玻璃钢模塑格栅25*100H25
欢迎询价。
Genius FRP
Glass fiber reinforced plastic ( FRP ) molding grid is a kind of plate material with a certain opening rate, which is made of unsaturated polyester resin ( including isophthalic up, linbenxing, type and fenquanxing, bisphenol ) as skeleton in the customization mold.
Name | Content | Type |
Resin | 35% | OFR-25、IFR-25、VEFR-25 |
Fiberglass | 33% | E |
Filler | 31% | ATH、PR |
Others | 1% | --- |
Resin type
Code | Resin type | Flame retardant property | Recommended usage occasions |
MP-5 | Phenolic type | Oxygen index can reach about 80 | Low toxicity and high flame retardant, fire safety is very important for the occasion |
VEFR-25 | Vinyl type | Oxygen index 28 or above | Acid, alkali and other corrosive harsh environment |
VEFR-10 | Vinyl type | Oxygen index 35 or above | Flame retardant requirements of high acid, alkali and good occasions |
IFR-25 | Meta benzene | Oxygen index 28 or above | A VEFR type economy, and excellent, moderate acid alkali and solvent |
IFGR-30 | Benzene food grade | Oxygen index 26 | Mainly used in meat products and food processing plants |
OFR-25 | Ortho type | Oxygen index 28 or above | General acid and alkali environment |
OCR | Ortho type | Oxygen index below 28 | OFR-25 economy, no flame retardant requirements |
The type selection of coarse glass fiber
Code | Coarse sand type | Recommended usage occasions |
E | Non alkali sand | For high strength requirements and high corrosion resistance of the occasio |
Selected filler type
Code | Filler type | Recommended usage occasions |
ATH | Aluminum hydroxide | Retardant, smoke suppression, corrosion-resistant occasions |
PR | No filler, pure resin | For high corrosion-resistant applications |




25*100*25(mm)
Panel size available:
1007*3007 Width stress
Bearing bar thickness (Top/Bottom):7.0/5.5
Bearing bar center:25
Open Aera:67%
Approx Weight:13kgs/m²

Liner load(units:mm)
Deflcvtion | kg/m | kg/m | kg/m | kg/m | kg/m | kg/m | Limit |
Span( mm) | 75 | 150 | 300 | 450 | 600 | 750 | Load |
| 300 | 0.33 | 0.48 | 0.74 | 0.99 | 1.27 | 1.52 | 9942 |
| 600 | 0.86 | 1.73 | 3.45 | 5.18 | 6.91 | 8.64 | 4305 |
| 750 | 1.40 | 2.72 | 5.11 | 7.16 | 9.55 | 11.9 | 3589 |
| 900 | 2.41 | 4.72 | 8.18 | 12.4 | 16.5 | 20.6 | 3216 |

Uniform load(units:mm)
Deflcvtion |
kg/m² |
kg/m² |
kg/m² |
kg/m² |
kg/m² |
kg/m² |
kg/m² |
Span( mm) | 240 | 480 | 980 | 1450 | 2450 | 3650 | 4880 |
| 300 | 0.28 | 0.38 | 0.53 | 0.71 | 1.04 | --- | 1.91 |
| 600 | 0.91 | 1.85 | 3.68 | 5.54 | 9.22 | --- | 18.5 |
| 900 | 3.63 | 6.6 | 12.6 | 18.5 | --- | --- | --- |
| 1050 | 8.01 | 14.9 | --- | --- | --- | --- | --- |

The characteristics:
Corrosion Resistant
Slip Resistant
Superior Ergonomics
Low Install Cost
Fire Retardant
Lightweight,Bi-directional Strength, and the cutting makes the pipes easier to install.
The internal and external uniform color and color can be arbitrary choice.
It has good social and economic benefits.
Can design , flexible and varied size, size stability
Widely used in:
Genius FRP grating is widely used in landing (industrial) floor, stairs and walkways and platforms. Using glass fiber reinforced plastic grille has many advantages: glass fiber reinforced plastic grille, weather resistance, low maintenance cost, has a long service life and good anti-skid performance. In addition, the glass fiber reinforced plastic grille is simple, fast, flexible processing and assembly.
应用场景
玻璃钢模塑格栅25*100H25适用于化工、石油、电力、海洋工程等领域的平台、走道、楼梯踏板及沟盖板。其耐腐蚀、防滑、轻质高强的特性使其在潮湿、酸碱等恶劣环境中表现优异。
选型指导
选型时需考虑承载要求、跨距、腐蚀环境及安全等级。25*100H25表示格栅厚度25mm、网格尺寸100mm。可根据具体需求选择不同树脂类型(如邻苯、间苯、乙烯基酯、酚醛等)以满足耐腐蚀或阻燃要求。
产品优势
玻璃钢模塑格栅具有重量轻、强度高、耐腐蚀、防滑、绝缘、免维护等特点,使用寿命长,安装简便,可有效降低长期成本。
询盘引导
如需了解更多关于玻璃钢模塑格栅25*100H25的详细规格、技术参数或获取报价,欢迎联系我们,我们将为您提供专业的技术支持和定制服务。