Structural Profiles - Floor Panels (Isophthalic)
Request a Quote
Please feel freely to contact with us for new price .
Genius FRP
FRP structural shapes profile is made of glass fiber reinforced material, resin as adhesive, glass fiber cloth as a package reinforcement layer, through the thorough penetration, in the metal mold heating, molding, curing, drawing in the traction machine pulled A new type of composite material, with good physical properties, widely used in high strength, large span Situation.

Varieties | Size(mm) | Weight(kg/m) | Size(in) | Weight(lbs/in) |
|---|---|---|---|---|
| FL-A | 508*7*50.8*8 | 19.7 | 20" x 1/4" x 2" x 5/16" | 43.4 |
| FL-B | 635*12*101.6*13 | 54.6 | 25" x 1/2" x 4" x 1/2" | 120 |
| FL-C | 498*4*50*4 | 9.4 | 20" x 3/16" x 2" x 3/16" | 20.7 |
| 50*20*4*4 | 0.7 | 2" x 13/16" x 3/16" x 3/16" | 1.54 | |
| 55*31*3*3 | 0.6 | 9/4" x 5/4" x 1/8" x 1/8" | 1.32 |
Markets

Architectural
Bridge & Highway
Chemical
Food & Beverage
Manufacturing
Metals & Mining
Microelectronics
Oil & Gsa
Pharmaceutical
Power
Pulp & Paper
Recreation
Telecommunications
Transportation
Water & Wastewater
The characteristics:
Corrosion Resistant
Low Maintenance
Fire Retardant
Low Install Cost
Heavy Metal Safe
Long Service Life
Electrically & Thermally Non Conductive
High Strength-to-Weight Ratio
Introduction of raw materials——Resin type
Code | Resin type | Flame retardant property | Recommended usage occasions |
|---|---|---|---|
VEFR-25 | Vinyl type | Oxygen index 28 or above | Acid, alkali and other corrosive harsh environment |
IFR-25 | Meta benzene | Oxygen index 28 or above | A VEFR type economy, and excellent, moderate acid alkali and solvent |
OFR-25 | Ortho type | Oxygen index 28 or above | General acid and alkali environment |
Application:
Genius© pultruded fiberglass structural shapes from Genius Composite Inc. are used in a wide range of applications and provide a unique combination of corrosion resistance, high strength, dimensional stability and light weight, along with thermal and electric non-conductivity. Durable Genius shapes provide years of low maintenance service in areas where steel, aluminum or wood components are traditionally specified. Today ,these shapes are often used in highly corrosive applications where stainless steel and other expensive components were once required.
Genius Shapes
Mechanical Properties | ASTM | Units | Value | Units | Value |
|---|---|---|---|---|---|
Tensile Stress, LW | D-638 | psi | 30000 | kgf/m² | 21092086 |
Tensile Stress, CW | D-638 | psi | 7000 | kgf/m² | 4921487 |
Tensile Modulus, LW | D-638 | 10^6psi | 2.5 | 10^6kgf/m² | 1758 |
Tensile Modulus, CW | D-638 | 10^6psi | 0.8 | 10^6kgf/m² | 562 |
Compressive Stress, LW | D-695 | psi | 30000 | kgf/m² | 21092086 |
Compressive Stress, CW | D-695 | psi | 15000 | kgf/m² | 10546043 |
Compressive Modulus, LW | D-695 | 10^6psi | 2.5 | 10^6kgf/m² | 1758 |
Compressive Modulus, CW | D-695 | 10^6psi | 1 | 10^6kgf/m² | 703 |
Flexural Stress, LW | D-790 | psi | 30000 | kgf/m² | 21092086 |
Flexural Stress, CW | D-790 | psi | 10000 | kgf/m² | 7030695 |
Flexural Modulus, LW | D-790 | 10^6psi | 1.8 | 10^6kgf/m² | 1266 |
Flexural Modulus, CW | D-790 | 10^6psi | 0.8 | 10^6kgf/m² | 562 |
Modulus of Elasticity | Full Section | 10^6psi | 2.8 | 10^6kgf/m² | 1969 |
Shear Modulus | --- | 10^6psi | 0.45 | 10^6kgf/m² | 316 |
Short Beam Shear | D-2344 | psi | 4500 | kgf/m² | 3163813 |
Punch Shear | D-732 | psi | 10000 | kgf/m² | 7030695 |
Notched Izod Impact,LW | D-256 | ft.-lbs./in. | 25 | kg/m | 3.46 |
Notched Izod Impact,CW | D-256 | ft.-lbs./in. | 4 | kg/m | 0.55 |
Excludes Round Rod and Square Bar
Physical Properties | ASTM | Units | Value |
|---|---|---|---|
Barcoal | D-495 | --- | 45 |
24 Hour Water Absorption | D-570 | %max | 0.45 |
Density | D-792 | lbs./in.³ | 0.062-0.07 |
Coefficient of Thermal Expansion,LW | D-696 | 10^-6in./in./℃ | 8 |
Flammability Properties | ASTM | Units | Value |
|---|---|---|---|
Tunnel test* | E-84 | Flame Spread | 25 max |
Flammability* | D-635 | --- | Non-Burning |
Electrical Properties | ASTM | Units | Value |
|---|---|---|---|
Arc Resistance,LW | D-495 | seconds | 120 |
Dielectric Strength,LW | D-149 | kv./in. | 35 |
Dielectric Strength,PF | D-149 | volts/mil | 200 |
Dielectric Constant,PF | D-150 | @60hz | 5 |
LW=Lengthwise, CW=Crosswise,PF=Perpendicular to Laminate Face
*Pertains to ISOFR and VEFR only
Application Scenarios
Isophthalic structural profile floor panels are suitable for industrial platforms, walkways, trench covers, and offshore facilities with high corrosion resistance requirements. Their lightweight, high-strength, and chemical-resistant properties make them widely used in chemical, marine, and wastewater treatment industries.
Selection Guide
Selection requires comprehensive consideration of load requirements, span, support spacing, and service environment. Profiles of different cross-sectional dimensions and thicknesses have varying load-bearing capacities. We recommend consulting our technical team based on actual engineering conditions to obtain suitable specification recommendations.
Product Advantages
The isophthalic resin system gives the floor panels excellent corrosion resistance and water resistance, while glass fiber reinforcement ensures high strength and stiffness. The products are lightweight for easy transportation and installation, and offer good insulation and aging resistance.
Inquiry Guide
For detailed specifications, technical parameters, or customized solutions, please contact us for professional support and quotations. We can provide selection advice and solutions based on your project requirements.
Operating Environment
- These isophthalic resin FRP floor profiles are pultruded glass fiber composites intended for both indoor plant flooring and outdoor walkways, platforms and stair treads, where the profile replaces steel grating in wet or humid service.
- The isophthalic resin matrix is chosen for resistance to mildly corrosive media - splash, salt-laden air and washdown conditions found in chemical, water treatment and marine-adjacent plants - rather than for concentrated acids or strong solvents.
- Because the pultruded profile carries no steel core, it is suited to areas where corrosion of conventional metal grating would demand frequent recoating; the surface is non-sparking and does not support rust staining of surrounding structures.
- Service temperature, chemical exposure and UV loading vary by installation; contact Greenlogy TEC with the actual service conditions so the appropriate resin grade, profile size from the FL-A / FL-B / FL-C range and fastening details can be confirmed.