LM (Coating) Filler Compacted Wire Rope GB6X19 (12/6+6F/1) IWRC
Request a Quote
Please feel freely to contact with us for new price .
Product Details
The core of 6X19 coated compacted filler wire rope (often referred to as 6x25) includes FC (fiber core) and IWRC (independent wire rope core). 6X19 wire rope can bear loads of 1T-5T and is used as wire rope. This construction is widely used in the North Sea oil industry.
Surface treatment: bright or galvanized
Standard: GB/T 20118-2006

Engineering Applications
Drilling line
Elevator hoisting rope
Wire rope sling
Luffing wire rope
Hoisting rope
Crane wire rope
Sand line, core line and swabbing line
Trawling / ocean sweeping
Grounding rope / ground drag rope
Oil well / oilfield
Excavator rope / scraper rope
Fishing line
Tow rope
Breaking load
|
|
Minimum breaking load |
Minimum breaking load |
Minimum breaking load | Minimum breaking load |
|---|---|---|---|---|---|
Diameter | Weight |
(1770Mpa) |
(1770Mpa) |
(1960Mpa) |
(1960Mpa) |
mm | kg/m | KN | Kg | KN | Kg |
| 14 | 0.78 | 124 | 12597 | 137 | 13949 |
| 16 | 1.02 | 161 | 16453 | 179 | 18219 |
| 18 | 1.3 | 204 | 20824 | 226 | 23059 |
| 20 | 1.6 | 252 | 25708 | 279 | 28468 |
| 22 | 1.94 | 305 | 31107 | 338 | 34447 |
| 24 | 2.3 | 363 | 37020 | 402 | 40994 |
| 26 | 2.7 | 426 | 43448 | 472 | 48111 |
| 28 | 3.14 | 494 | 50389 | 547 | 55798 |
| 30 | 3.6 | 567 | 57845 | 628 | 64054 |
| 32 | 4.1 | 645 | 65814 | 715 | 72879 |
| 34 | 4.62 | 728 | 74298 | 807 | 82274 |
| 36 | 5.18 | 817 | 83296 | 904 | 92238 |
| 38 | 5.78 | 910 | 92809 | 1008 | 102771 |
| 40 | 6.4 | 1008 | 102835 | 1116 | 113874 |
| 42 | 7.06 | 1112 | 113376 | 1231 | 125546 |
| 44 | 7.74 | 1220 | 124431 | 1351 | 137788 |
| 46 | 8.46 | 1333 | 136000 | 1476 | 150598 |
| 48 | 9.22 | 1452 | 148083 | 1608 | 163979 |
General Engineering Wire Rope
Greenlogy TEC specializes in supplying multi-strand bright or galvanized steel wire rope. Our products range in diameter from 0.5mm to 64mm, covering 1X19, 7X7, 6X19, 7X19, 6X36, 8X19, 8X36, 19X7 and 35X7 configurations with fiber core and steel core. In addition to these standard wire ropes, we can also supply high-quality special wire ropes.
Most wire ropes operate under demanding conditions and must resist crushing, bending fatigue and abrasion. All our wire ropes aim for a high performance level to extend service life and thereby improve end-user productivity. We therefore ensure all materials are produced in accordance with wire rope industry standards. Every wire rope can be supplied with fittings such as thimbles, swaged terminals, wedge sockets and many other assembly components. We also offer customization services; our engineering team can manufacture wire rope to your required specifications. All materials are certified, traceable and comply with ISO9001.
Selection Guide
Choose the appropriate diameter, surface finish (bright or galvanized) and core type (FC or IWRC) based on your application, required breaking load and working environment (such as corrosion and temperature). Contact us and our technical team will provide selection recommendations according to your specific needs.
Product Advantages
This wire rope adopts a compacted filler structure, offering high breaking strength and fatigue resistance, while the galvanized surface enhances corrosion resistance. It is suitable for a variety of heavy-load and dynamic application scenarios.
Inquiry Guide
For detailed specifications, quotations or customization services, please contact us through our website or by phone. We look forward to providing you with quality products and solutions.
Cut to Length
Need rope in fixed lengths? We cut wire rope to your required segment lengths before delivery (e.g. 5 m x 4 pcs + 10 m x 2 pcs), with end treatment per your needs. Request cut-to-length rope.
简体中文
English