  FRP pultruded profiles are a new composite material made with fiberglass reinforcement as the base material, resin as the adhesive, and fiberglass cloth as the wrapping reinforcement layer; after full impregnation, the material is heated, formed, and cured in a metal mold and pulled by a pulling machine. With good physical properties, they are widely used in high-strength and long-span applications.  

FRP fiberglass H-beam structural profile with flanges and web

Type

Size (mm)

Weight (kg/m)

Size (in)

Weight (lbs/in)

H-beam

A*B*T1*T2


A*B*T1*T2


HB7676*76*6.4*6.42.672.99*2.99*0.25*0.255.73
HB102A102*102*6.4*6.43.594.02*4.02*0.25*0.257.91
HB102B102*102*8*84.54.02*4.02*0.31*0.319.92
HB152A152*152*6.4*6.45.435.98*5.98*0.25*0.2511.97
HB152B152*152*9.5*9.58.15.98*5.98*0.37*0.3717.86
HB203A203*203*9.5*9.510.87.99*7.99*0.37*0.3723.81
HB203B203*203*12.7*12.714.47.99*7.99*0.5*0.531.66
HB203C203*203*6.4*6.47.57.99*7.99*0.25*0.2516.53
HB254A254*254*9.5*9.513.610*10*0.37*0.3729.98
HB254B254*254*12.7*12.71810*10*0.5*0.539.77
HB305305*305*12.7*12.721.512.01*12.01*0.5*0.547.4

Market  

FRP H-beam applications in construction, bridges and highways

  • Construction

  • Bridges and highways

  • Chemical

  • Food and beverage

  • Manufacturing

  • Metals and mining

  • Microelectronics

  • Oil and gas

  • Pharmaceutical

  • Power

  • Pulp and paper

  • Recreation

  • Telecommunications

  • Transportation

  • Water and wastewater treatment

Features:

  • Corrosion resistance

  • Low maintenance

  • Flame retardant

  • Low installation cost

  • Resistant to heavy metal corrosion

  • Long service life

  • Non-conductive and non-thermally conductive

  • High strength-to-weight ratio

Raw material introduction — resin types

Code

Resin type

Flame retardant performance

Standard colors

Recommended applications

VEFR-25

Vinyl ester type

Oxygen index 28 and above

Grass green, yellow, gray, orange

Acid, alkali and other harsh corrosive environments

IFR-25

Isophthalic type

Oxygen index 28 and above

Grass green, yellow, gray

VEFR economical type, with good, moderate resistance to acids, alkalis and solvents

OFR-25

Orthophthalic type

Oxygen index 28 and above

Grass green, yellow, gray

General acid and alkali environments

Applications:

  Greenlogy TEC pultruded FRP structural profiles are widely used in various applications, combining corrosion resistance, high strength, dimensional stability and light weight, with thermal insulation and non-conductive properties. Durable Greenlogy TEC profiles provide years of low-maintenance service in areas where steel, aluminum or timber members have traditionally been specified. Today these profiles are often used in highly corrosive environments where stainless steel and other costly components were previously required.  

