LM Stainless Steel Wire Rope GB1X19 (12/6/1)
Please feel freely to contact with us for new price .
Product Details
1X19 stainless steel strand is a very popular stainless steel construction. Used heavily throughout the marine industry, 1X19’s excellent breaking load and low stretch characteristics along with its aesthetic appeal makes it a favourite for marine, structural and balustrade applications as well as many others.
Surface treatment:Ungalv or Galvanized
Standard:GB/T 20118-2006

Applications
Balustrades
Standing rigging
Mast stays
Guardrail
Structural
Stay wires
Marine/Saltwater environment
Sewage treatment work
Breaking Loads
Diameter
| Weight
|
Min Breaking Loads(1570Mpa)
|
Min Breaking Loads(1570Mpa)
|
mm | kg/m | KN |
Kg |
| 4 | 0.09 | 14.5 | 1479 |
| 5 | 0.14 | 23.9 | 2438 |
| 6 | 0.2 | 34.8 | 3550 |
| 7 | 0.27 | 48.2 | 4916 |
| 8 | 0.35 | 60.3 | 6151 |
| 9 | 0.44 | 73.5 | 7497 |
| 10 | 0.55 | 95.8 | 9772 |
| 11 | 0.66 | 110 | 11220 |
| 12 | 0.79 | 141 | 14382 |
General Engineering Ropes
GREENLOGY TEC(LM) specializes in supplying multiple strands of ungalvanised and galvanized steel wire ropes. Our products range from 0.5mm to 64mm, including 1X19, 7X7, 6X19, 7X19, 6X36, 8X19, 8X36, 19X7 and 35X7 with both Fibre Core and Steel Cores. In addition to these conventional steel wire ropes, we can also provide high-quality special steel wire ropes.
Most wire ropes are used in harsh conditions and must have resistance to extrusion, bending fatigue and abrasion. All of our wire ropes are guaranteed to achieve the highest level , maximizing the service life to increase the productivity of end users. We ensure that all materials are produced in accordance with the best standards in the wire rope industry. Each wire rope can be supplied with a thimble eyes, swaged ends and wedge sockets ,as well as many other assembly components.In addition, we also provide customized services, our team of engineers can manufacture wire ropes of your required specifications. All materials are certified, traceable, and comply with ISO9001 standards.