FRP Molded Grating 25*100 H25 Standard Load Type
Request a Quote
Please feel freely to contact with us for new price .
Greenlogy TEC
Glass fiber reinforced plastic ( FRP ) molding grid is a kind of plate material with a certain opening rate, which is made of unsaturated polyester resin ( including isophthalic up, linbenxing, type and fenquanxing, bisphenol ) as skeleton in the customization mold.
Name | Content | Type |
|---|---|---|
Resin | 35% | OFR-25,IFR-25,VEFR-25 |
Fiberglass | 33% | E |
Filler | 31% | ATH,PR |
Others | 1% | --- |
Resin type
Code | Resin type | Flame retardant property | Recommended usage occasions |
|---|---|---|---|
MP-5 | Phenolic type | Oxygen index can reach about 80 | Low toxicity and high flame retardant, fire safety is very important for the occasion |
VEFR-25 | Vinyl type | Oxygen index 28 or above | Acid, alkali and other corrosive harsh environment |
VEFR-10 |
Vinyl type | Oxygen index 35 or above | Flame retardant requirements of high acid, alkali and good occasions |
IFR-25 | Meta benzene | Oxygen index 28 or above | A VEFR type economy, and excellent, moderate acid alkali and solvent |
IFGR-30 | Benzene food grade | Oxygen index 26 | Mainly used in meat products and food processing plants |
OFR-25 | Ortho type | Oxygen index 28 or above | General acid and alkali environment |
OCR | Ortho type | Oxygen index below 28 | OFR-25 economy, no flame retardant requirements |
The type selection of coarse glass fiber
Code | Coarse sand type | Recommended usage occasions |
E | Non alkali sand | For high strength requirements and high corrosion resistance of the occasio |
Selected filler type
Code | Filler type | Recommended usage occasions |
|---|---|---|
ATH | Aluminum hydroxide | Retardant, smoke suppression, corrosion-resistant occasions |
PR | No filler, pure resin | For high corrosion-resistant applications |




25*100*25(mm)
Panel size available:
1220*3660 Length stress\Width stress
Bearing bar thickness (Top/Bottom):6.5/5.0
Bearing bar center:25
Open Aera:67%
Approx Weight:13.83kgs/m²

The characteristics:
Corrosion Resistant
Slip Resistant
Superior Ergonomics
Low Install Cost
Fire Retardant
Lightweight,Bi-directional Strength, and the cutting makes the pipes easier to install.
The internal and external uniform color and color can be arbitrary choice.
It has good social and economic benefits.
Can design , flexible and varied size, size stability
Widely used in:
Greenlogy TEC FRP grating is widely used in landing (industrial) floor, stairs and walkways and platforms. Using glass fiber reinforced plastic grille has many advantages: glass fiber reinforced plastic grille, weather resistance, low maintenance cost, has a long service life and good anti-skid performance. In addition, the glass fiber reinforced plastic grille is simple, fast, flexible processing and assembly.
Application Scenarios
FRP molded grating 25*100 H25 standard load type is suitable for general industrial platforms, walkways, trench covers and equipment operating surfaces where slip resistance, corrosion resistance and moderate load-bearing capacity are required. In chemical, water treatment, electroplating and other environments with certain corrosive media, this specification can serve as one of the common options; for specific suitability, please contact us to confirm based on your actual working conditions.
Selection Guide
During selection, the resin system, grating thickness and mesh size can be matched to the corrosion level and load requirements of the service environment: the 25mm thick, 100mm mesh specification focuses on standard load and routine slip resistance. If special media, high temperature or higher load-bearing requirements are involved, we recommend providing working condition parameters, and we can assist in recommending a more suitable resin type and structural solution; please contact us for detailed specifications and quotations.
Product Advantages
This molded grating is integrally formed from unsaturated polyester resin and E-glass fiber in a custom mold, possessing the common characteristics of FRP materials such as light weight, high strength, corrosion resistance, slip resistance and insulation. The molding process enables continuous fibers to be distributed in both the longitudinal and transverse directions, giving good impact resistance and integrity, while also being easy to cut and install, helping to reduce subsequent maintenance workload.
Inquiry Guide
If you need to know the specifications and parameters, resin selection or supply information for FRP molded grating 25*100 H25 standard load type, please contact us for detailed specifications and quotations. We will provide targeted product recommendations and technical support based on your actual application scenarios.
Operating Environment
- This FRP molded grating is built on unsaturated polyester resin, so it is typically specified for industrial settings where continuous or intermittent contact with corrosive media such as acids, alkalis and salts would shorten the life of conventional metal gratings.
- The molded open-grid structure makes the grating suitable for both indoor plant areas and outdoor installations, including walkways, platforms and trench covers that are exposed to sunlight, rain and wash-down.
- Because the resin system can be selected from isophthalic, vinyl ester or bisphenol types, the grating is commonly used in chemical, wastewater and marine-adjacent environments where humidity and chemical splash are part of normal operation.
- Service temperature and chemical resistance vary with the chosen resin grade; contact us for the suitable resin type and the full parameter list for your specific operating conditions.
Custom Cutting
Need panels that fit, or cut to shape? We custom cut FRP grating and profiles to your drawing: panels cut to size or to shape (corner cuts, cutouts), cut edges sealed with resin, and pre-cut and pre-drilled to drawing before shipping. See the custom cutting services.
简体中文
English