LM Marine Grade stainless steel Wire Rope GB6x36 (14/7+7/7/1) IWRC

LM Marine Grade stainless steel Wire Rope GB6x36 (14/7+7/7/1) IWRC

¥ 1.00 1.0 CNY

¥ 1.00

Add To Cart


Please feel freely to contact with us for new price .

Product Details

6x36 is the most flexible of our stainless steel wire ropes. It is available with either FC (fibre core) or IWRC (independent wire rope core) ,having a superior breaking load and a good fatigue life.6x36 stainless steel wire ropes are often used for larger diameter stainless steel slings as well as for general engineering applications.

Surface treatment:Ungalv  or  Galvanized

Standard:GB/T 20118-2006

LM Marine Grade stainless steel Wire Rope GB6x36 (14/7+7/7/1) IWRC

Applications

  • Marine crane rope

  • Luffing ropes

  • Lifeboat falls

  • Davit ropes

  • Large diameter stainless steel wire rope slings

  • Marine/Saltwater environment

  • Sewage treatment works

Breaking Loads 

Diameter

Weight 

Min Breaking Loads(1570Mpa)

Min Breaking Loads(1570Mpa)

mm

kg/m

KN

Kg

80.2835.83651
90.3545.34620
100.4355.95701
110.5467.66895
120.6280.58211
140.8411011169
161.114314596
181.3918118462
201.7222422848
222.1627127642
242.4832232844
262.7637838515
283.3743844676
303.8750351306
324.4157258344

General Engineering Ropes

  GREENLOGY TEC(LM) specializes in supplying multiple strands of  ungalvanised and galvanized steel wire ropes. Our products range from 0.5mm to 64mm, including 1X19, 7X7, 6X19, 7X19, 6X36, 8X19, 8X36, 19X7 and 35X7 with both Fibre Core and Steel Cores. In addition to these conventional steel wire ropes, we can also provide high-quality special steel wire ropes.

   Most wire ropes are used in harsh conditions and must have resistance to extrusion, bending fatigue and abrasion. All of our wire ropes are guaranteed to achieve the highest level , maximizing the service life to increase the productivity of end users. We ensure that all materials are produced in accordance with the best standards in the wire rope industry. Each wire rope can be supplied with a thimble eyes, swaged ends and wedge sockets ,as well as many other assembly components.In addition, we also provide customized services, our team of engineers can manufacture wire ropes of your required specifications. All materials are certified, traceable, and comply with ISO9001 standards.


选型指导

请根据实际使用场景确认所需结构(如6x36 FC纤维芯或IWRC独立钢丝绳芯)、公称直径、表面处理(光面或镀锌)及强度等级。若您不确定具体规格,欢迎将工况条件告知我们,由技术人员协助推荐合适型号。

产品优势

该结构钢丝绳柔韧性好,具备良好的抗疲劳性能与断裂载荷能力,适用于船用起重机、变幅绳、救生艇及海水环境等场景。光面或镀锌表面处理可满足不同海洋防腐蚀需求。

询盘引导

如需了解库存、价格、起订量或交期等商务信息,欢迎联系我们获取详细规格与报价。请提供所需直径、芯型、表面处理及数量,以便我们快速响应。

Free,easy click for support

7*24 professional team support. Within 24 Hours, our team will give you the feedback.

Send   
 Website Visitor