32X7 is available in both galvanised and ungalvanised finish with either ordinary or langs lay. The construction family includes: 34X7, 35X7 and 37X7.

Surface treatment:Ungalv  or  Galvanized

Standard:GB/T 20118-2006

LM Rotation Resistant Wire Rope GB 32X7 (6/1)

Applications

  • Offshore crane rope

  • Deck crane rope

  • Pillar crane rope

  • Whip hoist rope

  • Main hoist rope

  • Crane rope

Breaking Loads  

Min Breaking Loads 

Min Breaking Loads

Diameter

Weight 

(1770Mpa) 

 (1770Mpa)

mm

kg/m

KN

Kg

80.2945.24606
90.3757.25829
100.4570.67197
110.5585.48708
120.6510210363
130.7711912163
140.8913814106
151.0215916193
161.1618118424
181.4722923318
191.6425525981
201.8228228788
222.234234834
242.6240641455

General Engineering Ropes

   绿盟(LM)专门供应多股光面或镀锌钢丝绳。我们的产品直径从0.5mm到64mm不等,包括带纤维芯和钢芯的1X19、7X7、6X19、7X19、6X36、8X19、8X36、19X7和35X7各种规格。除这些常规钢丝绳外,我们还可以提供优质的特种钢丝绳。

   Most wire ropes are used in harsh conditions and must have resistance to extrusion, bending fatigue and abrasion. All of our wire ropes are guaranteed to achieve the highest level , maximizing the service life to increase the productivity of end users. We ensure that all materials are produced in accordance with the best standards in the wire rope industry. Each wire rope can be supplied with a thimble eyes, swaged ends and wedge sockets ,as well as many other assembly components.In addition, we also provide customized services, our team of engineers can manufacture wire ropes of your required specifications. All materials are certified, traceable, and comply with ISO9001 standards.


选型指导

LM 旋转抗扭钢丝绳 GB 32X7(6/1)适用于需要抗旋转性能的起重与吊装场景。选型时请结合工况的载荷、滑轮组配置、弯曲频率与腐蚀环境,确认所需直径、芯型(纤维芯或钢芯)及表面处理(光面或镀锌)。如需针对具体项目推荐合适规格,欢迎联系我们获取详细规格与报价。

产品优势

该结构通过股绳与绳芯的捻向配合,有助于在单绳吊装时减少旋转倾向,提升操作稳定性。光面或镀锌表面可适应不同腐蚀环境,并可按需提供纤维芯或钢芯版本。绿盟(LM)可供应多种常规及特种钢丝绳,满足不同工程需求。

询盘引导

如需了解 LM 旋转抗扭钢丝绳 GB 32X7(6/1)的可用直径、芯型、表面处理及包装方式,欢迎联系我们获取详细规格与报价。请提供您的工况参数与所需数量,我们将协助您确认合适的产品方案。

Free,easy click for support

7*24 professional team support. Within 24 Hours, our team will give you the feedback.

Send   
 Website Visitor