Structural Profiles - Hook Plate (Vinyl Ester)

Structural Profiles - Hook Plate (Vinyl Ester)

Price on request

Request a Quote


Please feel freely to contact with us for new price .

Greenlogy TEC

    FRP pultruded profiles are made from fiberglass reinforcement as the raw material, resin as the binder, and fiberglass cloth as the wrapping reinforcement layer. After full impregnation, they are heated, formed and cured in a metal mold and pultruded under the traction of a pulling machine to produce a new type of composite material with good physical properties, widely used in high-strength and long-span applications.  

FRP hook plate structural profile VEFR-25 product photo

Type

Size (mm)

Weight (kg/m)

Size (in)

Weight (lbs/in)

Hook Plate

A*B*T


A*B*T



9*70*3.2 (beveled edge)0.48

1" x 1" x 1/8" (beveled edge)

1.06

25*60*30.5

1" x 19/8" x 1/8"

1.1

25*50*3(75°)0.45

1" x 2" x 1/8" (75°)

0.99

30*70*4(90°)0.75

19/16" x 11/4" x 3/16" (90°)

1.65

30*70*3.2(90°)0.7

19/16" x 11/4" x 1/8" (90°)

1.54

30*90*3(87°)0.72

19/16" x 7/2" x 1/8" (87°)

1.59

38*230*3.2(87°)1.65

3/2" x 9" x 1/8" (87°)

3.64

40*254*6.4(87°)3.55

25/16" x 10" x 1/4" (87°)

7.83

50*140*3.2(87°)1.19

2" x 11/2" x 1/8" (87°)

2.62

55*152*3.6(87°)1.55

9/4" x 6" x 1/8" (87°)

3.42

55*230*3.6(87°)2.14

9/4" x 9" x 1/8" (87°)

4.72

55*205*3.2(87°)1.62

9/4" x 8" x 1/8" (87°)

3.57

55*55*3.2(87°)0.8

9/4" x 9/4" x 1/8" (87°)

1.76

55*70*3.2(87°)0.9

9/4" x 11/4" x 1/8" (87°)

1.98

30*76*30.6

19/16" x 3" x 1/8"

1.32

30*76*40.8

19/16" x 3" x 3/16"

1.76

25*50*3.2(90°)0.45

1" x 2" x 1/8" (90°)

0.99

25*50*4(90°)0.51

1" x 2" x 3/16" (90°)

1.12

25*100*3.2(87°)0.75

1" x 4" x 1/8" (87°)

1.65
Rounded corner30*75*3.50.69

19/16" x 3" x 1/8"

1.52
Rounded corner30*100*3.20.8

19/16" x 4" x 1/8"

1.76
Right angle30*100*3.20.85

19/16" x 4" x 1/8"

1.87

30*152*3.21.2

19/16" x 6" x 1/8"

2.65
Rounded corner30*230*3.21.6

19/16" x 9" x 1/8"

3.53
Right angle30*230*3.21.7

19/16" x 9" x 1/8"

3.75

55*300*4(90°)2.8

9/4" x 12" x 3/16" (90°)

6.17

55*345*4(87°)3.25

9/4" x 27/2" x 3/16" (87°)

7.17

30*381*3.2(87°)2.7

19/16" x 15" x 1/8" (87°)

5.95

55*400*3.22.8

9/4" x 63/4" x 1/8"

6.17

Markets 

Applications and markets for FRP hook plate profiles

  • Construction

  • Bridges and highways

  • Chemical

  • Food and beverage

  • Manufacturing

  • Metals and mining

  • Microelectronics

  • Oil and gas

  • Pharmaceutical

  • Power

  • Pulp and paper

  • Leisure and entertainment

  • Telecommunications

  • Transportation

  • Water and wastewater treatment

Features:

  • Corrosion resistance

  • Low maintenance

  • Flame retardant

  • Low installation cost

  • Heavy metal safety

  • Long service life

  • Electrical and thermal insulation

  • High strength-to-weight ratio

Raw material introduction — resin types

Code

Resin type

Flame retardant performance

Recommended applications

VEFR-25

Vinyl ester type

Oxygen index 28 and above

Harsh acid, alkali and other corrosive environments

IFR-25

Isophthalic type

Oxygen index 28 and above

VEFR type, economical grade, good resistance to moderate acids, alkalis and solvents

OFR-25

Orthophthalic type

Oxygen index 28 and above

General acid and alkali environments

Applications: 

  Greenlogy TEC pultruded FRP structural profiles from Greenlogy TEC are widely used in various applications, combining corrosion resistance, high strength, dimensional stability and light weight, with thermal insulation and electrical insulation properties. Durable Greenlogy TEC profiles provide years of low-maintenance service in areas traditionally using steel, aluminum or wood components. Today, these profiles are often used in highly corrosive applications where stainless steel and other expensive components were previously required.   

