 Glass fiber reinforced plastic ( FRP ) molding grid is a kind of plate material with a certain opening rate, which is made of unsaturated polyester resin ( including isophthalic up, linbenxing, type and fenquanxing, bisphenol ) as skeleton in the customization mold. 

Name

Content

Type

Resin

35%

OFR-25,IFR-25,VEFR-25

Fiberglass

33%

E

Filler

31%

ATH,PR

Others

1%

---

Introduction of raw materials

Resin type

Code

Resin type

Flame retardant property

Recommended usage occasions

MP-5

Phenolic type

Oxygen index can reach about 80

Low toxicity and high flame retardant, fire safety is very important for the occasion

VEFR-25

Vinyl type

Oxygen index 28 or above

Acid, alkali and other corrosive harsh environment

VEFR-10

Vinyl type

Oxygen index 35 or above

Flame retardant requirements of high acid, alkali and good occasions

IFR-25

Meta benzene

Oxygen index 28 or above

A VEFR type economy, and excellent, moderate acid alkali and solvent

IFGR-30

Benzene food grade

Oxygen index 26

Mainly used in meat products and food processing plants

OFR-25

Ortho type

Oxygen index 28 or above

General acid and alkali environment

OCR

Ortho type

Oxygen index below 28

OFR-25 economy, no flame retardant requirements

The type selection of coarse glass fiber  

Code

Coarse sand type

Recommended usage occasions

E

Non alkali sand

For high strength requirements and high corrosion resistance of the occasion

Selected filler type  

Code


Recommended usage occasions

ATH

Aluminum hydroxide

Retardant, smoke suppression, corrosion-resistant occasions

PR

No filler, pure resin

For high corrosion-resistant applications

Software - Sample 1 for three columns

Groove type

 

Software - Sample 2 for three columns

Polished type

 

Software - Sample 3 for three columns

Shop sand type

79 79 H23

79*79*23(mm)

Panel size available:

405*3569 Bidirectional force.

Bearing bar thickness (Top/Bottom):6.5/5.0

Bearing bar center:79

Open Aera:80%

Approx Weight:5.7kgs/m²

79 79 H23

The characteristics:

  1. Corrosion Resistant 

  2. Slip Resistant 

  3. Superior Ergonomics 

  4. Low Install Cost 

  5. Fire Retardant 

  6. Lightweight,Bi-directional Strength, and the cutting makes the pipes easier to install.

  7. The internal and external uniform color and color can be arbitrary choice.

  8. It has good social and economic benefits.

  9. Can design , flexible and varied size, size stability

Widely used in:

Genius FRP grating is widely used in landing (industrial) floor, stairs and walkways and platforms. Using glass fiber reinforced plastic grille has many advantages: glass fiber reinforced plastic grille, weather resistance, low maintenance cost, has a long service life and good anti-skid performance. In addition, the glass fiber reinforced plastic grille is simple, fast, flexible processing and assembly.  

Software - Sample 1 for three columns
Software - Sample 2 for three columns
Software - Sample 3 for three columns

Application Scenarios

FRP molded grating 79*79 H23 offers corrosion resistance, light weight, high strength and slip resistance, making it suitable for operating platforms, walkways and trench covers in corrosive environments such as chemical, electroplating, wastewater treatment and marine engineering. Its 79*79 mm mesh and 23 mm thickness design balance load-bearing with water and air permeability, and it is also commonly used in industrial sites with cleanliness and safety requirements. For advice on matching specific working conditions, please contact us.

Selection Guide

During selection, the actual load, span, support method and type of corrosive medium should be taken into account to confirm whether the grating's resin system, thickness and mesh size match. This product is molded from unsaturated polyester resin and E-glass fiber, and different resin types can be selected according to the service environment to balance corrosion resistance and flame retardant requirements. If you provide your working condition parameters, we can help recommend suitable specifications; please contact us to obtain detailed specifications and quotations.

Product Advantages

Molded grating is formed in one piece with uniform fiber and resin distribution, offering excellent corrosion resistance and bidirectional load-bearing capacity, as well as light weight, easy cutting and installation, and low maintenance costs. The surface can be treated for slip resistance to reduce operational risks in wet and slippery environments. Compared with traditional metal grating, it has a longer service life in acid, alkali and salt environments and requires no frequent anti-corrosion maintenance.

Inquiry Guidance

For detailed specifications, resin options, color customization and bulk supply solutions for FRP molded grating 79*79 H23, please contact us to obtain detailed specifications and quotations. Please inform us of your application scenario, required dimensions and quantity, and we will provide selection support and a commercial response as soon as possible.

Operating Environment

  • Molded FRP grating with a 79*79mm mesh and 23mm depth is built from unsaturated polyester resin and E-glass fiber, so it suits outdoor as well as indoor installations where moisture and weather exposure are continuous.
  • The isophthalic, bisphenol and phenolic resin options allow the grating to serve in chemically aggressive surroundings such as plating, chemical processing and wastewater treatment areas, where steel grating would corrode.
  • Because the molded grid carries a defined open area, it works well on walkways, platforms and trench covers where drainage, airflow and light passage through the panel are required.