FRP Molded Grating 50*50 H50

FRP Molded Grating 50*50 H50

Price on request

Request a Quote


Please feel freely to contact with us for new price .

Genius FRP  

Glass fiber reinforced plastic ( FRP ) molding grid is a kind of plate material with a certain opening rate, which is made of unsaturated polyester resin ( including isophthalic up, linbenxing, type and fenquanxing, bisphenol ) as skeleton in the customization mold.

Name

Content

Type

Resin

35%

OFR-25,IFR-25,VEFR-25

Fiberglass

33%

E

Filler

31%

ATH,PR

Others

1%

---

Introduction of raw materials

Resin type

Code

Resin type

Flame retardant property

Recommended usage occasions

MP-5

Phenolic type

Oxygen index can reach about 80

Low toxicity and high flame retardant, fire safety is very important for the occasion

VEFR-25

Vinyl type

Oxygen index 28 or above

Acid, alkali and other corrosive harsh environment

VEFR-10

Vinyl type

Oxygen index 35 or above

Flame retardant requirements of high acid, alkali and good occasions

IFR-25

Meta benzene

Oxygen index 28 or above

A VEFR type economy, and excellent, moderate acid alkali and solvent

IFGR-30

Benzene food grade

Oxygen index 26

Mainly used in meat products and food processing plants

OFR-25

Ortho type

Oxygen index 28 or above

General acid and alkali environment

OCR

Ortho type

Oxygen index below 28

OFR-25 economy, no flame retardant requirements

The type selection of coarse glass fiber  

Code

Coarse sand type

Recommended usage occasions

E

Non alkali sand

For high strength requirements and high corrosion resistance of the occasion

Selected filler type  

Code

Filler type

Recommended usage occasions

ATH

Aluminum hydroxide

Retardant, smoke suppression, corrosion-resistant occasions

PR

No filler, pure resin

For high corrosion-resistant applications

Software - Sample 1 for three columns

Groove type
Software - Sample 2 for three columns

Polished type
Software - Sample 3 for three columns

Shop sand type

50 50 H50

50*50*50(mm)

Panel size available:

1800*4000,1524*4000,1220*3660,

1220*2440,915*3050 Bidirectional force.

Bearing bar thickness (Top/Bottom):8.0/6.0

Bearing bar center:50

Open Aera:78%

Approx Weight:23.7kgs/m²

Liner load

Liner load(units:mm)

Deflcvtion

kg/m

kg/m

kg/m

kg/m

kg/m

kg/m

Limit

Span( mm)

150

300

450

600

750

1500

Load

3000.310.410.480.641.041.4521727
6000.510.811.231.753.334.2711713
9001.122.243.25.166.5813.57780
12001.332.615.989.9511.9---5834
Uniform load

Uniform load(units:mm)

Deflcvtion

kg/m²

kg/m²

kg/m²

kg/m²

kg/m²

kg/m²

kg/m²

Span( mm)

240

480

980

1450

2450

3650

4880

3000.250.280.330.380.480.74---
6000.380.580.971.372.134.12---
9001.192.113.945.779.4518.6---
12002.414.939.961516.821.6---
50 50 H50

The characteristics:

  1. Corrosion Resistant 

  2. Slip Resistant 

  3. Superior Ergonomics 

  4. Low Install Cost 

  5. Fire Retardant 

  6. Lightweight,Bi-directional Strength, and the cutting makes the pipes easier to install.

  7. The internal and external uniform color and color can be arbitrary choice.

  8. It has good social and economic benefits.

  9. Can design , flexible and varied size, size stability

Widely used in:

Genius FRP grating is widely used in landing (industrial) floor, stairs and walkways and platforms. Using glass fiber reinforced plastic grille has many advantages: glass fiber reinforced plastic grille, weather resistance, low maintenance cost, has a long service life and good anti-skid performance. In addition, the glass fiber reinforced plastic grille is simple, fast, flexible processing and assembly.  

50 50 H50
50 50 H50
50 50 H50

Application Scenarios

FRP molded grating is widely used for operating platforms, walkways, stair treads and trench covers in chemical, petroleum, power, wastewater treatment, marine engineering and other fields. Its corrosion resistance, slip resistance, light weight and high strength make it perform well in harsh environments such as humid, acid and alkaline conditions.

Selection Guide

Selection requires comprehensive consideration of load requirements, span, corrosive environment and fire rating. Different resin types (such as orthophthalic, isophthalic, vinyl ester and phenolic) suit different corrosive media and temperature conditions. Contact us for detailed specifications and selection advice, and we will provide a suitable solution based on your operating conditions.

Product Advantages

FRP molded grating offers excellent corrosion resistance, light weight and high strength, slip resistance, insulation and maintenance-free characteristics, with a long service life and easy installation. Compared with traditional metal grating, it can significantly reduce maintenance costs, especially in highly corrosive environments.

Inquiry Guide

For more product information, technical parameters or a quotation, please contact us. Provide your specific application scenario, size requirements and quantity, and we will provide professional support as soon as possible.

立即联系我们,我们将有专业人员为您服务。

7*24 professional team support. Within 24 Hours, our team will give you the feedback.

Send