LM Wire Rope GB 1X19(12/6/1)

LM Wire Rope GB 1X19(12/6/1)

¥ 1.00 1.0 CNY

¥ 1.00

Add To Cart


Please feel freely to contact with us for new price .

Product Details

1x19 galvanised steel strand’s excellent breaking load and low stretch characteristics along with its’ aesthetic appeal make it a favourite for small diameter applications.

Surface treatment:Ungalv  or  Galvanized

Standard:GB/T 20118-2006

LM Wire Rope GB 1X19(12/6/1)

Applications  

  • General engineering applications 

  • Small diameter wire rope slings

  • Stay wires

  • Fencing rope

  • Catenary wires

  • Garage door cables

  • Standing rigging

  • Hanging signs

  • Ski-lifts

Breaking Loads 

 

  Min Breaking Loads

Min Breaking Loads

  Min Breaking Loads

Min Breaking Loads


 Diameter

Weight 

     (1770Mpa)

    (1770Mpa)

   (1960Mpa)

   1960Mpa)

mm

kg/m

KN

Kg

KN

Kg

10.0050.93951.03105
1.20.0071.341361.48151
1.50.012.092132.32236
1.80.0163.013073.33340
20.023.723794.12420
2.30.0264.925015.44555
2.50.035.815926.43656
30.058.368539.26944
40.0814.9151616.51678
50.1223.2236825.72622
60.1833.53410373776
70.2445.5464250.45140
80.3259.5606265.96713
90.475.3767383.38496
100.592.9947210310489
110.61121146212512692
120.711341364014815105
140.971821856620220559
161.272382425026326853
191.793353419637137866
222.44504584749850768
263.356286403469670908

 General Engineering Ropes

       GREENLOGY TEC(LM) specializes in supplying multiple strands of  ungalvanised and galvanized steel wire ropes. Our products range from 0.5mm to 64mm, including 1X19, 7X7, 6X19, 7X19, 6X36, 8X19, 8X36, 19X7 and 35X7 with both Fibre Core and Steel Cores. In addition to these conventional steel wire ropes, we can also provide high-quality special steel wire ropes.

    Most wire ropes are used in harsh conditions and must have resistance to extrusion, bending fatigue and abrasion. All of our wire ropes are guaranteed to achieve the highest level , maximizing the service life to increase the productivity of end users. We ensure that all materials are produced in accordance with the best standards in the wire rope industry. Each wire rope can be supplied with a thimble eyes, swaged ends and wedge sockets ,as well as many other assembly components.In addition, we also provide customized services, our team of engineers can manufacture wire ropes of your required specifications. All materials are certified, traceable, and comply with ISO9001 standards.


选型指导

1x19结构钢丝绳刚性较高、破断荷载大且拉伸低,适用于对尺寸稳定性要求高的吊索、支索和固定拉索等场景。选型时请结合所需直径、表面处理(光面或镀锌)及实际工况的破断荷载要求综合判断,欢迎联系我们获取详细规格与选型建议。

产品优势

1x19镀锌钢丝绳外观美观,兼具优异的断裂荷载能力和低拉伸特性,是小直径钢丝绳中较受欢迎的结构形式。其致密的股结构在承受较高拉力时变形小,适合建筑、索具及各类固定支撑用途。

询盘引导

如需特定直径、表面处理或批量供应,欢迎联系我们获取详细规格与报价。请提供所需直径、表面处理方式及用途等信息,我们将据此为您推荐合适的产品并回复商业条款。