FRP molded grating 60*220 H40
Request a Quote
Please feel freely to contact with us for new price .
Greenlogy TEC
Glass fiber reinforced plastic ( FRP ) molding grid is a kind of plate material with a certain opening rate, which is made of unsaturated polyester resin ( including isophthalic up, linbenxing, type and fenquanxing, bisphenol ) as skeleton in the customization mold.
Name | Content | Type |
|---|---|---|
Resin | 35% | OFR-25,IFR-25,VEFR-25 |
Fiberglass | 33% | E |
Filler | 31% | ATH,PR |
Others | 1% | --- |
Resin type
Code | Resin type | Flame retardant property | Recommended usage occasions |
|---|---|---|---|
MP-5 | Phenolic type | Oxygen index can reach about 80 | Low toxicity and high flame retardant, fire safety is very important for the occasion |
VEFR-25 | Vinyl type | Oxygen index 28 or above | Acid, alkali and other corrosive harsh environment |
VEFR-10 | Vinyl type | Oxygen index 35 or above | Flame retardant requirements of high acid, alkali and good occasions |
IFR-25 | Meta benzene | Oxygen index 28 or above | A VEFR type economy, and excellent, moderate acid alkali and solvent |
IFGR-30 | Benzene food grade | Oxygen index 26 | Mainly used in meat products and food processing plants |
OFR-25 | Ortho type | Oxygen index 28 or above | General acid and alkali environment |
OCR | Ortho type | Oxygen index below 28 | OFR-25 economy, no flame retardant requirements |
The type selection of coarse glass fiber
Code | Coarse sand type | Recommended usage occasions |
E | Non alkali sand | For high strength requirements and high corrosion resistance of the occasio |
Selected filler type
Code | Filler type | Recommended usage occasions |
|---|---|---|
ATH | Aluminum hydroxide | Retardant, smoke suppression, corrosion-resistant occasions |
PR | No filler, pure resin | For high corrosion-resistant applications |




60*220*40(mm)
Panel size available:
1788*2238 Length stress
Bearing bar thickness (Top/Bottom):6.3/5.0
Bearing bar center:60
Open Aera:67%
Approx Weight:8.8kgs/m²

The characteristics:
Corrosion Resistant
Slip Resistant
Superior Ergonomics
Low Install Cost
Fire Retardant
Lightweight,Bi-directional Strength, and the cutting makes the pipes easier to install.
The internal and external uniform color and color can be arbitrary choice.
It has good social and economic benefits.
Can design , flexible and varied size, size stability
Widely used in:
Greenlogy TEC grating is widely used in landing (industrial) floor, stairs and walkways and platforms. Using glass fiber reinforced plastic grille has many advantages: glass fiber reinforced plastic grille, weather resistance, low maintenance cost, has a long service life and good anti-skid performance. In addition, the glass fiber reinforced plastic grille is simple, fast, flexible processing and assembly.
Application scenarios
FRP molded grating is corrosion-resistant, lightweight and high-strength, and is commonly used for operating platforms, walkways, trench covers and stair treads in the chemical, wastewater treatment, marine engineering and electric power sectors. Different resin types correspond to different corrosion resistance and flame-retardant requirements, and can be applied in a variety of corrosive environments. Contact us for a suitable solution based on your specific operating conditions.
Selection guide
When selecting, you need to comprehensively consider the load-bearing requirements, span, corrosive media in the service environment and flame-retardant grade. This product has a mesh size of 60*220 and a thickness of 40 mm, which can meet general load-bearing and ventilation needs. If you provide load, span and media information, we can assist you in confirming the appropriate resin type and grating specification. Contact us for detailed selection advice.
Product advantages
FRP molded grating is molded from unsaturated polyester resin and fiberglass, featuring corrosion resistance, anti-slip performance, lightweight and high strength, insulation and maintenance-free advantages, and a long service life. The surface can be given an anti-slip treatment to improve safety. If you need to know specific performance data, contact us for detailed technical information.
Inquiry guide
If you need to know the detailed specifications, resin type selection, price and delivery information of this product, please contact us. Please provide your application scenario, load-bearing requirements and quantity, and we will provide you with a suitable solution and quotation as soon as possible.
Custom Cutting
Need panels that fit, or cut to shape? We custom cut FRP grating and profiles to your drawing: panels cut to size or to shape (corner cuts, cutouts), cut edges sealed with resin, and pre-cut and pre-drilled to drawing before shipping. See the custom cutting services.