LM (Coating) Wire Rope GB6X37.IWRC
Please feel freely to contact with us for new price .
Product Details
6x37 is a cross laid construction used for general engineering applications. 6x37 is also available with IWRC (independent wire rope core). In the UK 6x36 is a far more popular construction, whilst on the European mainland, vast quantities of 6x37 are used for a variety of applications.。
Surface treatment:Ungalv or Galvanized
Standard:GB/T 20118-2006

Applications
General engineering applications
Crane ropes
Hoist rope
Breaking Loads
|
|
Min Breaking Loads |
Min Breaking Loads |
Min Breaking Loads | Min Breaking Loads |
Diameter | Weight |
(1770Mpa) |
(1770Mpa) |
(1960Mpa) |
(1960Mpa) |
mm | kg/m | KN | Kg | KN | Kg |
| 12 | 0.55 | 81.3 | 8293 | 90 | 9183 |
| 13 | 0.64 | 95.4 | 9733 | 106 | 10777 |
| 14 | 0.75 | 111 | 11288 | 123 | 12499 |
| 16 | 0.98 | 145 | 14743 | 160 | 16326 |
| 18 | 1.23 | 183 | 18659 | 203 | 20662 |
| 20 | 1.52 | 226 | 23036 | 250 | 25509 |
| 22 | 1.84 | 273 | 27874 | 302 | 30866 |
| 24 | 2.2 | 325 | 33173 | 360 | 36734 |
| 26 | 2.58 | 382 | 38932 | 423 | 43111 |
| 28 | 2.99 | 443 | 45152 | 490 | 49999 |
| 30 | 3.43 | 508 | 51833 | 563 | 57397 |
| 32 | 3.9 | 578 | 58974 | 640 | 65305 |
| 34 | 4.4 | 653 | 66576 | 723 | 73723 |
| 36 | 4.94 | 732 | 74639 | 810 | 82651 |
| 38 | 5.5 | 815 | 83163 | 903 | 92090 |
| 40 | 6.1 | 903 | 92147 | 1000 | 102039 |
| 42 | 6.72 | 996 | 101592 | 1103 | 112498 |
| 44 | 7.38 | 1093 | 111498 | 1211 | 123467 |
| 46 | 8.06 | 1195 | 121865 | 1323 | 134946 |
| 48 | 8.78 | 1301 | 132692 | 1441 | 146936 |
General Engineering Ropes
GREENLOGY TEC(LM) specializes in supplying multiple strands of ungalvanised and galvanized steel wire ropes. Our products range from 0.5mm to 64mm, including 1X19, 7X7, 6X19, 7X19, 6X36, 8X19, 8X36, 19X7 and 35X7 with both Fibre Core and Steel Cores. In addition to these conventional steel wire ropes, we can also provide high-quality special steel wire ropes.
Most wire ropes are used in harsh conditions and must have resistance to extrusion, bending fatigue and abrasion. All of our wire ropes are guaranteed to achieve the highest level , maximizing the service life to increase the productivity of end users. We ensure that all materials are produced in accordance with the best standards in the wire rope industry. Each wire rope can be supplied with a thimble eyes, swaged ends and wedge sockets ,as well as many other assembly components.In addition, we also provide customized services, our team of engineers can manufacture wire ropes of your required specifications. All materials are certified, traceable, and comply with ISO9001 standards.
选型指导
LM(涂层)钢丝绳 GB6X37.IWRC 适用于通用工程、起重与吊索等场景,选型时请根据实际工况确认直径、表面处理(光面或镀锌)及所需最小断裂荷载等级。不同直径对应不同的重量与承载能力,建议结合设备轮槽尺寸、安全系数和使用频率综合评估。欢迎联系我们获取详细规格与选型建议。
产品优势
该产品采用 6x37 结构并可选 IWRC(独立钢丝绳芯),柔韧性与耐磨性兼顾,适合交叉铺设和频繁弯曲的工程应用。表面可提供光面或镀锌处理,以适应不同腐蚀环境;执行 GB/T 20118-2006 标准,质量稳定可靠。具体性能表现请以实际检测与工况为准,欢迎来询。
询盘引导
如需了解 LM(涂层)钢丝绳 GB6X37.IWRC 的详细规格、表面处理选项、包装方式及供货能力,欢迎联系我们获取详细规格与报价。请提供所需直径、芯型、表面处理及预计用量,我们将尽快为您匹配合适的方案。