The core of 6X19 filler wire rope (often referred to as 6x25) includes FC (fiber core) and IWRC (independent wire rope core). 6X19 filler wire rope can bear loads of 1T-5T and is used as wire rope slings. This structure is widely used in North Sea oil industry.

Surface treatment: bright or galvanized

Standard: GB/T 20118-2006

Greenlogy TEC GB Filler Wire Rope 6X19(12/6+6F/1) IWRC

Engineering applications

  • Drilling line

  • Elevator hoist rope

  • Wire rope slings

  • Luffing wire rope

  • Hoisting rope

  • Crane wire rope


  • Sand line, core line and swabbing line

  • Trawling / ocean sweep

  • Ground rope / ground drag rope

  • Oil well / oilfield

  • Excavator rope / scraper rope

  • Fishing rope

  • Tow rope

Breaking load

Minimum breaking load

Minimum breaking load

Minimum breaking load

Minimum breaking load


Diameter

Weight

(1770Mpa)

(1770Mpa)

(1770Mpa)

(1960Mpa)

mm

kg/m

KN

Kg

KN

Kg

140.781241259713713949
161.021611645317918219
181.32042082422623059
201.62522570827928468
221.943053110733834447
242.33633702040240994
262.74264344847248111
283.144945038954755798
303.65675784562864054
324.16456581471572879
344.627287429880782274
365.188178329690492238
385.78910928091008102771
406.410081028351116113874
427.0611121133761231125546
447.7412201244311351137788
468.4613331360001477150598
489.2214521480831608163979

General Engineering Wire Rope

   Greenlogy TEC (LM) specializes in supplying multi-strand bright or galvanized wire rope. Our products range in diameter from 0.5mm to 64mm, including 1X19, 7X7, 6X19, 7X19, 6X36, 8X19, 8X36, 19X7 and 35X7 specifications with fiber core and steel core. In addition to these conventional wire ropes, we can also supply premium specialty wire ropes.

Most wire ropes work under demanding conditions and must possess resistance to crushing, bending fatigue and abrasion. All our wire ropes strive to achieve a high level of performance to extend service life and thereby improve end-user productivity. We therefore ensure that all materials are produced in accordance with wire rope industry standards. Each wire rope can be supplied with fittings such as thimbles, swaged ends and wedge sockets as well as many other assembly components. We also offer customization services; our engineering team can manufacture wire ropes to your required specifications. All materials are certified, traceable and compliant with ISO9001.


Selection Guide

When selecting, please consider factors such as the equipment's rated load, sheave or drum diameter, operating environment (e.g. humid, corrosive or outdoor) and whether a galvanized surface finish is required, to determine the wire rope diameter and core type (FC or IWRC). The diameter ranges and load grades listed on this page are for preliminary reference. For matching recommendations for specific working conditions, please contact us for technical selection support.

Product Advantages

6X19 filler wire rope is available with a fiber core or independent wire rope core structure, balancing flexibility and load-bearing capacity, with a bright or galvanized surface finish, suitable for applications such as drilling lines, elevator lifting, slings and oilfields. The product is manufactured in accordance with GB/T 20118-2006; performance parameters for specific batches are subject to actual testing and contractual agreement. Please contact us to confirm detailed specifications.

Inquiry Guide

For information on this product's diameter specifications, surface finish, packaging and bulk supply arrangements, please contact us for detailed specifications and quotations. Please provide information such as the application scenario, required diameter and quantity before ordering, and we will arrange further communication on samples and commercial terms according to your needs.