The core of 6X19 compacted filler wire rope (often referred to as 6x25) includes FC (fiber core) and IWRC (independent wire rope core). 6X19 wire rope can handle loads of 1T-5T and is used as wire rope slings. This construction is widely used in the North Sea oil industry.
Surface treatment: bright or galvanized
Standard: GB/T 20118-2006

Engineering Applications
Drilling line
Elevator hoisting rope
Wire rope slings
Luffing wire rope
Hoisting rope
Crane wire rope
Sand line, core line and swabbing line
Trawling / ocean sweeping
Ground rope / ground drag rope
Oil well / oilfield
Excavator rope / scraper rope
Fishing line
Tow rope
Breaking load
|
Minimum breaking load |
Minimum breaking load |
Minimum breaking load | Minimum breaking load | |
|---|---|---|---|---|---|
Diameter | Weight |
(1770Mpa) |
(1770Mpa) |
(1960Mpa) |
(1960Mpa) |
mm | kg/m | KN | Kg | KN | Kg |
| 10 | 0.36 | 58.4 | 5957 | 64.7 | 6597 |
| 11 | 0.43 | 70.7 | 7208 | 78.3 | 7982 |
| 12 | 0.52 | 84.1 | 8579 | 93.1 | 9500 |
| 13 | 0.61 | 98.7 | 10068 | 109 | 11149 |
| 14 | 0.7 | 114 | 11677 | 127 | 12930 |
| 16 | 0.92 | 150 | 15252 | 166 | 16889 |
| 18 | 1.16 | 189 | 19303 | 210 | 21375 |
| 20 | 1.44 | 234 | 23831 | 259 | 26389 |
| 22 | 1.74 | 283 | 28835 | 313 | 31931 |
| 24 | 2.07 | 336 | 34317 | 373 | 38000 |
| 26 | 2.43 | 395 | 40274 | 437 | 44598 |
| 28 | 2.82 | 458 | 46709 | 507 | 51723 |
| 30 | 3.23 | 526 | 53620 | 582 | 59376 |
| 32 | 3.68 | 598 | 61008 | 662 | 67556 |
| 34 | 4.15 | 675 | 68872 | 748 | 76265 |
| 36 | 4.65 | 757 | 77213 | 838 | 85501 |
| 38 | 5.18 | 843 | 86030 | 934 | 95265 |
| 40 | 5.74 | 935 | 95325 | 1035 | 105557 |
| 42 | 6.33 | 1030 | 105095 | 1141 | 116377 |
General Engineering Wire Rope
Greenlogy TEC specializes in supplying multi-strand bright or galvanized wire rope. Our products range in diameter from 0.5mm to 64mm, including 1X19, 7X7, 6X19, 7X19, 6X36, 8X19, 8X36, 19X7 and 35X7 specifications with fiber core and steel core. In addition to these standard wire ropes, we can also supply high-quality special wire ropes.
Most wire ropes work under demanding conditions and must resist crushing, bending fatigue and wear. All our wire ropes strive to achieve a high performance level to extend service life and thereby improve end-user productivity. We therefore ensure all materials are produced in accordance with wire rope industry standards. Every wire rope can be supplied with assembly components such as thimbles, swaged terminals and wedge sockets, as well as many others. We also offer customization services; our engineering team can manufacture wire ropes to your required specifications. All materials are certified, traceable and compliant with ISO9001.
Selection Guide
When selecting, determine the wire rope diameter, construction and surface treatment (bright or galvanized) according to the load requirements, operating environment (such as corrosion and temperature) and installation method of the actual application. We recommend referring to national standard GB/T 20118-2006, and you are welcome to contact us for detailed specifications and selection support.
Product Advantages
This product adopts a 6X19 compacted strand construction, offering high breaking force and fatigue resistance, while the fiber core (FC) provides good flexibility. The galvanized surface treatment enhances corrosion resistance, making it suitable for a variety of industrial applications.
Inquiry Guide
For detailed technical parameters, prices and delivery times, please contact us at any time. Please provide specific requirements such as diameter, length and surface treatment, and we will provide a professional quotation and solution.
Cut to Length
Need rope in fixed lengths? We cut wire rope to your required segment lengths before delivery (e.g. 5 m x 4 pcs + 10 m x 2 pcs), with end treatment per your needs. Request cut-to-length rope.
简体中文
English