic and bisphenol types) as the matrix and produced in custom molds.
| Name | Content | Type |
|---|---|---|
Resin | 35% | OFR-25,IFR-25,VEFR-25 |
Glass fiber | 33% | E |
Filler | 31% | ATH,PR |
Others | 1% | --- |
Resin type
Code | Resin type | Flame retardant performance | Standard color | Recommended applications |
|---|---|---|---|---|
MP-5 | Phenolic type | Oxygen index up to about 80 | Brown | Low toxicity and high flame retardancy; applications with high fire safety requirements |
VEFR-25 | Vinyl type | Oxygen index above 28 | Grass green, yellow, gray, orange | Harsh corrosive environments such as acids and alkalis |
VEFR-10 | Vinyl type | Oxygen index above 35 | Dark gray, black | For applications requiring high acid and high alkali resistance and good flame retardancy |
IFR-25 | Isophthalic type | Oxygen index above 28 | Grass green, yellow, gray | VEFR type is economical with good performance, resistant to moderate acids, alkalis and solvents |
IFGR-30 | Phthalic anhydride type, food grade | Limiting oxygen index 26 | Yellow | Mainly used in meat processing and food processing plants |
OFR-25 | Orthophthalic type | Oxygen index above 28 | Grass green, yellow, gray | General acid and alkali environments |
OCR | Orthophthalic type | Limiting oxygen index below 28 | Green, yellow, gray | OFR-25 economical type, no flame retardancy requirement |
Coarse fiberglass type selection
| Code | Coarse fiber type | Recommended applications |
E | Alkali-free (E-glass) fiber | For applications requiring high strength and high corrosion resistance |
Selected filler type
Code | Filler type | Recommended applications |
|---|---|---|
ATH | Aluminum hydroxide | Flame-retardant, smoke-suppressing and corrosion-resistant applications |
PR | Unfilled, pure resin | Suitable for high-corrosion-resistance applications |




38*38*30(mm)
Optional panel sizes:
1524*4000,1220*4000,1220*3660,1220*2440,915*3050 Bidirectional load bearing.
Load-bearing flat bar thickness (top/bottom): 6.0/5.0
Load-bearing flat bar center spacing: 38
Open area: 68%
Approximate weight: 14.6 kgs/m²

Line load (unit: mm)
Deflection | kg/m | kg/m | kg/m | kg/m |
kg/m |
kg/m |
Ultimate |
|---|---|---|---|---|---|---|---|
Span (mm) | 75 | 150 | 300 | 450 | 750 | 1500 | Load |
| 300 | <0.25 | <0.25 | 0.25 | 0.51 | 0.76 | 1.52 | 9923.4 |
| 450 | 0.25 | 0.51 | 1.02 | 1.52 | 2.54 | 3.92 | 4827.6 |
| 600 | 0.51 | 1.27 | 2.29 | 3.56 | 5.84 | 7.38 | 4112.4 |
| 750 | 1.27 | 2.54 | 4.83 | 7.37 | 12.5 | 16.0 | 3173.7 |
| 900 | 2.27 | 4.54 | 9.08 | 13.6 | 18.7 | 22.1 | 2637.3 |

Uniformly distributed load (unit: mm)
Deflection |
kg/m² |
kg/m² |
kg/m² |
kg/m² |
kg/m² |
kg/m² |
|---|---|---|---|---|---|---|
Span (mm) | 350 | 500 | 750 | 1000 | 1500 | 2500 |
| 300 | 0.29 | 0.48 | 0.57 | 0.75 | 1.15 | 1.82 |
| 450 | 0.78 | 1.19 | 1.81 | 2.47 | 3.54 | 4.95 |
| 600 | 1.76 | 2.66 | 4.28 | 5.56 | 8.41 | 13.2 |
| 750 | 3.48 | 5.12 | 8.21 | 11.0 | 16.42 | --- |
| 900 | 5.89 | 8.81 | 14.2 | 18.9 | --- | --- |

Features:
Corrosion-resistant
Slip-resistant
Excellent ergonomic design
Low installation cost
Flame-retardant
Lightweight with high bidirectional strength; cutting makes the panels easier to install.
Uniform color inside and out; colors can be selected freely.
Delivers favorable social and economic benefits.
Flexible design, a variety of sizes, and dimensional stability
Widely used in:
Greenlogy TEC FRP grating is widely used for platform (industrial) flooring, stairways, walkways and platforms. Using FRP grating offers many advantages: good weather resistance, low maintenance cost, long service life and good slip resistance. In addition, FRP grating is simple, fast and flexible to fabricate and assemble.



Application scenarios
FRP molded grating 38*38H30 is suitable for corrosive environments such as chemical plants, wastewater treatment and marine engineering, and can also be used as platforms, walkways, trench covers and other applications requiring slip resistance and corrosion resistance. Its lightweight, high-strength characteristics make it an ideal alternative to conventional metal grating.
Selection guidance
When selecting, consider the resin type (such as orthophthalic, isophthalic and vinyl ester types) to suit different corrosion resistance requirements, and choose the appropriate grating thickness and mesh size according to load requirements. For detailed technical parameters and selection advice, please contact us for professional guidance.
Product advantages
This grating features excellent corrosion resistance, light weight and high strength, slip resistance, insulation and easy installation, along with low maintenance cost and long service life. The molded process ensures dimensional stability and a smooth surface, and colors can be customized on request.
Inquiry guidance
For specific specifications, pricing or customization requirements for FRP molded grating 38*38H30, please contact us via the contact details on this website, and we will provide a detailed quotation and technical support.
Service environment
- This FRP molded grating is molded from unsaturated polyester resin (including orthophthalic, bisphenol and phenolic types) combined with glass fiber, and can be used for indoor and outdoor installation.
- Molded mesh structures with a specific open area are typically used in industrial plants and process areas where corrosive media, moisture and humid atmospheres are present.
- For installations exposed to specific chemicals, temperature or humidity conditions, please select a resin type that matches the actual service environment (for example, phenolic type may be chosen where low toxicity and high flame retardancy are required).
- Please contact us for the complete parameter table and to confirm the resin grade and glass fiber content suitable for your operating conditions.
Custom Cutting
Need panels that fit, or cut to shape? We custom cut FRP grating and profiles to your drawing: panels cut to size or to shape (corner cuts, cutouts), cut edges sealed with resin, and pre-cut and pre-drilled to drawing before shipping. See the custom cutting services.
简体中文