FRP molded grating 25*100H30

FRP molded grating 25*100H30

Price on request

Get a quote
Request a Quote


Please feel freely to contact with us for new price .

Greenlogy TEC

Glass fiber reinforced plastic ( FRP ) molding grid is a kind of plate material with a certain opening rate, which is made of unsaturated polyester resin ( including isophthalic up, linbenxing, type and fenquanxing, bisphenol ) as skeleton in the customization mold. 

Name

Content

Type

Resin

35%

OFR-25,IFR-25,VEFR-25

Fiberglass

33%

E

Filler

31%

ATH,PR

Others

1%

---

Introduction of raw materials

 Resin type  

Code

Resin type

Flame retardant property

Recommended usage occasions

MP-5

Phenolic type

Oxygen index can reach about 80

Low toxicity and high flame retardant, fire safety is very important for the occasion

VEFR-25

Vinyl type

Oxygen index 28 or above

Acid, alkali and other corrosive harsh environment

VEFR-10

Vinyl type

Oxygen index 35 or above

Flame retardant requirements of high acid, alkali and good occasions

IFR-25

Meta benzene

Oxygen index 28 or above

A VEFR type economy, and excellent, moderate acid alkali and solvent

IFGR-30

Benzene food grade

Oxygen index 26

Mainly used in meat products and food processing plants

OFR-25

Ortho type

Oxygen index 28 or above

General acid and alkali environment

OCR

Ortho type

Oxygen index below 28

OFR-25 economy, no flame retardant requirements

The type selection of coarse glass fiber  

Code

Coarse sand type

Recommended usage occasions

E

Non alkali sand

For high strength requirements and high corrosion resistance of the occasio

Selected filler type  

Code

Filler type

Recommended usage occasions

ATH

Aluminum hydroxide

Retardant, smoke suppression, corrosion-resistant occasions

PR

No filler, pure resin

For high corrosion-resistant applications

Software - Sample 1 for three columns

Groove type
Software - Sample 2 for three columns

Polished type
Software - Sample 3 for three columns

Shop sand type

25 100 H30

25*100*30(mm)

Panel size available:

1007*3007 Width stress 

Bearing bar thickness (Top/Bottom):7.0/5.5

Bearing bar center:25

Open Aera:67%

Approx Weight:15.6kgs/m²

25 100 H30

The characteristics:

  1. Corrosion Resistant 

  2. Slip Resistant 

  3. Superior Ergonomics 

  4. Low Install Cost 

  5. Fire Retardant 

  6. Lightweight,Bi-directional Strength, and the cutting makes the pipes easier to install.

  7. The internal and external uniform color and color can be arbitrary choice.

  8. It has good social and economic benefits.

  9. Can design , flexible and varied size, size stability

Widely used in:

Greenlogy TEC FRP grating is widely used in landing (industrial) floor, stairs and walkways and platforms. Using glass fiber reinforced plastic grille has many advantages: glass fiber reinforced plastic grille, weather resistance, low maintenance cost, has a long service life and good anti-skid performance. In addition, the glass fiber reinforced plastic grille is simple, fast, flexible processing and assembly.  

Software - Sample 1 for three columns
Software - Sample 2 for three columns
Software - Sample 3 for three columns

Application Scenarios

FRP molded grating offers excellent corrosion resistance, light weight and high strength, and anti-slip performance. It is widely used in operating platforms, walkways, trench covers and stair treads in chemical, petroleum, power, marine engineering and other fields. Its open mesh structure allows liquids and gases to pass through, reducing water accumulation and wind resistance, making it suitable for industrial environments with high requirements for safety and durability. For specific application cases, please contact us.

Selection Guide

When selecting, factors such as the corrosiveness of the service environment, load requirements, fire rating and color should be considered. For example, in highly corrosive environments, isophthalic or vinyl ester resin is recommended; where high fire resistance is required, phenolic resin (such as MP-5) can be used. Different mesh sizes and thicknesses affect load-bearing capacity; please consult our technical team based on your actual needs to obtain professional advice.

Product Advantages

FRP molded grating is integrally molded from high-strength glass fiber and resin. It features light weight and high strength, corrosion resistance, anti-slip, electrical insulation, non-magnetic properties and easy installation, with long service life and low maintenance cost. Its unique mesh design effectively drains water and prevents dust accumulation, and colors and sizes can be customized according to customer requirements to meet diverse industrial needs.

Inquiry Guide

For detailed specifications, technical parameters, samples or quotations, please contact us anytime. Our professional team will provide customized solutions based on your specific needs to ensure we provide you with the most suitable products and services.

Operating Environment

  • This molded FRP grating (25*100H30) is built on an unsaturated polyester resin skeleton with E-glass fiber and ATH or PR filler, so the finished panel is suited to both indoor and outdoor installations where moisture and weather exposure are constant.
  • The resin system is selected according to the service medium, so the grating can be specified for areas with corrosive chemical splash, fumes or washdown, and the recommended resin grade should be confirmed with us for each project.
  • Typical applications include walkways, platforms, stair treads and trench covers in plants, where the open mesh lets liquids and debris pass through and the FRP surface is used in place of painted steel.
  • Where fire safety or low-toxicity performance is a concern, the phenolic-type resin option is available and its flame-retardant behaviour should be discussed with us against the actual operating conditions.

Custom Cutting

Need panels that fit, or cut to shape? We custom cut FRP grating and profiles to your drawing: panels cut to size or to shape (corner cuts, cutouts), cut edges sealed with resin, and pre-cut and pre-drilled to drawing before shipping. See the custom cutting services.

WhatsApp