Greenlogy TEC Profiles

Mechanical Properties

ASTM

Unit

Value

Unit

Value

Tensile stress, longitudinal

D-638

psi

30000

kgf/m²

21092086

Tensile stress, transverse

D-638

psi

7000

kgf/m²

4921487

Tensile modulus, longitudinal

D-638

10^6psi

2.5

10^6kgf/m²

1758

Tensile modulus, transverse

D-638

10^6psi

0.8

10^6kgf/m²

562

Compressive stress, longitudinal

D-695

psi

30000

kgf/m²

21092086

Compressive stress, transverse

D-695

psi

15000

kgf/m²

10546043

Compressive modulus, longitudinal

D-695

10^6psi

2.5

10^6kgf/m²

1758

Compressive modulus, transverse

D-695

10^6psi

1

10^6kgf/m²

703

Flexural stress, longitudinal

D-790

psi

30000

kgf/m²

21092086

Flexural stress, transverse

D-790

psi

10000

kgf/m²

7030695

Flexural modulus, longitudinal

D-790

10^6psi

1.8

10^6kgf/m²

1266

Flexural modulus, transverse

D-790

10^6psi

0.8

10^6kgf/m²

562

Modulus of elasticity

Full section

10^6psi

2.8

10^6kgf/m²

1969

Shear modulus

---

10^6psi

0.45

10^6kgf/m²

316

Short-beam shear

D-2344

psi

4500

kgf/m²

3163813

Punch shear

D-732

psi

10000

kgf/m²

7030695

Notched Izod impact, LW

D-256

ft.-lbs./in.

25

kg/m

3.46

Notched Izod impact, CW

D-256

ft.-lbs./in.

4

kg/m

0.55

  Excluding round bars and square bars

Physical properties

ASTM

Unit

Value

Barcol hardness

D-495

---

45

24-hour water absorption

D-570

% max

0.45

Density

D-792

lbs./in.³

0.062-0.07

Coefficient of thermal expansion, LW

D-696

10^-6in./in./℃

8

Flame retardant performance

ASTM

Unit

Value

Tunnel test*

E-84

Flame spread

Max. 25

Flame retardancy*

D-635

---

Non-combustible

Electrical properties

ASTM

Unit

Value

Arc resistance, LW

D-495

秒(s)

120

Dielectric strength, LW

D-149

kv./in.

35

Dielectric strength, PF

D-149

Volt/mil

200

Dielectric constant, PF

D-150

@60hz

5

LW = lengthwise, CW = crosswise, PF = perpendicular to laminate surface

*Applies to ISOFR and VEFR only


Applications

FRP H-beams are commonly used in load-bearing structures requiring strength, corrosion resistance and electrical insulation, such as platform frames, walkway supports, cable trays, and beam and column members in corrosive environments including chemical, water treatment and marine applications. Their lightweight, high-strength characteristics suit long spans and applications requiring reduced maintenance. Contact us for detailed specifications and quotations.

Selection Guide

When selecting, evaluate span, load conditions, installation method and service environment together against the A×B×T1×T2 cross-section dimensions and unit weight. If you are unsure of the right specification, contact us and our technical team will help confirm detailed specifications and quotations.

Product Advantages

FRP H-beams are pultruded from glass fiber reinforcement and resin, offering lightweight, high strength, corrosion resistance, electrical insulation and ease of cutting and installation, which helps reduce later maintenance. Compared with traditional metal profiles, they are better suited to harsh environments such as damp, acid and alkaline conditions. Contact us for detailed specifications and quotations.

Inquiry

For information on FRP H-beam cross-section specifications, lengths, colors and matching connection solutions, please contact us and we will provide detailed specifications and quotations based on your project requirements. Please let us know your service environment and quantity so we can respond faster.

Service Environment

  • These FRP H-beams are suitable for indoor and outdoor structural applications, where the glass fiber reinforced resin matrix resists water and moisture without the corrosion problems that affect steel.
  • Typical service conditions include chemical plants, wastewater treatment facilities, cooling towers and coastal installations, where pultruded H-beams can withstand corrosive media, salt spray and industrial flue gas.
  • Composite structures also perform normally under the temperature conditions commonly found in industrial processing areas, retaining their shape and load-bearing function where metal profiles may expand, rust or require frequent painting.
  • For outdoor walkways, platforms and handrail frames, the UV-resistant resin system and non-conductive properties of H-beams help them operate reliably in wet and dry environments; please contact us to discuss your specific service conditions.

Custom Cutting

Need panels that fit, or cut to shape? We custom cut FRP grating and profiles to your drawing: panels cut to size or to shape (corner cuts, cutouts), cut edges sealed with resin, and pre-cut and pre-drilled to drawing before shipping. See the custom cutting services.

WhatsApp