LM Compacted Wire Rope GB6x36 (14/7+7/7/1) FC
Request a Quote
Please feel freely to contact with us for new price .
Product Details
6x36 wire rope is available with FC (fiber core) or IWRC (independent wire rope core), and is a general-purpose flexible engineering wire rope. This wire rope offers superior breaking load capacity and good fatigue resistance, with a long service life and wide range of applications.
Surface finish: bright or galvanized
Standard: GB/T 20118-2006

Engineering Applications
General engineering applications
Grab crane ropes
Wire rope slings
Crane ropes
Slings
Winch ropes
Lifeboat ropes
Mooring ropes
Search ropes
Luffing ropes
Traction ropes
Breaking load
|
|
Minimum breaking load |
Minimum breaking load |
Minimum breaking load | Minimum breaking load |
|---|---|---|---|---|---|
Diameter | Weight |
(1770Mpa) |
(1770Mpa) |
(1960Mpa) |
(1960Mpa) |
mm | kg/m | KN | Kg | KN | Kg |
| 8 | 0.24 | 37.4 | 3813 | 41.4 | 4222 |
| 9 | 0.3 | 47.3 | 4825 | 52.4 | 5343 |
| 10 | 0.37 | 58.4 | 5957 | 64.7 | 6597 |
| 11 | 0.44 | 70.7 | 7208 | 78.3 | 7982 |
| 12 | 0.53 | 84.1 | 8579 | 93.1 | 9500 |
| 14 | 0.72 | 114 | 11677 | 127 | 12930 |
| 16 | 0.94 | 150 | 15252 | 166 | 16889 |
| 18 | 1.19 | 189 | 19303 | 210 | 21375 |
| 20 | 1.47 | 234 | 23831 | 259 | 26389 |
| 22 | 1.78 | 283 | 28835 | 313 | 31931 |
| 24 | 2.11 | 336 | 34317 | 373 | 38000 |
| 26 | 2.48 | 395 | 40274 | 437 | 44598 |
| 28 | 2.88 | 458 | 46709 | 507 | 51723 |
| 30 | 3.3 | 526 | 53620 | 582 | 59376 |
| 32 | 3.76 | 598 | 61008 | 662 | 67556 |
| 34 | 4.24 | 675 | 68872 | 748 | 76265 |
| 36 | 4.76 | 757 | 77213 | 838 | 85501 |
| 38 | 5.3 | 843 | 86030 | 934 | 95265 |
| 40 | 5.87 | 935 | 95325 | 1035 | 105557 |
| 42 | 6.47 | 1030 | 105095 | 1141 | 116377 |
| 44 | 7.11 | 1131 | 115343 | 1252 | 127724 |
| 46 | 7.77 | 1236 | 126067 | 1369 | 139600 |
| 48 | 8.46 | 1346 | 137268 | 1490 | 152003 |
| 50 | 9.18 | 1460 | 148945 | 1617 | 164934 |
| 52 | 9.92 | 1579 | 161099 | 1749 | 178392 |
| 56 | 11.5 | 1832 | 186837 | 2020 | 206893 |
| 60 | 13.2 | 2103 | 214481 | 2328 | 237504 |
General-purpose engineering wire rope
Greenlogy TEC LM specializes in supplying multi-strand bright or galvanized wire rope. Our products range in diameter from 0.5 mm to 64 mm, including 1X19, 7X7, 6X19, 7X19, 6X36, 8X19, 8X36, 19X7 and 35X7 specifications with fiber cores and steel cores. In addition to these standard wire ropes, we can also supply high-quality special wire ropes.
Most wire ropes work under demanding conditions and must possess resistance to crushing, bending fatigue, and abrasion. All our wire ropes are designed to achieve a high level of performance to extend service life and thereby improve end-user productivity. We therefore ensure that all materials are produced in accordance with wire rope industry standards. Each wire rope can be supplied with assembly components such as thimbles, swaged ends, and wedge sockets, as well as many other fittings. In addition, we offer customization services: our engineering team can manufacture wire ropes to the specifications you require. All materials are certified, traceable, and comply with ISO9001.
Selection Guide
This product is a 6x36 compacted strand wire rope (14/7+7/7/1), supplied with fiber core (FC) as standard; independent wire rope core (IWRC) is also available. Please specify your requirement when ordering. Please select according to your actual working conditions, including diameter, lay direction, tensile strength grade, and surface finish (bright or galvanized). If you need assistance with selection, please contact us for detailed specifications and a quotation.
Product Advantages
The 6x36 structure gives this wire rope good flexibility and fatigue resistance, with excellent breaking load capacity, and the compacted strand process further enhances wear resistance and service life. It is suitable for applications involving frequent bending and alternating loads, making it a reliable choice for general engineering, lifting, and sling applications.
Inquiry Guide
For detailed information such as specific diameter, lay direction, tensile strength grade, surface finish, packaging, and transportation, please contact us for detailed specifications and a quotation. We will provide professional selection advice and commercial support according to your working conditions.
Operating Environment
- This LM Compacted Wire Rope GB6x36 (14/7+7/7/1) FC, with its fiber core and compacted strand construction, is suited to general engineering applications in both indoor and outdoor environments, including workshops, yards and construction sites.
- The fiber core makes this wire rope suitable for use in ambient temperature ranges typical of general lifting and pulling operations; for high-temperature or specialized conditions, please contact us for application-specific guidance.
- Available in bright or galvanized finish, this wire rope can be selected for use in humid, mildly corrosive or outdoor environments according to the level of protection required; the galvanized option is intended for applications where additional corrosion resistance is beneficial.
- As a general-purpose flexible wire rope, it is employed in crane ropes, winch ropes, slings, mooring ropes and similar duties; for use in highly corrosive media or extreme environments, please consult us for the most suitable finish and construction.
Cut to Length
Need rope in fixed lengths? We cut wire rope to your required segment lengths before delivery (e.g. 5 m x 4 pcs + 10 m x 2 pcs), with end treatment per your needs. Request cut-to-length rope.