 Glass fiber reinforced plastic ( FRP ) molding grid is a kind of plate material with a certain opening rate, which is made of unsaturated polyester resin ( including isophthalic up, linbenxing, type and fenquanxing, bisphenol ) as skeleton in the customization mold. 

Name

Content

Type

Resin

35%

OFR-25,IFR-25,VEFR-25

Fiberglass

33%

E

Filler

31%

ATH,PR

Others

1%

---

Introduction of raw materials

Resin type

Code

Resin type

Flame retardant property

Recommended usage occasions

MP-5

Phenolic type

Oxygen index can reach about 80

Low toxicity and high flame retardant, fire safety is very important for the occasion

VEFR-25

Vinyl type

Oxygen index 28 or above

Acid, alkali and other corrosive harsh environment

VEFR-10

Vinyl type

Oxygen index 35 or above

Flame retardant requirements of high acid, alkali and good occasions

IFR-25

Meta benzene

Oxygen index 28 or above

A VEFR type economy, and excellent, moderate acid alkali and solvent

IFGR-30

Benzene food grade

Oxygen index 26

Mainly used in meat products and food processing plants

OFR-25

Ortho type

Oxygen index 28 or above

General acid and alkali environment

OCR

Ortho type

Oxygen index below 28

OFR-25 economy, no flame retardant requirements

The type selection of coarse glass fiber  

Code

Coarse sand type

Recommended usage occasions

E

Non alkali sand

For high strength requirements and high corrosion resistance of the occasion

Selected filler type  

Code

Filler type

Recommended usage occasions

ATH

Aluminum hydroxide

Retardant, smoke suppression, corrosion-resistant occasions

PR

No filler, pure resin

For high corrosion-resistant applications

Software - Sample 1 for three columns

Groove type

Software - Sample 2 for three columns

Polished type

Software - Sample 3 for three columns

Shop sand type

25 25 H50

25*25*50(mm)

Panel size available:

1524*4000 Bidirectional force.

Bearing bar thickness (Top/Bottom):8.0/6.0

Bearing bar center:25

Open Aera:55%

Approx Weight:28.5kgs/m²

25 25 H50

The characteristics:

  1. Corrosion Resistant 

  2. Slip Resistant 

  3. Superior Ergonomics 

  4. Low Install Cost 

  5. Fire Retardant 

  6. Lightweight,Bi-directional Strength, and the cutting makes the pipes easier to install.

  7. The internal and external uniform color and color can be arbitrary choice.

  8. It has good social and economic benefits.

  9. Can design , flexible and varied size, size stability

Widely used in:

Greenlogy TEC FRP grating is widely used in landing (industrial) floor, stairs and walkways and platforms. Using glass fiber reinforced plastic grille has many advantages: glass fiber reinforced plastic grille, weather resistance, low maintenance cost, has a long service life and good anti-skid performance. In addition, the glass fiber reinforced plastic grille is simple, fast, flexible processing and assembly.

Software - Sample 1 for three columns
Software - Sample 2 for three columns
Software - Sample 3 for three columns

Application Scenarios

FRP Molded Grating 25*25H50 features corrosion resistance, light weight, high strength and slip resistance. It is suitable for operating platforms, walkways, stair treads and trench covers in chemical, electroplating, water treatment, marine engineering and other industries. Its 25 mm mesh and 50 mm thickness strike a balance between load bearing and drainage, making it suitable for medium-load industrial environments. For specific scenario selection, please contact us for detailed recommendations.

Selection Guide

During selection, confirm the resin type (such as orthophthalic, isophthalic, vinyl ester or bisphenol A) to match corrosion resistance requirements, and choose grating thickness and mesh size according to load and span (this product is 25*25H50). Surface anti-slip treatment (such as gritted) and color customization can also be considered. For technical selection support, please contact us for detailed specifications and quotations.

Product Advantages

This product is molded from unsaturated polyester resin and E-glass fiber, offering excellent corrosion resistance, aging resistance and electrical insulation, as well as light weight, easy installation and low maintenance cost. Its structural design balances load bearing and drainage, making it suitable for various industrial environments. Please contact us for detailed specifications and quotations.

Inquiry Guide

For detailed specifications, technical parameters, customization options and commercial terms of FRP Molded Grating 25*25H50, please contact us via the website or by phone. We will provide professional technical support and quotation solutions based on your specific needs.

Operating Environment

  • Molded FRP grating with 25×25 mm mesh and 50 mm depth is suited to both indoor and outdoor service in industrial plants, where the unsaturated polyester resin matrix resists moisture and wash-down.
  • The corrosion-resistant resin types (isophthalic, vinyl ester and bisphenol) make this grating suitable for chemically aggressive areas such as process platforms, walkways and trench covers exposed to acids, alkalis and salts.
  • Flame-retardant grades are available for locations where fire safety is a concern, including areas requiring low toxicity and high flame retardance.
  • For the full temperature and chemical resistance parameters of each resin grade, contact Greenlogy TEC for the detailed data sheet.

Custom Cutting

Need panels that fit, or cut to shape? We custom cut FRP grating and profiles to your drawing: panels cut to size or to shape (corner cuts, cutouts), cut edges sealed with resin, and pre-cut and pre-drilled to drawing before shipping. See the custom cutting services.

WhatsApp