拉挤格栅 T-2510

拉挤格栅 T-2510

¥ 1.00 1.0 CNY

¥ 1.00

Add To Cart


Please feel freely to contact with us for new price .

Genius FRP  

  Pultruded FRP grating is made of pultruded "I", "T" shaped profile as a bearing strip, with a solid pipe or bar as a connecting rod, made by a certain assembly process with a gap of the plate.  

Name

Contect

Type

Resin

25%

OFR-25、IFR-25、VEFR-25

Fiberglass

65%

E

Filler

8%

ATH、PR

Others

2%

---

Introduction of raw materials 
Resin type

Code

Resin type

Flame retardant property

Recommended usage occasions

MP-5

Phenolic type

Oxygen index can reach about 80

Low toxicity and high flame retardant, fire safety is very important for the occasion

VEFR-25

Vinyl type

Oxygen index 28 or above

Acid, alkali and other corrosive harsh environment

VEFR-10

Vinyl type

Oxygen index 35 or above

Flame retardant requirements of high acid, alkali and good occasions

IFR-25

Meta benzene

Oxygen index 28 or above

A VEFR type economy, and excellent, moderate acid alkali and solvent

IFGR-30

Benzene food grade

Oxygen index 26

Mainly used in meat products and food processing plants

OFR-25

Ortho type

Oxygen index 28 or above

General acid and alkali environment

OCR

Ortho type

Oxygen index below 28

OFR-25 economy, no flame retardant requirements

The type selection of coarse glass fiber   

Code

Coarse sand type

Recommended usage occasions

E

Non alkali sand

For high strength requirements and high corrosion resistance of the occasion

Selected filler type  

Code

Filler type

Recommended usage occasions

ATH

Aluminum hydroxide

Retardant, smoke suppression, corrosion-resistant occasions

PR

No filler, pure resin

For high corrosion-resistant applications

Software - Sample 1 for three columns

Sand surface
Software - Sample 2 for three columns

Smooth surface
Software - Sample 3 for three columns

Antiskid groove surface

T2510

Standard Panel Size:
1220mm,915mm-wide  3050mm,6100mm-length
Bearing Bar: 25mm
Open Area: 25%

Approx Weight (With three-core shoots): 13.6kg/m²
Liner load

Liner load(units:mm)

Spacing

kg/m

kg/m

kg/m

kg/m

kg/m

kg/m

Limit

(mm)

15030045075015003000

Load

4500.250.510.761.272.795.594619
6000.511.021.782.795.5911.43472
9001.783.565.599.14------2310
12002.034.328.3812.7------1728
Uniform load

Uniform load(units:mm)

Spacing

kg/m²

kg/m²

kg/m²

kg/m²

kg/m²

kg/m²

Limit

(mm)

4509501450240048509500

Load

4500.250.510.761.272.545.0810638
6000.761.522.033.567.11---8003
9003.566.8610.4---------5075
120010.7---------------2830

The characteristics:

  • Fire Retardant

  • High Flame Resistance

  • Low Smoke and Toxic Fume Emissions

  • High Strength-to-Weight Ratio

  • Corrosion Resistant

  • Low Maintenance

  • Slip Resistant

  • Electrically & Thermally Non-Conductive

  • Easily Fabricated

  • Impact Resistant 

  • UV resistance

  • Maintenance free

Installation and accessories  

Installation and accessories

应用场景

拉挤格栅 T-2510 常用于对承载与耐腐蚀同时有要求的平台、走道、地沟盖板及设备操作面等场合,尤其适合潮湿、酸碱或需减轻自重的工业环境。具体工况的适配性建议结合荷载、跨距与介质条件与我们沟通确认。

选型指导

选型时需重点考虑承载方向、支撑跨距、使用环境与阻燃要求,并根据树脂体系(如邻苯、间苯、乙烯基或酚醛型)选择对应耐蚀与防火等级。欢迎联系我们提供工况参数,由技术人员协助完成规格匹配与选型建议。

产品优势

以拉挤“I”“T”型材作承力条、实心管或棒作连接杆组装而成,具有轻质高强、耐腐蚀、易切割安装及维护成本低等特点,且表面可做防滑处理。相比传统金属格栅,其在腐蚀性环境中使用寿命更长,且不导电、无磁性。

询盘引导

如需获取 T-2510 的详细规格、树脂体系选项、承载数据及报价,欢迎联系我们,我们将根据您的项目需求提供针对性方案与商业条款。