FRP Molded Grating 38*38H30 (OFR-25)
Request a Quote
Please feel freely to contact with us for new price .
Genius FRP
Glass fiber reinforced plastic ( FRP ) molding grid is a kind of plate material with a certain opening rate, which is made of unsaturated polyester resin ( including isophthalic up, linbenxing, type and fenquanxing, bisphenol ) as skeleton in the customization mold.
| Name | Content | Type |
|---|---|---|
Resin | 35% | OFR-25,IFR-25,VEFR-25 |
Fiberglass | 33% | E |
Filler | 31% | ATH,PR |
Others | 1% | --- |
Resin type
Code | Resin type | Flame retardant property | Standard color | Recommended usage occasions |
|---|---|---|---|---|
MP-5 | Phenolic type | Oxygen index can reach about 80 | Brown | Low toxicity and high flame retardant, fire safety is very important for the occasion |
VEFR-25 | Vinyl type | Oxygen index 28 or above | Grass green,Yellow, Grey, Orange | Acid, alkali and other corrosive harsh environment |
VEFR-10 | Vinyl type | Oxygen index 35 or above | Dark grey, Black | Flame retardant requirements of high acid, alkali and good occasions |
IFR-25 | Meta benzene | Oxygen index 28 or above | Grass green,Yellow, Grey | A VEFR type economy, and excellent, moderate acid alkali and solvent |
IFGR-30 | Benzene food grade | Oxygen index 26 | Yellow | Mainly used in meat products and food processing plants |
OFR-25 | Ortho type | Oxygen index 28 or above | Grass green,Yellow, Grey | General acid and alkali environment |
OCR | Ortho type | Oxygen index below 28 | Green,Yellow, Grey | OFR-25 economy, no flame retardant requirements |
The type selection of coarse glass fiber
| Code | Coarse sand type | Recommended usage occasions |
E | Non alkali sand | For high strength requirements and high corrosion resistance of the occasion |
Selected filler type
Code | Filler type | Recommended usage occasions |
|---|---|---|
ATH | Aluminum hydroxide | Retardant, smoke suppression, corrosion-resistant occasions |
PR | No filler, pure resin | For high corrosion-resistant applications |




38*38*30(mm)
Panel size available:
1524*4000,1220*4000,1220*3660,1220*2440,915*3050 Bidirectional force.
Bearing bar thickness (Top/Bottom):6.0/5.0
Bearing bar center:38
Open Aera:68%
Approx Weight:14.6kgs/m²

Liner load(units:mm)
Deflection | kg/m | kg/m | kg/m | kg/m |
kg/m |
kg/m |
Limit |
|---|---|---|---|---|---|---|---|
Span(mm) | 75 | 150 | 300 | 450 | 750 | 1500 | load |
| 300 | <0.25 | <0.25 | 0.25 | 0.51 | 0.76 | 1.52 | 9923.4 |
| 450 | 0.25 | 0.51 | 1.02 | 1.52 | 2.54 | 3.92 | 4827.6 |
| 600 | 0.51 | 1.27 | 2.29 | 3.56 | 5.84 | 7.38 | 4112.4 |
| 750 | 1.27 | 2.54 | 4.83 | 7.37 | 12.5 | 16.0 | 3173.7 |
| 900 | 2.27 | 4.54 | 9.08 | 13.6 | 18.7 | 22.1 | 2637.3 |

Uniform load(units:mm)
Deflection |
kg/m² |
kg/m² |
kg/m² |
kg/m² |
kg/m² |
kg/m² |
|---|---|---|---|---|---|---|
Span(mm) | 350 | 500 | 750 | 1000 | 1500 | 2500 |
| 300 | 0.29 | 0.48 | 0.57 | 0.75 | 1.15 | 1.82 |
| 450 | 0.78 | 1.19 | 1.81 | 2.47 | 3.54 | 4.95 |
| 600 | 1.76 | 2.66 | 4.28 | 5.56 | 8.41 | 13.2 |
| 750 | 3.48 | 5.12 | 8.21 | 11.0 | 16.42 | --- |
| 900 | 5.89 | 8.81 | 14.2 | 18.9 | --- | --- |

The characteristics:
Corrosion Resistant
Slip Resistant
Superior Ergonomics
Low Install Cost
Fire Retardant
Lightweight,Bi-directional Strength, and the cutting makes the pipes easier to install.
The internal and external uniform color and color can be arbitrary choice.
It has good social and economic benefits.
Can design , flexible and varied size, size stability
Widely used in:
Genius FRP grating is widely used in landing (industrial) floor, stairs and walkways and platforms. Using glass fiber reinforced plastic grille has many advantages: glass fiber reinforced plastic grille, weather resistance, low maintenance cost, has a long service life and good anti-skid performance. In addition, the glass fiber reinforced plastic grille is simple, fast, flexible processing and assembly.



Application Scenarios
FRP molded grating 38*38H30 is suitable for corrosive environments such as chemical, wastewater treatment, and marine engineering. It can also be used as platforms, walkways, trench covers, and other applications requiring slip resistance and corrosion resistance. Its lightweight and high-strength characteristics make it an ideal replacement for traditional metal grating.
Selection Guide
When selecting, consider the resin type (such as orthophthalic, isophthalic, vinyl ester, etc.) to suit different corrosion resistance requirements, and choose the appropriate grating thickness and mesh size based on load-bearing needs. For detailed technical parameters and selection advice, please contact us for professional guidance.
Product Advantages
This grating features excellent corrosion resistance, lightweight and high strength, slip resistance, insulation, and easy installation, with low maintenance costs and long service life. The molded process ensures stable dimensions and a smooth surface, and colors can be customized upon request.
Inquiry Guide
For specific specifications, pricing, or customization needs of FRP molded grating 38*38H30, please contact us through the website contact information. We will provide you with detailed quotations and technical support.
Operating Environment
- This FRP molded grating is built from unsaturated polyester resin (including isophthalic, bisphenol and phenolic types) combined with fiberglass, allowing it to serve in both indoor and outdoor installations.
- The molded grid structure with a defined opening rate is typically used where corrosive media, moisture and humid atmospheres are present in industrial plants and process areas.
- For installations exposed to specific chemicals, temperature or humidity conditions, select the resin type (such as phenolic for low toxicity and high flame retardant demands) that matches the actual service environment.
- Contact us for the full parameter list and to confirm the resin grade and fiberglass content suitable for your operating conditions.