Greenlogy TEC profiles

Mechanical properties

ASTM

Unit

Value

Unit

Value

Tensile stress, LW

D-638

psi

30000

kgf/m²

21092086

Tensile stress, CW

D-638

psi

7000

kgf/m²

4921487

Tensile modulus, LW

D-638

10^6psi

2.5

10^6kgf/m²

1758

Tensile modulus, CW

D-638

10^6psi

0.8

10^6kgf/m²

562

Compressive stress, LW

D-695

psi

30000

kgf/m²

21092086

Compressive stress, CW

D-695

psi

15000

kgf/m²

10546043

Compressive modulus, LW

D-695

10^6psi

2.5

10^6kgf/m²

1758

Compressive modulus, CW

D-695

10^6psi

1

10^6kgf/m²

703

Flexural stress, LW

D-790

psi

30000

kgf/m²

21092086

Flexural stress, CW

D-790

psi

10000

kgf/m²

7030695

Flexural modulus, LW

D-790

10^6psi

1.8

10^6kgf/m²

1266

Flexural modulus, CW

D-790

10^6psi

0.8

10^6kgf/m²

562

Modulus of elasticity

Full section

10^6psi

2.8

10^6kgf/m²

1969

Shear modulus

---

10^6psi

0.45

10^6kgf/m²

316

Short-beam shear

D-2344

psi

4500

kgf/m²

3163813

Punch shear

D-732

psi

10000

kgf/m²

7030695

Notched cantilever beam impact, LW

D-256

ft.-lbs./in.

25

kg/m

3.46

Notched cantilever beam impact, CW

D-256

ft.-lbs./in.

4

kg/m

0.55

   Excluding round rods and square rods

Physical properties

ASTM

Unit

Value

Barcol hardness

D-495

---

45

24-hour water absorption

D-570

% max

0.45

Density

D-792

lbs./in.³

0.062-0.07

Coefficient of thermal expansion, LW

D-696

10^-6in./in./℃

8

Flame retardant performance

ASTM

Unit

Value

Tunnel test*

E-84

Flame spread

Max. 25

Combustibility*

D-635

---

Non-combustible

Electrical properties

ASTM

Unit

Value

Arc resistance, LW

D-495

秒(s)

120

Dielectric strength, LW

D-149

kv./in.

35

Dielectric strength, PF

D-149

V/mil

200

Dielectric constant, PF

D-150

@60hz

5

LW = lengthwise, CW = crosswise, PF = perpendicular to laminate surface

*Applies to ISOFR and VEFR only


Applications

As an accessory for vinyl structural profiles, hook plates are commonly used in FRP grating, platforms, walkways and handrail systems where connections and fastening are required. Their shape facilitates close fitting to profile surfaces, making them suitable for use with FRP structures in corrosive environments or outdoor conditions. Please contact us to confirm suitability for your specific application.

Selection Guide

When selecting, match the A*B*T dimensions and weight parameters in the specification table above against the cross-section size, installation angle and load direction of the profile being connected. If you are unsure which model corresponds, please provide drawings or details of the service environment and we can help recommend a suitable specification.

Product Advantages

This hook plate is pultruded from fiberglass reinforcement and a resin system, offering the lightweight, corrosion-resistant and insulating properties typical of FRP profiles. The surface is treated with an added veil layer, making it suitable for long-term exposure to humid or chemical media. Compared with metal connectors, it helps reduce maintenance needs caused by rust.

Inquiry

For detailed specifications, material options or bulk supply solutions, please contact us for detailed specifications and a quotation. Please provide the required dimensions, quantity and service environment, and we will reply as soon as possible.

Operating Environment

  • Suitable for indoor and outdoor installation; hook plates are used to support or connect FRP structural profiles in walkway, platform and handrail systems.
  • The vinyl resin system and fiberglass reinforcement resist moisture, humidity and various corrosive industrial atmospheres, making the hook plate suitable for chemical, marine and wastewater treatment environments.
  • Because it contains no steel, the hook plate does not rust or corrode, so it maintains its mechanical properties in humid or salt-laden air without additional coating.
  • The service temperature range depends on the specific resin formulation and load conditions; for detailed temperature limits and chemical resistance data, please contact Greenlogy TEC with details of your application.