FRP Molded Grating 40*40H40
Request a Quote
Please feel freely to contact with us for new price .
Genius FRP
Glass fiber reinforced plastic ( FRP ) molding grid is a kind of plate material with a certain opening rate, which is made of unsaturated polyester resin ( including isophthalic up, linbenxing, type and fenquanxing, bisphenol ) as skeleton in the customization mold.
Name | Content | Type |
|---|---|---|
Resin | 35% | OFR-25,IFR-25,VEFR-25 |
Fiberglass | 33% | E |
Filler | 31% | ATH,PR |
Others | 1% | --- |
Introduction of raw materials
Resin type
Code | Resin type | Flame retardant property | Recommended usage occasions |
|---|---|---|---|
MP-5 | Phenolic type | Oxygen index can reach about 80 | Low toxicity and high flame retardant, fire safety is very important for the occasion |
VEFR-25 | Vinyl type | Oxygen index 28 or above | Acid, alkali and other corrosive harsh environment |
VEFR-10 | Vinyl type | Oxygen index 35 or above | Flame retardant requirements of high acid, alkali and good occasions |
IFR-25 | Meta benzene | Oxygen index 28 or above | A VEFR type economy, and excellent, moderate acid alkali and solvent |
IFGR-30 | Benzene food grade | Oxygen index 26 | Mainly used in meat products and food processing plants |
OFR-25 | Ortho type | Oxygen index 28 or above | General acid and alkali environment |
OCR | Ortho type | Oxygen index below 28 | OFR-25 economy, no flame retardant requirements |
The type selection of coarse glass fiber
Code | Coarse sand type | Recommended usage occasions |
E | Non alkali sand | For high strength requirements and high corrosion resistance of the occasion |
Selected filler type
Code | Filler type | Recommended usage occasions |
|---|---|---|
ATH | Aluminum hydroxide | Retardant, smoke suppression, corrosion-resistant occasions |
PR | No filler, pure resin | For high corrosion-resistant applications |




40*40*40(mm)
Panel size available:
1247*4047,1007*4047,1007*3007
Bidirectional force.
Bearing bar thickness (Top/Bottom):7.0/5.0
Bearing bar center:40
Open Aera:67%
Approx Weight:19.2kgs/m²

Liner load(units:mm)
Span in (mm) | Load in kn/m of widht (concentrated) | Maximum Recommended | Apparent E1*10^6 N-mm^2/m |
| 400 | 7.3 | 19 | 7.14 |

Uniform load(units:mm)
Span in (mm) | Load in kn/sqm (uniformed) | Maximum Recommended | Apparent E1*10^6 N-mm^2/m |
|---|---|---|---|
| 400 | 1.8 | 100 | 7.14 |
| 600 | 7.7 | 45 | 8.55 |

The characteristics:
Corrosion Resistant
Slip Resistant
Superior Ergonomics
Low Install Cost
Fire Retardant
Lightweight,Bi-directional Strength, and the cutting makes the pipes easier to install.
The internal and external uniform color and color can be arbitrary choice.
It has good social and economic benefits.
Can design , flexible and varied size, size stability
Widely used in:
Genius FRP grating is widely used in landing (industrial) floor, stairs and walkways and platforms. Using glass fiber reinforced plastic grille has many advantages: glass fiber reinforced plastic grille, weather resistance, low maintenance cost, has a long service life and good anti-skid performance. In addition, the glass fiber reinforced plastic grille is simple, fast, flexible processing and assembly.



Application Scenarios
FRP molded grating 40*40H40 is suitable for platforms, walkways, trench covers and equipment operating surfaces that require corrosion resistance, slip resistance and load-bearing capacity. It is commonly used in chemical, water treatment, power and marine engineering environments. For suitability under specific working conditions, we recommend confirming with us based on the medium, load and installation method.
Selection Guidance
During selection, factors such as the resin system, grating thickness, mesh size and support span can be considered comprehensively. For example, in corrosive medium environments, priority can be given to the corrosion-resistant resin type, while in areas with higher load-bearing requirements, attention can be paid to the grating height and support conditions. You are welcome to contact us, and our technical staff will provide selection advice and detailed specifications based on your actual working conditions.
Product Advantages
The molded process forms the grating as a whole, with uniform distribution of fibers and resin. It features light weight and high strength, corrosion resistance, slip resistance, and easy cutting and installation, which facilitates on-site processing and later maintenance. Compared with traditional metal materials, it helps extend the service life in humid and corrosive environments.
Inquiry Guidance
If you need to know the detailed specifications, colors, surface forms and commercial terms of FRP molded grating 40*40H40, you are welcome to contact us for detailed specifications and quotations. Please provide information such as the usage environment, load-bearing requirements and quantity, and we will recommend a suitable solution accordingly.
Operating Environment
- This molded FRP grating is built for service in corrosive chemical environments, where its unsaturated polyester resin and glass fiber reinforcement resist degradation from acids, alkalis and salts.
- It is suited to both indoor and outdoor installations, including industrial plants, walkways and platforms exposed to weather and repeated washdown.
- With flame-retardant resin options, the grating supports use in areas where fire safety is a consideration, such as chemical processing and other industrial settings.
- It performs in humid and wet conditions where traditional metal grating would corrode; for specific temperature, chemical exposure or load requirements, contact us for the full parameter list.
简体中文