Glass fiber reinforced plastic ( FRP ) molding grid is a kind of plate material with a certain opening rate, which is made of unsaturated polyester resin ( including isophthalic up, linbenxing, type and fenquanxing, bisphenol ) as skeleton in the customization mold. 

Name

Content

Type

Resin

35%

OFR-25,IFR-25,VEFR-25

Fiberglass

33%

E

Filler

31%

ATH,PR

Others

1%

---

Introduction of raw materials

 Resin type  

Code

Resin type

Flame retardant property

Recommended usage occasions

MP-5

Phenolic type

Oxygen index can reach about 80

Low toxicity and high flame retardant, fire safety is very important for the occasion

VEFR-25

Vinyl type

Oxygen index 28 or above

Acid, alkali and other corrosive harsh environment

VEFR-10

Vinyl type

Oxygen index 35 or above

Flame retardant requirements of high acid, alkali and good occasions

IFR-25

Meta benzene

Oxygen index 28 or above

A VEFR type economy, and excellent, moderate acid alkali and solvent

IFGR-30

Benzene food grade

Oxygen index 26

Mainly used in meat products and food processing plants

OFR-25

Ortho type

Oxygen index 28 or above

General acid and alkali environment

OCR

Ortho type

Oxygen index below 28

OFR-25 economy, no flame retardant requirements

The type selection of coarse glass fiber   

Code

Coarse sand type

Recommended usage occasions

E

Non alkali sand

For high strength requirements and high corrosion resistance of the occasio

Selected filler type  

Code

Filler type

Recommended usage occasions

ATH

Aluminum hydroxide

Retardant, smoke suppression, corrosion-resistant occasions

PR

No filler, pure resin

For high corrosion-resistant applications

Software - Sample 1 for three columns

Groove type

Software - Sample 2 for three columns

Polished type
Software - Sample 3 for three columns

Shop sand type

20 20 H30

20*20*30(mm)

Panel size available:

1007*4047,1007*3007 Bidirectional force.     

Bearing bar thickness (Top/Bottom):7.0/5.0

Bearing bar center:20

Open Aera:42%

Approx Weight:18kgs/m²

20 20 H30

The characteristics:

  1. Corrosion Resistant 

  2. Slip Resistant 

  3. Superior Ergonomics 

  4. Low Install Cost 

  5. Fire Retardant 

  6. Lightweight,Bi-directional Strength, and the cutting makes the pipes easier to install.

  7. The internal and external uniform color and color can be arbitrary choice.

  8. It has good social and economic benefits.

  9. Can design , flexible and varied size, size stability

Widely used in:

Greenlogy TEC FRP grating is widely used in landing (industrial) floor, stairs and walkways and platforms. Using glass fiber reinforced plastic grille has many advantages: glass fiber reinforced plastic grille, weather resistance, low maintenance cost, has a long service life and good anti-skid performance. In addition, the glass fiber reinforced plastic grille is simple, fast, flexible processing and assembly.   

Software - Sample 1 for three columns
Software - Sample 2 for three columns
Software - Sample 3 for three columns

Application Scenarios

FRP molded grating is commonly used in platforms, walkways and trench covers with high corrosion resistance requirements in electroplating, chemical, wastewater treatment and marine engineering, and is also suitable for maintenance access ways requiring insulation and lightweight load-bearing. The 20×20H30 mesh size suits areas with combined requirements on open area and load capacity. Welcome to contact us to describe your working conditions for suitable recommendations.

Selection Guide

When selecting, it is usually necessary to confirm the resin system (such as orthophthalic, isophthalic, vinyl ester, phenolic, etc.), grating thickness and mesh size, load rating, and the corrosive media and temperature conditions of the service environment. The raw material formulation and resin type listed on this page are for reference only; please confirm specific specifications with us. Welcome to contact us for detailed specifications and a quotation.

Product Advantages

FRP molded grating is integrally molded from glass fiber reinforced resin, featuring corrosion resistance, lightweight and high strength, insulation and non-magnetic properties, and ease of cutting and installation, with relatively low long-term maintenance costs. Different resin systems can correspond to different corrosion-resistance and flame-retardant requirements; specific performance needs to be evaluated based on actual working conditions. Welcome to contact us for detailed specifications and a quotation.

Inquiry Guidance

To learn about the dimensional tolerances, colors, surface treatments, packaging and transportation details of FRP Grating 20×20H30, please provide information such as the application scenario, quantity and target market so that we can offer a targeted solution. Welcome to contact us for detailed specifications and a quotation, and we will arrange a dedicated contact as soon as possible.

Operating Environment

  • This molded FRP grating uses unsaturated polyester resin—including isophthalic, bisphenol, and phenolic types—as its matrix, allowing it to serve in indoor and outdoor installations where moisture and chemical exposure are routine.
  • The phenolic resin option provides high flame retardancy with an oxygen index of about 80, making this FRP grating suitable for fire-sensitive industrial environments where low toxicity and fire safety are priorities.
  • With E-glass fiber reinforcement and ATH or PR fillers, the grating handles corrosive media commonly found in chemical processing, wastewater treatment, and marine/offshore walkways and platforms.
  • Contact us for the full parameter list and to confirm the resin grade and configuration that match your specific operating conditions.

Custom Cutting

Need panels that fit, or cut to shape? We custom cut FRP grating and profiles to your drawing: panels cut to size or to shape (corner cuts, cutouts), cut edges sealed with resin, and pre-cut and pre-drilled to drawing before shipping. See the custom cutting services.

WhatsApp