Genius FRP  

 Fiberglass Reinforced Plastic (FRP) grating is a panel with a certain open area, custom-molded using unsaturated polyester resin (including isophthalic, phenylene, and phenolic/bisphenol types) as the matrix. 

Name

Content

Type

Resin

35%

OFR-25、IFR-25、VEFR-25

Glass Fiber

33%

E

Filler

31%

ATH、PR

Others

1%

---

Raw Material Introduction

 Resin Type

Code

Resin Type

Flame Retardancy

Recommended Applications

MP-5

Phenolic Type

Oxygen index up to approximately 80

Low toxicity, high flame retardancy, for applications where fire safety is extremely important

VEFR-25

Vinyl Ester Type

Oxygen index 28 or above

For highly corrosive environments such as acids, alkalis, and solvents

VEFR-10

Vinyl Ester Type

Oxygen index 35 or above

For applications requiring high flame retardancy and excellent acid and alkali resistance

IFR-25

Isophthalic Type

Oxygen index 28 or above

More economical than VEFR type, excellent acid resistance, moderate alkali resistance

IFGR-30

Isophthalic food grade

Oxygen index 26

Mainly used in meat product and food processing plants

OFR-25

Orthophthalic type

Oxygen index 28 or above

General acid and alkali environments

OCR

Orthophthalic type

Oxygen index below 28

More economical than OFR-25, no flame retardant requirement

Type of glass fiber grit selected   

Code

Grit type

Recommended Applications

E

E-glass grit

Used in applications requiring high strength and high corrosion resistance

Type of filler selected   

Code

Filler type

Recommended Applications

ATH

Aluminum hydroxide

Flame retardant, smoke suppressant, corrosion resistant applications

PR

No filler, pure resin

For high corrosion resistance applications

Software - Sample 1 for three columns

Grooved type

Software - Sample 2 for three columns

Sanded type

Software - Sample 3 for three columns

Gritted type

13 13 H30

13*13*30(mm)

Full panel size:

1220*3660,1220*2440,915*3050 Bidirectional load bearing.     

Bearing bar wall thickness (top/bottom): 7.5&4.5/6.0

Bearing bar center spacing: 13

Open area: 30%

Approximate weight per square meter: 19.5kgs/m²

Software image and text block

Molded grating features:

  1. Corrosion resistant 

  2. High slip resistance 

  3. Good work efficiency 

  4. Low installation cost 

  5. Fire Retardant 

  6. Lightweight,Bi-directional Strength, and the cutting makes the pipes easier to install.

  7. The internal and external uniform color and color can be arbitrary choice.

  8. It has good social and economic benefits.

  9. Can design , flexible and varied size, size stability


Widely used in:

Genius FRP grating is widely used in landing (industrial) floor, stairs and walkways and platforms. Using glass fiber reinforced plastic grille has many advantages: glass fiber reinforced plastic grille, weather resistance, low maintenance cost, has a long service life and good anti-skid performance. In addition, the glass fiber reinforced plastic grille is simple, fast, flexible processing and assembly.   

Software - Sample 1 for three columns


Software - Sample 2 for three columns


耐腐蚀FRP格栅产品展示图



Selection guide

13*13H30 indicates the grating mesh size and thickness combination. When selecting, the resin system and fiberglass type should be confirmed according to load requirements, support span and corrosive media. Resins can be selected from orthophthalic, isophthalic, vinyl ester or phenolic types, and fillers can also be chosen from ATH flame retardant and smoke suppressant or pure resin options for high corrosion resistance. Please contact us for a suitable configuration based on your working conditions.

Inquiry guide

To confirm the load capacity, surface type (grooved, sanded or gritted) and applicable resin system of this specification, please contact us for detailed specifications and a quotation. Please provide the service environment, load requirements and dimensional requirements, and we will assist you in completing the selection.

Free,easy click for support

7*24 professional team support. Within 24 Hours, our team will give you the feedback.

Send   
 Website Visitor