FRP Molded Grating 38*152H38 T-Type

FRP Molded Grating 38*152H38 T-Type

Price on request

Get a quote
Request a Quote


Please feel freely to contact with us for new price .

Greenlogy TEC

Glass fiber reinforced plastic ( FRP ) molding grid is a kind of plate material with a certain opening rate, which is made of unsaturated polyester resin ( including isophthalic up, linbenxing, type and fenquanxing, bisphenol ) as skeleton in the customization mold. 

Name

Content

Type

Resin

35%

OFR-25,IFR-25,VEFR-25

Fiberglass

33%

E

Filler

31%

ATH,PR

Others

1%

---

Introduction of raw materials

 Resin type  

Code

Resin type

Flame retardant property

Recommended usage occasions

MP-5

Phenolic type

Oxygen index can reach about 80

Low toxicity and high flame retardant, fire safety is very important for the occasion

VEFR-25

Vinyl type

Oxygen index 28 or above

Acid, alkali and other corrosive harsh environment

VEFR-10

Vinyl type

Oxygen index 35 or above

Flame retardant requirements of high acid, alkali and good occasions

IFR-25

Meta benzene

Oxygen index 28 or above

A VEFR type economy, and excellent, moderate acid alkali and solvent

IFGR-30

Benzene food grade

Oxygen index 26

Mainly used in meat products and food processing plants

OFR-25

Ortho type

Oxygen index 28 or above

General acid and alkali environment

OCR

Ortho type

Oxygen index below 28

OFR-25 economy, no flame retardant requirements

The type selection of coarse glass fiber   

Code

Coarse sand type

Recommended usage occasions

E

Non alkali sand

For high strength requirements and high corrosion resistance of the occasio

Selected filler type  

Code

Filler type

Recommended usage occasions

ATH

Aluminum hydroxide

Retardant, smoke suppression, corrosion-resistant occasions

PR

No filler, pure resin

For high corrosion-resistant applications

Software - Sample 1 for three columns

Groove type
Software - Sample 2 for three columns

Polished type
Software - Sample 3 for three columns

Shop sand type

38 152 H38 T shape

38*152*38(mm)

Panel size available:

1220*3660 Length stress      

Bearing bar thickness (Top/Bottom):15.0/8.0

Bearing bar center:38

Open Aera:62%

Approx Weight:18.6kgs/m²

38 152 H38 T shape

The characteristics:

  1. Corrosion Resistant 

  2. Slip Resistant 

  3. Superior Ergonomics 

  4. Low Install Cost 

  5. Fire Retardant 

  6. Lightweight,Bi-directional Strength, and the cutting makes the pipes easier to install.

  7. The internal and external uniform color and color can be arbitrary choice.

  8. It has good social and economic benefits.

  9. Can design , flexible and varied size, size stability

Widely used in:

Greenlogy TEC grating is widely used in landing (industrial) floor, stairs and walkways and platforms. Using glass fiber reinforced plastic grille has many advantages: glass fiber reinforced plastic grille, weather resistance, low maintenance cost, has a long service life and good anti-skid performance. In addition, the glass fiber reinforced plastic grille is simple, fast, flexible processing and assembly.  

Software - Sample 1 for three columns
Software - Sample 2 for three columns
Software - Sample 3 for three columns

Application Scenarios

FRP molded grating 38×152H38 T-Type is widely used for platforms, walkways, trench covers and stair treads in chemical, petroleum, power, wastewater treatment, marine engineering and other fields. Its corrosion resistance, slip resistance, light weight and high strength make it perform well in harsh environments such as humid and acid-alkali conditions. If you need a suitable solution recommended for your specific working conditions, please contact us for detailed specifications and quotations.

Selection Guide

When selecting, please take into account load requirements, span, corrosive environment and safety level. T-type grating offers higher load capacity and slip resistance, making it suitable for heavy-duty applications or where higher safety requirements apply. Please provide your specific service conditions, and we will assist you in choosing the most suitable resin type and grating specifications.

Product Advantages

This product is molded from unsaturated polyester resin and E-glass fiber, featuring excellent corrosion resistance, light weight and high strength, slip resistance and electrical insulation, and ease of installation and maintenance. Compared with traditional metal grating, it has a longer service life and requires no frequent anti-corrosion treatment, resulting in lower overall cost.

Inquiry Guidance

Please contact us for detailed specifications, technical parameters and quotations. We can provide customized solutions according to your needs and offer you professional technical support.

Custom Cutting

Need panels that fit, or cut to shape? We custom cut FRP grating and profiles to your drawing: panels cut to size or to shape (corner cuts, cutouts), cut edges sealed with resin, and pre-cut and pre-drilled to drawing before shipping. See the custom cutting services.

WhatsApp