LM (Coating) Compacted Wire Rope GB6x36 (14/7+7/7/1) FC
Please feel freely to contact with us for new price .
Product Details
6x36 wire rope is a flexible general engineering wire rope available with either FC (fibre core) or IWRC (independent wire rope core). The wire rope has a superior breaking load and a good fatigue life. This wire rope can be used for a wide range of applications.
Surface treatment:Ungalv or Galvanized
Standard:GB/T 20118-2006

Applications
General engineering
Ropes for grab cranes
Wire rope slings
Crane rope
Hoist rope
Winch ropes
Lifeboat falls
Mooring ropes
Pursing wires
Luffing ropes
Luffing ropes
Breaking Loads
|
|
Min Breaking Loads |
Min Breaking Loads |
Min Breaking Loads | Min Breaking Loads |
Diameter | Weight |
(1770Mpa) |
(1770Mpa) |
(1960Mpa) |
(1960Mpa) |
mm | kg/m | KN | Kg | KN | Kg |
| 8 | 0.24 | 37.4 | 3813 | 41.4 | 4222 |
| 9 | 0.3 | 47.3 | 4825 | 52.4 | 5343 |
| 10 | 0.37 | 58.4 | 5957 | 64.7 | 6597 |
| 11 | 0.44 | 70.7 | 7208 | 78.3 | 7982 |
| 12 | 0.53 | 84.1 | 8579 | 93.1 | 9500 |
| 14 | 0.72 | 114 | 11677 | 127 | 12930 |
| 16 | 0.94 | 150 | 15252 | 166 | 16889 |
| 18 | 1.19 | 189 | 19303 | 210 | 21375 |
| 20 | 1.47 | 234 | 23831 | 259 | 26389 |
| 22 | 1.78 | 283 | 28835 | 313 | 31931 |
| 24 | 2.11 | 336 | 34317 | 373 | 38000 |
| 26 | 2.48 | 395 | 40274 | 437 | 44598 |
| 28 | 2.88 | 458 | 46709 | 507 | 51723 |
| 30 | 3.3 | 526 | 53620 | 582 | 59376 |
| 32 | 3.76 | 598 | 61008 | 662 | 67556 |
| 34 | 4.24 | 675 | 68872 | 748 | 76265 |
| 36 | 4.76 | 757 | 77213 | 838 | 85501 |
| 38 | 5.3 | 843 | 86030 | 934 | 95265 |
| 40 | 5.87 | 935 | 95325 | 1035 | 105557 |
| 42 | 6.47 | 1030 | 105095 | 1141 | 116377 |
| 44 | 7.11 | 1131 | 115343 | 1252 | 127724 |
| 46 | 7.77 | 1236 | 126067 | 1369 | 139600 |
| 48 | 8.46 | 1346 | 137268 | 1490 | 152003 |
| 50 | 9.18 | 1460 | 148945 | 1617 | 164934 |
| 52 | 9.92 | 1579 | 161099 | 1749 | 178392 |
| 56 | 11.5 | 1832 | 186837 | 2020 | 206893 |
| 60 | 13.2 | 2103 | 214481 | 2328 | 237504 |
General Engineering Ropes
GREENLOGY TEC(LM) specializes in supplying multiple strands of ungalvanised and galvanized steel wire ropes. Our products range from 0.5mm to 64mm, including 1X19, 7X7, 6X19, 7X19, 6X36, 8X19, 8X36, 19X7 and 35X7 with both Fibre Core and Steel Cores. In addition to these conventional steel wire ropes, we can also provide high-quality special steel wire ropes.
Most wire ropes are used in harsh conditions and must have resistance to extrusion, bending fatigue and abrasion. All of our wire ropes are guaranteed to achieve the highest level , maximizing the service life to increase the productivity of end users. We ensure that all materials are produced in accordance with the best standards in the wire rope industry. Each wire rope can be supplied with a thimble eyes, swaged ends and wedge sockets ,as well as many other assembly components.In addition, we also provide customized services, our team of engineers can manufacture wire ropes of your required specifications. All materials are certified, traceable, and comply with ISO9001 standards.
选型指导
请根据实际工况的信赖荷载、滑轮或卷筒直径、腐蚀环境与安全系数要求,确定钢丝绳直径、芯型(FC纤维芯或IWRC钢芯)以及1770Mpa或1960Mpa强度等级。若对弯曲疲劳寿命或抗挤压性能有较高要求,建议提供详细使用条件以便我们协助选型。欢迎联系我们获取针对具体应用的结构与规格建议。
产品优势
该6x36结构兼顾柔韧性与承载能力,FC纤维芯提供良好的可弯曲性,适合频繁弯曲的通用工程场景;表面可选光面或镀锌,以适应不同环境条件。产品寿命较长且抗疲劳性能良好,可用于吊索、起重机、绞车与系泊等多种应用。具体性能表现请结合实际使用条件评估。
询盘引导
欢迎联系我们获取详细规格、直径与长度选项、表面处理方式及报价信息。如需批量采购或定制结构,请告知您的应用场景与技术要求,我们将据此提供进一步支持。
简体中文
English