FRP Molded Grating 50.8*50.8 H13

FRP Molded Grating 50.8*50.8 H13

Price on request

Request a Quote


Please feel freely to contact with us for new price .

Genius FRP  

Glass fiber reinforced plastic ( FRP ) molding grid is a kind of plate material with a certain opening rate, which is made of unsaturated polyester resin ( including isophthalic up, linbenxing, type and fenquanxing, bisphenol ) as skeleton in the customization mold. 

Name

Content

Type

Resin

35%

OFR-25,IFR-25,VEFR-25

Fiberglass

33%

E

Filler

31%

ATH,PR

Others

1%

---


Introduction of raw materials

Resin type

Code

Resin type

Flame retardant property

Recommended usage occasions

MP-5

Phenolic type

Oxygen index can reach about 80

Low toxicity and high flame retardant, fire safety is very important for the occasion

VEFR-25

Vinyl type

Oxygen index 28 or above

Acid, alkali and other corrosive harsh environment

VEFR-10

Vinyl type

Oxygen index 35 or above

Flame retardant requirements of high acid, alkali and good occasions

IFR-25

Meta benzene

Oxygen index 28 or above

A VEFR type economy, and excellent, moderate acid alkali and solvent

IFGR-30

Benzene food grade

Oxygen index 26

Mainly used in meat products and food processing plants

OFR-25

Ortho type

Oxygen index 28 or above

General acid and alkali environment

OCR

Ortho type

Oxygen index below 28

OFR-25 economy, no flame retardant requirements

The type selection of coarse glass fiber  

Code

Coarse sand type

Recommended usage occasions

E

Non alkali sand

For high strength requirements and high corrosion resistance of the occasion

Selected filler type  

Code

Filler type

Recommended usage occasions

ATH

Aluminum hydroxide

Retardant, smoke suppression, corrosion-resistant occasions

PR

No filler, pure resin

For high corrosion-resistant applications

Software - Sample 1 for three columns

Groove type
Software - Sample 2 for three columns

Polished type
Software - Sample 3 for three columns

Shop sand type

50.8 50.8 H13

50.8*50.8*13(mm)

Panel size available:

1220*4000,1220*3660,1220*2440,

915*3050 Bidirectional force.

Bearing bar thickness (Top/Bottom):7.0/6.0

Bearing bar center:50.8

Open Aera:82%

Approx Weight:5.8kgs/m²

Liner load

Liner load(units:mm)

Span in (mm)

Load in kn/m of widht (concentrated)

Maximum Recommended

Apparent E1*10^6 N-mm^2/m

4001.53011.8
6003.92114.9
8008.41216.5
100015.91017.0
Uniform load

Uniform load(units:mm)

Span in (mm)

Load in kn/sqm (uniformed)

Maximum Recommended

Apparent E1*10^6 N-mm^2/m

4000.415411.8
6001.57314.9
8000.43516.5
10009.92117.0
50.8 50.8 H13

The characteristics:

  1. Corrosion Resistant 

  2. Slip Resistant 

  3. Superior Ergonomics 

  4. Low Install Cost 

  5. Fire Retardant 

  6. Lightweight,Bi-directional Strength, and the cutting makes the pipes easier to install.

  7. The internal and external uniform color and color can be arbitrary choice.

  8. It has good social and economic benefits.

  9. Can design , flexible and varied size, size stability

Widely used in: 

Genius FRP grating is widely used in landing (industrial) floor, stairs and walkways and platforms. Using glass fiber reinforced plastic grille has many advantages: glass fiber reinforced plastic grille, weather resistance, low maintenance cost, has a long service life and good anti-skid performance. In addition, the glass fiber reinforced plastic grille is simple, fast, flexible processing and assembly.  

50.8 50.8 H13
50.8 50.8 H13
50.8 50.8 H13

Application Scenarios

FRP molded grating 50.8*50.8 H13 is suitable for walkways, platforms, trench covers and stair treads that require slip resistance, corrosion resistance and load-bearing capacity, and is commonly used in corrosive environments such as chemical, water treatment, electroplating and offshore platform applications. Its grid structure facilitates drainage, light transmission and ventilation, and different resin systems can be selected according to specific working conditions. Contact us to describe your service environment and obtain suitable recommendations.

Selection Guide

When selecting, it is recommended to first confirm the load-bearing requirements, span, corrosive media and flame retardancy requirements, and then choose the resin type (such as orthophthalic, isophthalic, vinyl ester or bisphenol A) as well as the grating thickness and mesh size accordingly. Different resin systems have different emphases in corrosion resistance and flame retardancy, and need to be weighed against actual working conditions. Contact us to provide your working condition parameters, and our technical personnel will assist with selection.

Product Advantages

Molded grating is formed in one piece from resin and fiberglass, featuring light weight, high strength, corrosion resistance, slip resistance and insulation, and is easy to cut, install and maintain later. Its grid structure reduces water and dust accumulation, making it suitable for long-term use in humid or chemically corrosive environments. Specific performance varies with different resin and fiber ratios. Contact us for detailed information.

Inquiry Guide

If you need to know the detailed specifications, resin options, price and delivery arrangements of FRP molded grating 50.8*50.8 H13, please contact us. Please provide your service environment, load-bearing requirements and required quantity, and we will recommend a suitable solution and reply with a quotation accordingly. Customization according to drawings and bulk purchase inquiries are supported.

Operating Environment

  • This molded FRP grating grade is built on unsaturated polyester resin, so it is suited to outdoor and indoor installations where moisture and washdown are routine, including walkways and platforms around process plants.
  • Because the resin is combined with E-glass fiber and an ATH filler system, the grating is intended for areas exposed to corrosive splashes and fumes; where a specific chemical resistance is required, confirm the grade with us before ordering.
  • The phenolic-based resin option (MP-5) is the recommended choice where low toxicity and flame retardant performance are the priority in the working area.
  • Typical service locations for this product line are industrial floors, access platforms and drainage covers that see continuous foot traffic in damp or chemically active surroundings.