Structural Profiles - Flat Bar (Isophthalic Resin)

Structural Profiles - Flat Bar (Isophthalic Resin)

Price on request

Request a Quote


Please feel freely to contact with us for new price .

Genius FRP   

  FRP structural shapes profile is made of glass fiber reinforced material, resin as adhesive, glass fiber cloth as a package reinforcement layer, through the thorough penetration, in the metal mold heating, molding, curing, drawing in the traction machine pulled A new type of composite material, with good physical properties, widely used in high strength, large span Situation.  

Riglet

Varieties

Size(mm)

Weight(kg/m)

Size(in)

Weight(lbs/in)

Riglet

Width*Thickness


Width*Thickness


FS19

19*6.4

0.25

3/4" x 1/4"

0.55

FS30A

30*3

0.18

19/16" x 1/8"

0.4

FS30B

30*6.4

0.37

19/16" x 1/4"

0.82

FS35

35*8

0.54

11/8" x 5/16"

1.19

FS38

38*5

0.37

3/2" x 3/16"

0.82

FS40A

40*8

0.62

25/16" x 5/16"

1.37

FS40B

40*10

0.79

25/16" x 3/8"

1.74

FS46B

46*6.4

0.58

29/16" x 1/4"

1.28

FS50A

50*2

0.25

2" x 1/16"

0.55

FS50B

50*4

0.38

2" x 3/16"

0.84

FS50C

50*6

0.59

2" x 1/4"

1.3

FS50D

50*8

0.76

2" x 5/16"

1.68

FS50E

50*15

1.43

2" x 9/16"

3.15

FS60A

60*2

0.24

19/8" x 1/16"

0.53

FS60B

60*4

0.48

19/8" x 3/16"

1.06

FS64

64*4.8

0.6

5/2" x 3/16"

1.32

FS70

70*4

0.55

11/4" x 3/16"

1.21

FS76

76*9.5

1.42

3" x 3/8"

3.13

FS100A

100*10

1.95

4" x 3/8"

4.3

FS100B

100*25

4.85

4" x 1"

10.7

FS102A

102*3.2

0.63

4" x 1/8"

1.39

FS102B

102*5

0.97

4" x 3/16"

2.4

FS102C

102*6.4

1.3

4" x 1/4"

2.87

FS120

120*10

2.4

19/4" x 3/8"

5.29

FS152A

152*10

2.92

6" x 3/8"

6.44

FS152B

152*20

5.9

6" x 13/16"

13

FS190

190*15

5.42

15/2" x 9/16"

12

FS280

280*10

5.32

11" x 3/8"

11.7

FS300

300*24

14.4

12" x 15/16"

31.8

FS355

355*5

3.5

14" x 3/16"

7.72

FS555

555*5

5.4

22" x 3/16"

11.9

FS751

751*5

7.2

30" x 3/16"

15.9

Markets 

Markets

  • Architectural

  • Bridge & Highway

  • Chemical

  • Food & Beverage

  • Manufacturing

  • Metals & Mining

  • Microelectronics

  • Oil & Gsa

  • Pharmaceutical

  • Power

  • Pulp & Paper

  • Recreation

  • Telecommunications

  • Transportation

  • Water & Wastewater

The characteristics:

  • Corrosion Resistant

  • Low Maintenance

  • Fire Retardant

  • Low Install Cost

  • Heavy Metal Safe

  • Long Service Life

  • Electrically & Thermally Non Conductive

  • High Strength-to-Weight Ratio

Introduction of raw materials——Resin type

Code

Resin type

Flame retardant property

Recommended usage occasions

VEFR-25

Vinyl type

Oxygen index 28 or above

Acid, alkali and other corrosive harsh environment

IFR-25

Meta benzene

Oxygen index 28 or above

A VEFR type economy, and excellent, moderate acid alkali and solvent

OFR-25

Ortho type

Oxygen index 28 or above

General acid and alkali environment

  Application:  

   Genius© pultruded fiberglass structural shapes from Genius Composite Inc. are used in a wide range of applications and provide a unique combination of corrosion resistance, high strength, dimensional stability and light weight, along with thermal and electric non-conductivity. Durable Genius shapes provide years of low maintenance service in areas where steel, aluminum or wood components are traditionally specified. Today ,these shapes are often used in highly corrosive applications where stainless steel and other expensive components were once required.   

