Structural Profiles - U-Channel Square Tube Handrail Profile (Orthophthalic Resin)

Structural Profiles - U-Channel Square Tube Handrail Profile (Orthophthalic Resin)

Price on request

Request a Quote


Please feel freely to contact with us for new price .

Greenlogy TEC

  FRP pultruded profiles use glass fiber reinforcement as the reinforcing body and resin as the matrix, with glass fiber cloth as the covering reinforcing layer; after full impregnation, they are heated, formed and cured in a metal mold and shaped under the traction of a pulling machine. This new type of composite material has good physical properties and is widely used in high-strength, large-span applications.  

U-shaped Square Tube Handrail Profile

Type

Size (mm)

Weight (kg/m)

Size (in)

Weight (lbs/in)

U-shaped Square Tube Handrail Profile

A*B*T


A*B*T



62*59*4.51.5

5/2" x 9/4" x 3/16"

3.31

62*60*51.7

5/2" x 19/8" x 3/16"

3.75

Markets

U-shaped fiberglass square tube handrail profile OFR-25 for construction applications

  • Construction

  • Bridges and highways

  • Chemical

  • Food and beverage

  • Manufacturing

  • Metals and mining

  • Microelectronics

  • Oil and gas

  • Pharmaceutical

  • Power

  • Pulp and paper

  • Recreation

  • Telecommunications

  • Transportation

  • Water and wastewater treatment

Features:

  • Corrosion resistance

  • Low maintenance

  • Flame retardant

  • Low installation cost

  • Heavy-metal safe

  • Long service life

  • Non-conductive and non-thermal-conductive

  • High strength-to-weight ratio

Raw material introduction — resin types

Code

Resin type

Flame retardant performance

Recommended applications

VEFR-25

Vinyl ester type

Oxygen index 28 and above

Acid, alkali and other harsh corrosive environments

IFR-25

Isophthalic type

Oxygen index 28 and above

VEFR: economical, good performance, moderate resistance to acids, alkalis and solvents

OFR-25

Orthophthalic type

Oxygen index 28 and above

General acid and alkali environments

Applications:

    Greenlogy TEC pultruded FRP structural profiles are widely used in various applications, combining corrosion resistance, high strength, dimensional stability and light weight, with thermal insulation and electrical insulation properties. Durable Greenlogy TEC profiles provide years of low-maintenance service in areas where steel, aluminum or wood members are traditionally specified. Today, these profiles are often used in highly corrosive applications that previously required stainless steel and other costly components.   

Greenlogy TEC profiles

Mechanical properties

ASTM

Unit

Value

Unit

Value

Tensile strength, LW

D-638

psi

30000

kgf/m²

21092086

Tensile strength, CW

D-638

psi

7000

kgf/m²

4921487

Tensile modulus, LW

D-638

10^6psi

2.5

10^6kgf/m²

1758

Tensile modulus, CW

D-638

10^6psi

0.8

10^6kgf/m²

562

Compressive strength, LW

D-695

psi

30000

kgf/m²

21092086

Compressive strength, CW

D-695

psi

15000

kgf/m²

10546043

Compressive modulus, LW

D-695

10^6psi

2.5

10^6kgf/m²

1758

Compressive modulus, CW

D-695

10^6psi

1

10^6kgf/m²

703

Flexural strength, LW

D-790

psi

30000

kgf/m²

21092086

Flexural strength, CW

D-790

psi

10000

kgf/m²

7030695

Flexural modulus, LW

D-790

10^6psi

1.8

10^6kgf/m²

1266

Flexural modulus, CW

D-790

10^6psi

0.8

10^6kgf/m²

562

Modulus of elasticity

Full section

10^6psi

2.8

10^6kgf/m²

1969

Shear modulus

---

10^6psi

0.45

10^6kgf/m²

316

Short-beam shear strength

D-2344

psi

4500

kgf/m²

3163813

Punch shear strength

D-732

psi

10000

kgf/m²

7030695

Notched Izod impact strength, LW

D-256

ft.-lbs./in.

25

kg/m

3.46

Notched Izod impact strength, CW

D-256

ft.-lbs./in.

4

kg/m

0.55

Excluding round rods and square rods  

Physical properties

ASTM

Unit

Value

Barcol hardness

D-495

---

45

24-hour water absorption

D-570

% maximum

0.45

Density

D-792

lbs./in.³

0.062-0.07

Coefficient of thermal expansion, LW

D-696

10^-6in./in./℃

8

Flame retardant performance

ASTM

Unit

Value

Tunnel test*

E-84

Flame spread

25 max

Flammability*

D-635

---

Non-burning

Electrical properties

ASTM

Unit

Value

Arc resistance, LW

D-495

秒(s)

120

Dielectric strength, LW

D-149

kv./in.

35

Dielectric strength, PF

D-149

Volts/mil

200

Dielectric constant, PF

D-150

@60hz

5

LW = lengthwise, CW = crosswise, PF = perpendicular to laminate surface

*Applies to ISOFR and VEFR only


Application Scenarios

This U-shaped square tube handrail profile is suitable for building railings, bridge walkway handrails, edge protection for platforms and walkways, and other applications with requirements for strength and corrosion resistance. Its glass fiber reinforced structure is suitable for large-span, high-strength installation environments, and can also be used in chemical, coastal, and other projects susceptible to moisture and chemical media. Please contact us to confirm a suitable solution based on your project conditions.

Selection Guidance

When selecting, start with the cross-section dimensions, wall thickness, and unit weight, and match them to the handrail span, installation method, and load requirements. The table provides various A*B*T specifications and their corresponding weights for preliminary screening according to structural design requirements. If you need recommendations for specific spans and loads, please contact us for detailed specifications and selection advice.

Product Advantages

This profile uses glass fiber as reinforcement and resin as binder, and is formed through impregnation, heated compression molding and curing, and pultrusion. It offers good physical performance and corrosion resistance. Compared with traditional metal profiles, it is lighter in weight, easier to transport and install on site, and is suitable for high-strength and relatively large-span applications. Specific performance should be evaluated according to actual service conditions; please contact us for further information.

Inquiry Guidance

If you need to confirm commercial information such as specifications, batch quantities, or delivery times, please contact us for detailed specifications and a quotation. Please provide the required cross-section dimensions, quantity, and service environment, and we will arrange follow-up communication accordingly. All commercial terms can be further negotiated according to your project requirements.

Custom Cutting

Need panels that fit, or cut to shape? We custom cut FRP grating and profiles to your drawing: panels cut to size or to shape (corner cuts, cutouts), cut edges sealed with resin, and pre-cut and pre-drilled to drawing before shipping. See the custom cutting services.

WhatsApp