LM Sealed Wire Rope GB6X19(9/9/1) FC
Please feel freely to contact with us for new price .
产品详情
6x19 sealed construction is a wire rope construction with superb breaking load characteristics and is used in a wide range of applications, available with both FC (fibre core) and IWRC (independent wire rope core). For applications that require higher wear resistance, 6x19 sealed wire ropes are more suitable than other 6x19 wire ropes.
Surface treatment:Ungalv or Galvanized
Standard:GB/T 20118-2006
.jpg?access_token=4fe5d99f-b4e6-443b-8e1c-c51ba327cdbb)
Applications
Drilling ropes
Elevator rope
Wire rope slings
Derricking ropes
Pendant ropes
Crane rope
Sand, coring and swabbing lines
Trawl wraps / Pelagic sweeps
Ground cables
Oil well / Oil field
Excavator rope / Scraper rope
Fishing rope
Drag ropes
Breaking Loads
|
|
Min Breaking Loads |
Min Breaking Loads |
Min Breaking Loads | Min Breaking Loads |
Diameter | Weight |
(1770Mpa) |
(1770Mpa) |
(1960Mpa) |
(1960Mpa) |
mm | kg/m | KN | Kg | KN | Kg |
| 10 | 0.36 | 58.4 | 5957 | 64.7 | 6597 |
| 11 | 0.43 | 70.7 | 7209 | 78.3 | 7982 |
| 12 | 0.52 | 84.1 | 8579 | 93.1 | 9500 |
| 13 | 0.61 | 98.7 | 10068 | 109 | 11149 |
| 14 | 0.7 | 115 | 11677 | 127 | 12930 |
| 16 | 0.92 | 150 | 15252 | 166 | 16889 |
| 18 | 1.16 | 189 | 19303 | 210 | 21375 |
| 20 | 1.44 | 234 | 23831 | 259 | 26389 |
| 22 | 1.74 | 283 | 28835 | 313 | 31931 |
| 24 | 2.07 | 336 | 34317 | 373 | 38000 |
| 26 | 2.43 | 395 | 40274 | 437 | 44598 |
| 28 | 2.82 | 458 | 46709 | 507 | 51723 |
| 30 | 3.23 | 526 | 53620 | 582 | 59376 |
| 32 | 3.68 | 598 | 61008 | 662 | 67557 |
| 34 | 4.15 | 675 | 68872 | 748 | 76265 |
| 36 | 4.65 | 757 | 77213 | 838 | 85501 |
| 38 | 5.18 | 843 | 86030 | 934 | 95265 |
| 40 | 5.74 | 935 | 95235 | 1035 | 105557 |
| 42 | 6.33 | 1030 | 105095 | 1141 | 116377 |
General Engineering Ropes
GREENLOGY TEC(LM) specializes in supplying multiple strands of ungalvanised and galvanized steel wire ropes. Our products range from 0.5mm to 64mm, including 1X19, 7X7, 6X19, 7X19, 6X36, 8X19, 8X36, 19X7 and 35X7 with both Fibre Core and Steel Cores. In addition to these conventional steel wire ropes, we can also provide high-quality special steel wire ropes.
Most wire ropes are used in harsh conditions and must have resistance to extrusion, bending fatigue and abrasion. All of our wire ropes are guaranteed to achieve the highest level , maximizing the service life to increase the productivity of end users. We ensure that all materials are produced in accordance with the best standards in the wire rope industry. Each wire rope can be supplied with a thimble eyes, swaged ends and wedge sockets ,as well as many other assembly components.In addition, we also provide customized services, our team of engineers can manufacture wire ropes of your required specifications. All materials are certified, traceable, and comply with ISO9001 standards.
选型指导
选型时可根据实际工况确认所需直径、公称抗拉强度等级、表面处理(光面或镀锌)以及是否需要纤维芯(FC)或独立钢丝绳芯(IWRC)等配置。不同芯型与强度等级对应的载荷表现存在差异,欢迎联系我们获取详细规格与报价。
产品优势
该产品符合 GB/T 20118-2006 标准,采用密封结构设计,在需要更高耐磨性的应用场景下相较其他 6x19 钢丝绳更具适应性。光面或镀锌表面处理可满足不同环境的使用需求,欢迎联系我们了解具体配置与适用建议。
询盘引导
如需确认规格、芯型与表面处理等配置,欢迎联系我们获取详细规格与报价。我们将根据您的应用场景提供相应的选型建议与技术支持。
简体中文
English