Structural Profiles - Square Tube Custom Profiles (Orthophthalic)

Structural Profiles - Square Tube Custom Profiles (Orthophthalic)

Price on request

Request a Quote


Please feel freely to contact with us for new price .

Greenlogy TEC

  FRP pultruded profiles are made from glass fiber reinforcement, with resin as the binder and glass fiber cloth as the wrapping reinforcement layer. After thorough impregnation, they are heated, formed and cured in a metal mold and then pulled by a pulling machine to form a new type of composite material with good physical properties, widely used in high-strength and long-span applications.  

Square FRP tube profile made of phthalate-based composite material

Type

Size (mm)

Weight (kg/m)

Size (in)

Weight (lbs/in)

Square Tube Profiles

A*B*T1*T2


A*B*T1*T2


STH5050*50*6.4*53

2" x 2" x 1/4" x 3/16"

6.61

Markets

FRP square tube applications across various markets

  • Construction

  • Bridges and highways

  • Chemical

  • Food and beverage

  • Manufacturing

  • Metals and mining

  • Microelectronics

  • Oil and gas

  • Pharmaceutical

  • Power

  • Pulp and paper

  • Recreation

  • Telecommunications

  • Transportation

  • Water and wastewater treatment

Features:

  • Corrosion resistance

  • Low maintenance

  • Flame retardant

  • Low installation cost

  • Safe in heavy-metal environments

  • Long service life

  • Electrically and thermally non-conductive

  • High strength-to-weight ratio

Raw material introduction — resin types

Code

Resin type

Flame retardant performance

Recommended applications

VEFR-25

Vinyl ester type

Oxygen index 28 and above

Harsh corrosive environments such as acids and alkalis

IFR-25

Isophthalic type

Oxygen index 28 and above

An economical VEFR grade with good to moderate resistance to acids, alkalis and solvents

OFR-25

Orthophthalic type

Oxygen index 28 and above

General acid and alkali environments

Applications: 

    Greenlogy TEC pultruded FRP profiles are widely used in various applications, combining corrosion resistance, high strength, dimensional stability and light weight, with thermal insulation and electrical insulation properties. Durable Greenlogy TEC profiles provide years of low-maintenance service in areas where steel, aluminum or wood components are traditionally used. Today, these profiles are commonly used in highly corrosive applications that previously required stainless steel and other expensive components.   

Greenlogy TEC profiles

Mechanical properties

ASTM

Unit

Value

Unit

Value

Tensile stress, longitudinal

D-638

psi

30000

kgf/m²

21092086

Tensile stress, transverse

D-638

psi

7000

kgf/m²

4921487

Tensile modulus, longitudinal

D-638

10^6psi

2.5

10^6kgf/m²

1758

Tensile modulus, transverse

D-638

10^6psi

0.8

10^6kgf/m²

562

Compressive stress, longitudinal

D-695

psi

30000

kgf/m²

21092086

Compressive stress, transverse

D-695

psi

15000

kgf/m²

10546043

Compressive modulus, longitudinal

D-695

10^6psi

2.5

10^6kgf/m²

1758

Compressive modulus, transverse

D-695

10^6psi

1

10^6kgf/m²

703

Flexural stress, longitudinal

D-790

psi

30000

kgf/m²

21092086

Flexural stress, transverse

D-790

psi

10000

kgf/m²

7030695

Flexural modulus, longitudinal

D-790

10^6psi

1.8

10^6kgf/m²

1266

Flexural modulus, transverse

D-790

10^6psi

0.8

10^6kgf/m²

562

Modulus of elasticity

Full section

10^6psi

2.8

10^6kgf/m²

1969

Shear modulus

---

10^6psi

0.45

10^6kgf/m²

316

Short-beam shear

D-2344

psi

4500

kgf/m²

3163813

Punch shear

D-732

psi

10000

kgf/m²

7030695

Notched Izod impact strength, LW

D-256

ft.-lbs./in.

25

kg/m

3.46

Notched Izod impact strength, CW

D-256

ft.-lbs./in.

4

kg/m

0.55

  Excluding round rods and square rods   

Physical properties

ASTM

Unit

Value

Barcol hardness

D-495

---

45

24-hour water absorption

D-570

% maximum

0.45

Density

D-792

lbs./in.³

0.062-0.07

Coefficient of thermal expansion, LW

D-696

10^-6in./in./℃

8

Flammability

ASTM

Unit

Value

Tunnel test*

E-84

Flame spread

25 max

Flammability*

D-635

---

Non-burning

Electrical properties

ASTM

Unit

Value

Arc resistance, LW

D-495

秒(s)

120

Dielectric strength, LW

D-149

kv./in.

35

Dielectric strength, PF

D-149

Volts/mil

200

Dielectric constant, PF

D-150

@60hz

5

LW = lengthwise, CW = crosswise, PF = perpendicular to laminate surface

*Applies to ISOFR and VEFR only


Application Scenarios

Structural Profiles - Custom Square Tube Profiles (Orthophthalic Type) are suitable for load-bearing and support structures requiring corrosion resistance, light weight and high strength, such as platform walkways, handrails and cable trays, as well as corrosive environments in the chemical and water treatment industries. When selecting for a specific project, we recommend considering both load and environmental conditions. Please contact us for detailed specifications and a quotation.

Selection Guide

When selecting, please confirm the cross-section dimensions, wall thickness and length requirements of the square tube, and evaluate them together with the actual loads, span and installation method. For advice on fatigue or long-term performance, please contact our technical team for detailed specifications and a quotation.

Product Advantages

Orthophthalic resin gives the profiles good chemical corrosion resistance and water resistance, while glass fiber reinforcement provides relatively high specific strength and specific stiffness. They are also lightweight and easy to cut and install. Compared with traditional metal profiles, maintenance costs are lower. Please contact us for detailed specifications and a quotation.

Inquiry Guidance

If you need detailed technical parameters, dimension tables or commercial terms for Structural Profiles - Custom Square Tube Profiles (Orthophthalic Type), please contact us directly. We can provide selection support based on your project requirements. Please contact us for detailed specifications and a quotation.

Operating Environment

  • These FRP structural profiles are produced with orthophthalic resin and glass fiber reinforcement, and are suitable for indoor and outdoor installations where moisture and water vapor are present.
  • They resist corrosion from a variety of acids, alkalis and salts, and are commonly used in chemical plants, food and beverage facilities and water treatment areas where metal profiles would degrade.
  • Typical applications include building structures, bridge and highway components, and industrial platforms exposed to weather and temperature changes.
  • For detailed operating temperature ranges or specific chemical resistance data, please contact us for the complete parameter table.

Custom Cutting

Need panels that fit, or cut to shape? We custom cut FRP grating and profiles to your drawing: panels cut to size or to shape (corner cuts, cutouts), cut edges sealed with resin, and pre-cut and pre-drilled to drawing before shipping. See the custom cutting services.

WhatsApp