FRP Molded Grating 25*152H38 Stair Tread

FRP Molded Grating 25*152H38 Stair Tread

Price on request

Get a quote
Request a Quote


Please feel freely to contact with us for new price .

Greenlogy TEC

Glass fiber reinforced plastic ( FRP ) molding grid is a kind of plate material with a certain opening rate, which is made of unsaturated polyester resin ( including isophthalic up, linbenxing, type and fenquanxing, bisphenol ) as skeleton in the customization mold. 

Name

Content

Type

Resin

35%

OFR-25,IFR-25,VEFR-25

Fiberglass

33%

E

Filler

31%

ATH,PR

Others

1%

---

Introduction of raw materials

 Resin type  

Code

Resin type

Flame retardant property

Recommended usage occasions

MP-5

Phenolic type

Oxygen index can reach about 80

Low toxicity and high flame retardant, fire safety is very important for the occasion

VEFR-25

Vinyl type

Oxygen index 28 or above

Acid, alkali and other corrosive harsh environment

VEFR-10

Vinyl type

Oxygen index 35 or above

Flame retardant requirements of high acid, alkali and good occasions

IFR-25

Meta benzene

Oxygen index 28 or above

A VEFR type economy, and excellent, moderate acid alkali and solvent

IFGR-30

Benzene food grade

Oxygen index 26

Mainly used in meat products and food processing plants

OFR-25

Ortho type

Oxygen index 28 or above

General acid and alkali environment

OCR

Ortho type

Oxygen index below 28

OFR-25 economy, no flame retardant requirements

The type selection of coarse glass fiber   

Code

Coarse sand type

Recommended usage occasions

E

Non alkali sand

For high strength requirements and high corrosion resistance of the occasio

Selected filler type  

Code

Filler type

Recommended usage occasions

ATH

Aluminum hydroxide

Retardant, smoke suppression, corrosion-resistant occasions

PR

No filler, pure resin

For high corrosion-resistant applications

Software - Sample 1 for three columns

Groove type
Software - Sample 2 for three columns

Polished type
Software - Sample 3 for three columns

Shop sand type

25 152 H38 Stair tread

25*152*38(mm)

Panel size available:

565*3050 Bidirectional force      

Bearing bar thickness (Top/Bottom):7.0/5.0

Bearing bar center:25

Open Aera:62%

Approx Weight:23.1kgs/m²

25 152 H38 Stair tread

The characteristics:

  1. Corrosion Resistant 

  2. Slip Resistant 

  3. Superior Ergonomics 

  4. Low Install Cost 

  5. Fire Retardant 

  6. Lightweight,Bi-directional Strength, and the cutting makes the pipes easier to install.

  7. The internal and external uniform color and color can be arbitrary choice.

  8. It has good social and economic benefits.

  9. Can design , flexible and varied size, size stability

Widely used in:

Greenlogy TEC grating is widely used in landing (industrial) floor, stairs and walkways and platforms. Using glass fiber reinforced plastic grille has many advantages: glass fiber reinforced plastic grille, weather resistance, low maintenance cost, has a long service life and good anti-skid performance. In addition, the glass fiber reinforced plastic grille is simple, fast, flexible processing and assembly.  

Software - Sample 1 for three columns
Software - Sample 2 for three columns
Software - Sample 3 for three columns

Application Scenarios

FRP molded grating 25*152H38 stair tread is suitable for platforms and stairways in corrosive environments such as chemical, wastewater treatment, electroplating, and marine engineering. Its molded structure provides a slip-resistant surface and load-bearing capacity, making it suitable for walkway areas requiring corrosion resistance, light weight, and low maintenance. Contact us to discuss adaptation solutions for your specific working conditions.

Selection Guide

When selecting, please confirm that the resin type (such as orthophthalic, isophthalic, vinyl ester, or phenolic) matches the corrosive media and flame retardant requirements of the service environment, and determine the grating thickness and support spacing based on load-bearing requirements and installation method. We can recommend a suitable configuration according to your working conditions. Contact us for detailed specifications and quotations.

Product Advantages

Molded grating features corrosion resistance, light weight and high strength, slip resistance, electrical insulation, and low maintenance. The 25*152H38 specification balances load-bearing and slip-resistant performance in stair tread applications. The product has a long service life and is easy to install, reducing later maintenance costs. Contact us for detailed specifications and quotations.

Inquiry Guide

For detailed specifications, resin selection, or bulk supply solutions for FRP molded grating 25*152H38 stair tread, contact us for detailed specifications and quotations. Our technical team can assist you with selection and engineering adaptation.

Operating Environment

  • Designed for both indoor and outdoor installations, this FRP molded grating stair tread (25*152H38) resists moisture, humidity and weathering without the corrosion that affects steel.
  • Made from unsaturated polyester resin (including isophthalic, vinyl ester and bisphenol types) with E-glass fiber, it performs in chemically aggressive surroundings such as process areas, wash-down zones and coastal atmospheres.
  • With phenolic-type resin options offering low toxicity and high flame retardance, the tread suits industrial environments where fire safety is a concern.
  • Its anti-slip molded grid surface keeps footing secure on walkways, platforms and stairways in wet or oily plant conditions.