LM Stainless Steel Wire Rope GB1X19 (12/6/1)
Please feel freely to contact with us for new price .
Product Details
1X19 stainless steel strand is a very popular stainless steel construction. Used heavily throughout the marine industry, 1X19’s excellent breaking load and low stretch characteristics along with its aesthetic appeal makes it a favourite for marine, structural and balustrade applications as well as many others.
Surface treatment:Ungalv or Galvanized
Standard:GB/T 20118-2006

Applications
Balustrades
Standing rigging
Mast stays
Guardrail
Structural
Stay wires
Marine/Saltwater environment
Sewage treatment work
Breaking Loads
Diameter
| Weight
|
Min Breaking Loads(1570Mpa)
|
Min Breaking Loads(1570Mpa)
|
mm | kg/m | KN |
Kg |
| 4 | 0.09 | 14.5 | 1479 |
| 5 | 0.14 | 23.9 | 2438 |
| 6 | 0.2 | 34.8 | 3550 |
| 7 | 0.27 | 48.2 | 4916 |
| 8 | 0.35 | 60.3 | 6151 |
| 9 | 0.44 | 73.5 | 7497 |
| 10 | 0.55 | 95.8 | 9772 |
| 11 | 0.66 | 110 | 11220 |
| 12 | 0.79 | 141 | 14382 |
General Engineering Ropes
GREENLOGY TEC(LM) specializes in supplying multiple strands of ungalvanised and galvanized steel wire ropes. Our products range from 0.5mm to 64mm, including 1X19, 7X7, 6X19, 7X19, 6X36, 8X19, 8X36, 19X7 and 35X7 with both Fibre Core and Steel Cores. In addition to these conventional steel wire ropes, we can also provide high-quality special steel wire ropes.
Most wire ropes are used in harsh conditions and must have resistance to extrusion, bending fatigue and abrasion. All of our wire ropes are guaranteed to achieve the highest level , maximizing the service life to increase the productivity of end users. We ensure that all materials are produced in accordance with the best standards in the wire rope industry. Each wire rope can be supplied with a thimble eyes, swaged ends and wedge sockets ,as well as many other assembly components.In addition, we also provide customized services, our team of engineers can manufacture wire ropes of your required specifications. All materials are certified, traceable, and comply with ISO9001 standards.
选型指导
选型时请先确认使用场景的载荷要求、腐蚀环境及结构连接方式,再据此确定钢丝绳的直径、结构(如 1x19、7x7、6x19 等)与表面处理(光面或镀锌)。不同直径与结构对应不同的最小断裂荷载,建议以实际工况参数为准。欢迎联系我们获取详细规格与报价,我们可协助您完成选型。
产品优势
LM 不锈钢钢丝绳采用 1x19 结构,具备高断裂荷载与低拉伸性,适合对尺寸稳定性要求较高的固定索具与结构支撑。产品可按需提供光面或镀锌表面处理,兼顾耐腐蚀与外观需求。依托绿盟在钢丝绳领域的供应经验,我们可提供多规格常规产品及特种钢丝绳选项。
询盘引导
如需了解具体直径、结构、表面处理或批量供货方案,欢迎联系我们获取详细规格与报价。请提供使用场景、所需直径及数量等信息,以便我们为您推荐合适的产品。我们期待与您沟通并支持您的项目需求。