FRP Molded Grating 38*100H38

FRP Molded Grating 38*100H38

Price on request

Get a quote
Request a Quote


Please feel freely to contact with us for new price .

Greenlogy TEC

Glass fiber reinforced plastic ( FRP ) molding grid is a kind of plate material with a certain opening rate, which is made of unsaturated polyester resin ( including isophthalic up, linbenxing, type and fenquanxing, bisphenol ) as skeleton in the customization mold. 

Name

Content

Type

Resin

35%

OFR-25,IFR-25,VEFR-25

Fiberglass

33%

E

Filler

31%

ATH,PR

Others

1%

---

Introduction of raw materials

 Resin type  

Code

Resin type

Flame retardant property

Recommended usage occasions

MP-5

Phenolic type

Oxygen index can reach about 80

Low toxicity and high flame retardant, fire safety is very important for the occasion

VEFR-25

Vinyl type

Oxygen index 28 or above

Acid, alkali and other corrosive harsh environment

VEFR-10

Vinyl type

Oxygen index 35 or above

Flame retardant requirements of high acid, alkali and good occasions

IFR-25

Meta benzene

Oxygen index 28 or above

A VEFR type economy, and excellent, moderate acid alkali and solvent

IFGR-30

Benzene food grade

Oxygen index 26

Mainly used in meat products and food processing plants

OFR-25

Ortho type

Oxygen index 28 or above

General acid and alkali environment

OCR

Ortho type

Oxygen index below 28

OFR-25 economy, no flame retardant requirements

The type selection of coarse glass fiber   

Code

Coarse sand type

Recommended usage occasions

E

Non alkali sand

For high strength requirements and high corrosion resistance of the occasio

Selected filler type  

Code

Filler type

Recommended usage occasions

ATH

Aluminum hydroxide

Retardant, smoke suppression, corrosion-resistant occasions

PR

No filler, pure resin

For high corrosion-resistant applications

Software - Sample 1 for three columns

Groove type
Software - Sample 2 for three columns

Polished type
Software - Sample 3 for three columns

Shop sand type

38 100 H38

38*100*38(mm)

Panel size available:

1220*3660,1220*2440,915*3050 Length stress      

Bearing bar thickness (Top/Bottom):8.0/6.0

Bearing bar center:38

Open Aera:65%

Approx Weight:16.4kgs/m²

38 100 H38

The characteristics:

  1. Corrosion Resistant 

  2. Slip Resistant 

  3. Superior Ergonomics 

  4. Low Install Cost 

  5. Fire Retardant 

  6. Lightweight,Bi-directional Strength, and the cutting makes the pipes easier to install.

  7. The internal and external uniform color and color can be arbitrary choice.

  8. It has good social and economic benefits.

  9. Can design , flexible and varied size, size stability

Widely used in:

Greenlogy TEC grating is widely used in landing (industrial) floor, stairs and walkways and platforms. Using glass fiber reinforced plastic grille has many advantages: glass fiber reinforced plastic grille, weather resistance, low maintenance cost, has a long service life and good anti-skid performance. In addition, the glass fiber reinforced plastic grille is simple, fast, flexible processing and assembly. 

Software - Sample 1 for three columns
Software - Sample 2 for three columns
Software - Sample 3 for three columns

Application Scenarios

FRP molded grating 38*100H38 is suitable for industrial and municipal applications such as walkways, trench covers, operating passages and equipment fencing that require slip resistance, corrosion resistance and load-bearing capacity. Its molded structure allows for easy on-site cutting and installation, and different resin systems can be selected according to actual working conditions to meet chemical resistance or flame retardant requirements. For specific applicable environments and installation methods, please contact us for detailed specifications and quotations.

Selection Guide

When selecting, please consider the medium type, temperature conditions, load-bearing requirements and fire rating of the service environment to confirm the required resin type, grating thickness and mesh size. Different resin systems have different emphases on corrosion resistance and flame retardant performance, and it is recommended to match them according to actual working conditions. If you need assistance with selection, please contact us for detailed specifications and quotations.

Product Advantages

FRP molded grating is integrally molded from resin and glass fiber, featuring light weight, high strength, corrosion resistance, slip resistance and insulation, and is easy to cut and install, which reduces later maintenance. Its surface color and anti-slip grit can be adjusted according to requirements, making it suitable for various industrial environments. Please contact us for detailed specifications and quotations.

Inquiry Guide

If you need to know the specific specifications, resin system options or commercial terms of FRP molded grating 38*100H38, please contact our sales team. Please provide your service environment, load-bearing requirements and required quantity, and we will recommend a suitable product solution for you. Please contact us for detailed specifications and quotations.

Operating Environment

  • Suitable for both indoor and outdoor installations, including platforms, walkways and stair treads where the molded FRP grating is exposed to weather and humidity.
  • Withstands humid and wet conditions typical of industrial plants, water treatment areas and marine environments, resisting moisture absorption and rust.
  • Resists corrosion from a range of chemical media such as acids, alkalis and salts, depending on the selected resin system (isophthalic, bisphenol or phenolic type).
  • Operates effectively across a wide ambient temperature range encountered in industrial settings, maintaining structural integrity without becoming brittle or soft.

Custom Cutting

Need panels that fit, or cut to shape? We custom cut FRP grating and profiles to your drawing: panels cut to size or to shape (corner cuts, cutouts), cut edges sealed with resin, and pre-cut and pre-drilled to drawing before shipping. See the custom cutting services.