Structural Profiles - Kick Plates (Orthophthalic)

Structural Profiles - Kick Plates (Orthophthalic)

Price on request

Request a Quote


Please feel freely to contact with us for new price .

Greenlogy TEC

  FRP structural profiles are made from glass fiber reinforcing material, with resin as the binder and glass fiber cloth as the wrapping reinforcement layer. After thorough impregnation, the material is heated, shaped and cured in a metal mold and then pultruded under the pull of a traction machine, forming a new type of composite material with good physical properties that is widely used in high-strength, long-span applications.  

Greenlogy TEC OFR-25 fiberglass composite structural profile kick plate

Variety

Size (mm)

Weight (kg/m)

Size (in)

Weight (lbs/in)

Kick Plate

A*B*T


A*B*T


M2

100*13*3.2 M型

1.1

4" x 1/2" x 1/8" M型

2.43

M3

100*16*5 M型

1.3

4" x 5/8" x 3/16" M型

2.87

M4

148*12*3 M型

1.27

23/4" x 1/2" x 1/8" M型

2.8

W1

100*19*5 W型

1.36

4" x 3/4" x 3/16" W型

3

W2

100*15*3.2 W型

1.1

4" x 9/16" x 1/8" W型

2.43

W3

150*15*3.2 W型

1.6

6" x 9/16" x 1/8" W型

3.53

Markets 

Applications of Greenlogy TEC fiberglass profiles in construction, bridges and highways
  • Construction

  • Bridges and highways

  • Chemical

  • Food and beverage

  • Manufacturing

  • Metals and mining

  • Microelectronics

  • Oil and gas

  • Pharmaceutical

  • Power

  • Pulp and paper

  • Recreation and entertainment

  • Telecommunications

  • Transportation

  • Water and wastewater treatment

Features:

  • Corrosion resistant

  • Low maintenance cost

  • Flame retardant

  • Low installation cost

  • Heavy-metal safe

  • Long service life

  • Non-conductive and non-thermal-conductive

  • High strength-to-weight ratio

Raw material introduction — resin types

Code

Resin type

Flame retardancy

Recommended applications

VEFR-25

Vinyl ester type

Oxygen index 28 and above

Harsh corrosive environments such as acids and alkalis

IFR-25

Isophthalic type

Oxygen index 28 and above

VEFR type: economical yet high-performing, suitable for medium acid, alkali and solvent environments

OFR-25

Orthophthalic type

Oxygen index 28 and above

General acid and alkali environments

 Applications: 

   Greenlogy TEC pultruded FRP structural profiles are widely used in various applications, combining corrosion resistance, high strength, dimensional stability and light weight, with thermal insulation and electrical insulation properties. Durable Greenlogy TEC profiles provide years of low-maintenance service in areas where steel, aluminum or wood components have traditionally been specified. Today, these profiles are commonly used in highly corrosive applications that previously required stainless steel and other costly components.   

Greenlogy TEC profiles

Mechanical Properties

ASTM

Unit

Value

Unit

Value

Tensile Stress, LW

D-638

psi

30000

kgf/m²

21092086

Tensile Stress, CW

D-638

psi

7000

kgf/m²

4921487

Tensile Modulus, LW

D-638

10^6psi

2.5

10^6kgf/m²

1758

Tensile Modulus, CW

D-638

10^6psi

0.8

10^6kgf/m²

562

Compressive Stress, LW

D-695

psi

30000

kgf/m²

21092086

Compressive Stress, CW

D-695

psi

15000

kgf/m²

10546043

Compressive Modulus, LW

D-695

10^6psi

2.5

10^6kgf/m²

1758

Compressive Modulus, CW

D-695

10^6psi

1

10^6kgf/m²

703

Flexural Stress, LW

D-790

psi

30000

kgf/m²

21092086

Flexural Stress, CW

D-790

psi

10000

kgf/m²

7030695

Flexural Modulus, LW

D-790

10^6psi

1.8

10^6kgf/m²

1266

Flexural Modulus, CW

D-790

10^6psi

0.8

10^6kgf/m²

562

Modulus of Elasticity

Full Section

10^6psi

2.8

10^6kgf/m²

1969

Shear Modulus

---

10^6psi

0.45

10^6kgf/m²

316

Short-Beam Shear

D-2344

psi

4500

kgf/m²

3163813

Punch Shear

D-732

psi

10000

kgf/m²

7030695

Notched Izod Impact, LW

D-256

ft.-lbs./in.

25

kg/m

3.46

Notched Izod Impact, CW

D-256

ft.-lbs./in.

4

kg/m

0.55

  Excluding Round Rods and Square Rods

Physical Properties

ASTM

Unit

Value

Barcol hardness

D-495

---

45

24-hour water absorption

D-570

% max

0.45

Density

D-792

lbs./in.³

0.062-0.07

Coefficient of thermal expansion, LW

D-696

10^-6in./in./℃

8

Flame retardancy

ASTM

Unit

Value

Tunnel test*

E-84

Flame spread

Max. 25

Combustibility*

D-635

---

Non-combustible

Electrical properties

ASTM

Unit

Value

Arc resistance, LW

D-495

秒(s)

120

Dielectric strength, LW

D-149

kv./in.

35

Dielectric strength, PF

D-149

Volts/mil

200

Dielectric constant, PF

D-150

@60hz

5

LW = lengthwise, CW = crosswise, PF = perpendicular to laminate surface

*Applies to ISOFR and VEFR only


Applications

Kick plate profiles are suitable for industrial platforms, floor edges, and protective and decorative edge finishing in corrosive environments, and can be used together with structural profile systems. In chemical plants, wastewater treatment facilities, marine engineering and similar locations, they provide corrosion-resistant, insulating kick protection and extend the service life of the base structure. Contact us to learn about specific application cases and suitable solutions.

Selection Guide

Please select the cross-section shape and thickness according to the dimensions of the installation location, load requirements and environmental conditions; for example, models such as M2, M3 and M4 correspond to different sizes. If custom lengths or colors are required, you can provide drawings or samples, and we will assist with selection. Contact us for detailed specification sheets and technical support.

Product Advantages

FRP kick plates feature light weight, high strength, corrosion resistance, insulation and low maintenance; their smooth surface is easy to clean, and they offer wide design flexibility. Compared with traditional metal materials, they last longer in damp or chemically corrosive environments and are easy to install. Contact us for samples and performance data.

Inquiry Guidance

To obtain product quotations, technical parameters or customization services, please contact us through the website and provide the required model, quantity and application; we will reply as soon as possible. We welcome your inquiries and cooperation.

Operating Environment

  • FRP kick plates are suitable for indoor and outdoor installation, including industrial plants, walkways and platforms.
  • The fiberglass-reinforced composite structure offers moisture and humidity resistance, making it suitable for use in damp or water-immersed environments.
  • These profiles can withstand a variety of corrosive media encountered in industrial environments, such as chemical plants and wastewater treatment facilities.
  • They can operate reliably across the range of ambient temperatures commonly found in industrial and commercial applications.

Custom Cutting

Need panels that fit, or cut to shape? We custom cut FRP grating and profiles to your drawing: panels cut to size or to shape (corner cuts, cutouts), cut edges sealed with resin, and pre-cut and pre-drilled to drawing before shipping. See the custom cutting services.

WhatsApp