Pultruded Grating T-3810

Pultruded Grating T-3810

Price on request

Get a quote
Request a Quote


Please feel freely to contact with us for new price .

Greenlogy TEC

  Pultruded FRP grating is made from pultruded "I"-shaped and "T"-shaped profiles as load-bearing bars, with solid tubes or rods as connecting rods, assembled through a specific assembly process, and the panel surface has a certain gap.  

Name

Content

Type

Resin

25%

OFR-25,IFR-25,VEFR-25

Glass fiber

65%

E

Filler

8%

ATH,PR

Other

2%

---

Raw material introduction
Resin type

Code

Resin type

Flame retardant performance

Recommended applications

MP-5

Phenolic type

Oxygen index up to about 80

Low toxicity and high flame retardancy, for applications with high fire safety requirements

VEFR-25

Vinyl type

Oxygen index 28 and above

Harsh environments with strong corrosiveness such as acids and alkalis

VEFR-10

Vinyl type

Oxygen index 35 and above

Strong acids and strong alkalis with high flame retardant requirements, and applications with good service conditions

IFR-25

Isophthalic type

Oxygen index 28 and above

VEFR economical grade, good performance, moderate acid/alkali and solvent resistance

IFGR-30

Benzene grade, food grade

Oxygen index 26

Mainly used in meat products and food processing plants

OFR-25

Orthophthalic type

Oxygen index 28 and above

General acid and alkali environments

OCR

Orthophthalic type

Oxygen index below 28

OFR-25 economical grade, no flame-retardant requirement

Coarse glass fiber selection 

Code

Coarse sand type

Recommended applications

E

Alkali-free sand

For applications requiring high strength and high corrosion resistance

Selected filler type  

Code

Filler type

Recommended applications

ATH

Aluminum hydroxide

Flame-retardant, smoke-suppressing, corrosion-resistant applications

PR

No filler, pure resin

For high corrosion resistance applications

Software - Three-column example 1

Sand surface
Software - Three-column example 2

Smooth surface
Software - Three-column example 3

Anti-slip grooved surface

T3810

Standard panel dimensions:
1220 mm, 915 mm wide; 3050 mm, 6100 mm long
Load-bearing flat bar: 25 mm
Open area: 38%

Approximate weight (including three-core strand): 11.8 kg/m²
Diagram showing concentrated line load on FRP grating T-3810

Pad load (unit: mm)

Spacing

kg/m

kg/m

kg/m

kg/m

kg/m

kg/m

Limit value

(mm)

300450750150030005950

Load

4500.711.021.733.456.91---8600
6001.552.343.897.75------6427
9004.837.21------------4180
120010.8---------------3018
Diagram showing uniformly distributed load on FRP grating T-3810

Uniform load (unit: mm)

Spacing

kg/m²

kg/m²

kg/m²

kg/m²

kg/m²

kg/m²

Limit value

(mm)

1000190039007000950019500

Load

4500.661.32.6256.53---37624
6001.963.897.77---------21087
9009.02---------------9158
12006.613------------9920

Features:

  • Flame retardant

  • High flame retardancy

  • Low smoke and low toxicity emissions

  • High strength-to-weight ratio

  • Corrosion resistant

  • Low maintenance

  • Anti-slip

  • Electrical and thermal non-conductive

  • Easy to fabricate

  • Impact resistance 

  • UV resistance

  • Maintenance-free

Installation and accessories

Installation and accessories

Application scenarios

Pultruded grating T-3810 is commonly used for industrial platforms, walkways, trench covers, stair treads and equipment operating surfaces that require load-bearing capacity and corrosion resistance. Because pultruded profiles are used as load-bearing bars, it is suitable for environments requiring long spans, light weight, high strength and resistance to chemical media, such as chemical processing, water treatment, electroplating and marine engineering. To confirm suitability for specific media and operating conditions, please contact us for detailed specifications and selection advice.

Selection guide

Selection should take into account the resin system, grating thickness, load-bearing bar spacing, load-bearing direction and installation support conditions. Different resin types differ in flame retardancy and corrosion resistance, and the matching resin grade should be selected according to the actual environment. We can provide selection guidance based on your load, span and media conditions; please contact us to discuss your specific requirements.

Product advantages

Pultruded grating is assembled from pultruded I/T profiles as load-bearing bars together with solid tubes or rods as connecting rods, combining high specific strength, light weight, corrosion resistance and ease of cutting and installation. Compared with conventional metal grating, it is insulating, non-magnetic and low in maintenance cost, making it suitable for long-term exposure to damp or corrosive environments. For more details on material composition and structural advantages, please contact us.

Inquiry guidance

For detailed specifications, load parameters, resin options and custom solutions for pultruded grating T-3810, please contact us. Please provide your operating environment, dimensional requirements and load requirements, and we will provide a quotation and technical support accordingly. All commercial terms are subject to the inquiry communication confirmed by both parties.

Operating environment

  • Pultruded FRP grating T-3810 is constructed from pultruded "I"-shaped or "T"-shaped profiles as load-bearing bars and solid tubes or rods as connecting rods, and is suitable for indoor and outdoor industrial platforms, walkways and tread boards.
  • The vinyl ester resin VEFR-25 used in this grating has an oxygen index of 28 or above, supporting use in damp or mildly corrosive environments with moisture and chemical exposure.
  • For fire-safety-critical locations with low-toxicity requirements, the MP-5 phenolic resin option can provide high flame retardancy, making the grating suitable for enclosed or high-risk process areas.
  • Please contact us for the complete parameter list to confirm resin selection and configuration according to your specific temperature, humidity and chemical exposure conditions.