Genius Shapes

Mechanical Properties

ASTM

Units

Value

Units

Value

Tensile Stress, LW

D-638

psi

30000

kgf/m²

21092086

Tensile Stress, CW

D-638

psi

7000

kgf/m²

4921487

Tensile Modulus, LW

D-638

10^6psi

2.5

10^6kgf/m²

1758

Tensile Modulus, CW

D-638

10^6psi

0.8

10^6kgf/m²

562

Compressive Stress, LW

D-695

psi

30000

kgf/m²

21092086

Compressive Stress, CW

D-695

psi

15000

kgf/m²

10546043

Compressive Modulus, LW

D-695

10^6psi

2.5

10^6kgf/m²

1758

Compressive Modulus, CW

D-695

10^6psi

1

10^6kgf/m²

703

Flexural Stress, LW

D-790

psi

30000

kgf/m²

21092086

Flexural Stress, CW

D-790

psi

10000

kgf/m²

7030695

Flexural Modulus, LW

D-790

10^6psi

1.8

10^6kgf/m²

1266

Flexural Modulus, CW

D-790

10^6psi

0.8

10^6kgf/m²

562

Modulus of Elasticity

Full Section

10^6psi

2.8

10^6kgf/m²

1969

Shear Modulus

---

10^6psi

0.45

10^6kgf/m²

316

Short Beam Shear

D-2344

psi

4500

kgf/m²

3163813

Punch Shear

D-732

psi

10000

kgf/m²

7030695

Notched Izod Impact,LW

D-256

ft.-lbs./in.

25

kg/m

3.46

Notched Izod Impact,CW

D-256

ft.-lbs./in.

4

kg/m

0.55

  Excludes Round Rod and Square Bar

Physical Properties

ASTM

Units

Value

Barcoal

D-495

---

45

24 Hour Water Absorption

D-570

%max

0.45

Density

D-792

lbs./in.³

0.062-0.07

Coefficient of Thermal Expansion,LW

D-696

10^-6in./in./℃

8

Flammability Properties

ASTM

Units

Value

Tunnel test*

E-84

Flame Spread

25 max

Flammability*

D-635

---

Non-Burning

Electrical Properties

ASTM

Units

Value

Arc Resistance,LW

D-495

seconds

120

Dielectric Strength,LW

D-149

kv./in.

35

Dielectric Strength,PF

D-149

volts/mil

200

Dielectric Constant,PF

D-150

@60hz

5

LW=Lengthwise, CW=Crosswise,PF=Perpendicular to Laminate Face

*Pertains to ISOFR and VEFR only


Application Scenarios

The structural profile flat bar (isophthalic resin) is suitable for platforms, walkways, handrails, supports and various structural support locations requiring corrosion resistance and strength, and is commonly found in chemical, water treatment, power and marine engineering environments. The isophthalic resin system gives it relatively stable performance under humid and chemical media conditions. Please contact us for detailed specifications and a quotation.

Selection Guide

During selection, the required width, thickness and span of the flat bar can be checked against the dimensions and weight parameters in the table above, and the media type and load-bearing method of the service environment should be specified. If you have special requirements for cross-section, length or resin system, please contact us for detailed specifications and a quotation, and our technical staff will assist in confirming a suitable solution.

Product Advantages

This flat bar is made of glass fiber as reinforcement and resin as binder, formed by the pultrusion process. It features light weight, high strength, corrosion resistance, insulation and easy processing, and is suitable for replacing some traditional metal profiles. The isophthalic resin system helps improve durability in complex environments. Please contact us for detailed specifications and a quotation.

Inquiry Guide

For information on the size range, surface treatment, packaging method and supply arrangements of the structural profile flat bar (isophthalic resin), please contact us for detailed specifications and a quotation. Please provide the required specifications, quantity and service environment, and we will provide a corresponding solution and commercial terms accordingly.

Operating Environment

  • FRP structural shapes profile is suitable for both indoor and outdoor installations, including applications exposed to weather and UV radiation.
  • The glass fiber reinforced composite with resin matrix resists moisture and humid conditions, making it appropriate for coastal or high-humidity industrial settings.
  • This profile performs well in corrosive environments where acids, alkalis, or salts are present, such as chemical processing plants and wastewater treatment facilities.
  • It maintains stable physical properties across a wide temperature range, from cold outdoor conditions to elevated temperatures in process areas.

立即联系我们,我们将有专业人员为您服务。

7*24 professional team support. Within 24 Hours, our team will give you the feedback.

Send