FRP molded grating is a panel with a certain open area, made with unsaturated polyester resin (including isophthalic, orthophthalic, phenolic and bisphenol types) as the matrix and produced in custom molds.

Name

Content

Type

Resin

35%

OFR-25,IFR-25,VEFR-25

Glass fiber

33%

E

Filler

31%

ATH,PR

Others

1%

---

Introduction to raw materials

Resin type 

Code

Resin type

Flame retardancy

Recommended applications

MP-5

Phenolic type

Oxygen index up to about 80

Low toxicity and high flame retardancy; suitable for applications with high fire safety requirements

VEFR-25

Vinyl ester type

Oxygen index 28 and above

Harsh corrosive environments such as acids and alkalis

VEFR-10

Vinyl ester type

Oxygen index 35 and above

Applications requiring high flame retardancy and good acid and alkali resistance

IFR-25

Isophthalic type

Oxygen index 28 and above

VEFR type, economical, good performance, resistant to moderate acids, alkalis and solvents

IFGR-30

Food grade

Oxygen index 26

Mainly used in meat products and food processing plants

OFR-25

Orthophthalic type

Oxygen index 28 and above

General acid and alkali environments

OCR

Orthophthalic type

Oxygen index below 28

OFR-25 economical type, no flame retardancy requirement

Selection of coarse glass fiber  

Code

Coarse roving

Recommended applications

E

E-glass roving

For applications requiring high strength and high corrosion resistance

Selection of filler type 

Code

Filler type

Recommended applications

ATH

Aluminum hydroxide

Flame-retardant, smoke-suppressing and corrosion-resistant applications

PR

No filler, pure resin

For high corrosion resistance applications

Software - Three-column example 1

Grooved type
Software - Three-column example 2

Polished type
Software - Three-column example 3

Sandblasted type

25 100 H25

25*100*25(mm)

Optional panel dimensions:

1007*3007 Bearing bar width     

Bearing bar thickness (top/bottom): 7.0/5.5

Bearing bar center distance: 25

Open area: 67%

Approximate weight: 13 kgs/m²

Diagram illustrating line load distribution on FRP molded grating

Line load (unit: mm)

Deflection

kg/m

kg/m

kg/m

kg/m

kg/m

kg/m

Ultimate

Span (mm)

75150300450600750

Load

3000.330.480.740.991.271.529942
6000.861.733.455.186.918.644305
7501.402.725.117.169.5511.93589
9002.414.728.1812.416.520.63216
Diagram illustrating uniform load distribution on FRP molded grating

Uniformly distributed load (unit: mm)

Deflection

kg/m²

kg/m²

kg/m²

kg/m²

kg/m²

kg/m²

kg/m²

Span (mm)

2404809801450245036504880
3000.280.380.530.711.04---1.91
6000.911.853.685.549.22---18.5
9003.636.612.618.5---------
10508.0114.9---------------
25 100 H25

Features:

  1. Corrosion resistant 

  2. Slip resistant 

  3. Excellent ergonomic design 

  4. Low installation cost 

  5. Flame retardant 

  6. Lightweight, high bi-directional strength, and easy to cut and install.

  7. Uniform color inside and out; color can be freely selected.

  8. Delivers good social and economic benefits.

  9. Designable, flexible and diverse in size, dimensionally stable

Widely used in:

Greenlogy TEC FRP grating is widely used for platform (industrial) flooring, stairways, walkways and platforms. Using FRP grating offers many advantages: good weather resistance, low maintenance cost, long service life and good anti-slip performance. In addition, FRP grating is simple, fast and flexible to process and assemble.

Software - Three-column example 1
Software - Three-column example 2
Software - Three-column example 3

Application scenarios

FRP molded grating 25*100H25 is suitable for platforms, walkways, stair treads and trench covers in chemical, petroleum, power, marine engineering and other fields. Its corrosion resistance, anti-slip performance and high strength-to-light weight make it perform well in harsh environments such as damp, acid and alkaline conditions.

Selection guide

When selecting, consider load-bearing requirements, span, corrosive environment and safety level. 25*100H25 indicates a grating thickness of 25 mm and a mesh size of 100 mm. Different resin types (such as orthophthalic, isophthalic, vinyl ester, phenolic, etc.) can be selected according to specific needs to meet corrosion resistance or flame retardant requirements.

Product advantages

FRP molded grating features light weight, high strength, corrosion resistance, anti-slip, insulation and maintenance-free operation, with a long service life and easy installation, effectively reducing long-term costs.

Inquiry guidance

For more detailed specifications or technical parameters of FRP molded grating 25*100H25, or to obtain a quotation, please contact us; we will provide professional technical support and customization services.

Operating environment

  • This FRP molded grating is based on unsaturated polyester resin and supports use in indoor and outdoor installations where moisture and humid air are present.
  • The phenolic resin option (MP-5) offers low toxicity and high flame retardant performance, suitable for fire-sensitive environments.
  • With its fiberglass reinforcement and resin matrix, the grating is suitable for areas exposed to corrosive media, as the material resists chemical attack.
  • Typical applications include walkways and platforms, where the grating must withstand foot traffic and environmental exposure without losing structural integrity.

Custom Cutting

Need panels that fit, or cut to shape? We custom cut FRP grating and profiles to your drawing: panels cut to size or to shape (corner cuts, cutouts), cut edges sealed with resin, and pre-cut and pre-drilled to drawing before shipping. See the custom cutting services.

WhatsApp