FRP Grating Stair Treads: Dimensions, Grip and Fixing

Tread depth, riser, surface and fixing decide whether a grating stair works in service

FRP Grating Stair Treads: Dimensions, Grip and Fixing

Why use FRP grating for stair treads

FRP grating treads weigh about a quarter of steel grating, resist corrosion, do not conduct electricity and need no painting. In chemical plants, wastewater works, offshore platforms and coastal factories, steel treads need derusting and repainting every two or three years, while FRP treads avoid that maintenance bill.

Their modulus of elasticity is lower than steel, so deflection is greater at the same span. Tread support spacing and panel depth must be checked against the product load table instead of copying steel grating practice.

A stair is walked on many times a day, and slip resistance, fixing and dimensional comfort cause more trouble than load capacity. The sections below take dimensions, surfaces, fixing, renovation and acceptance in turn.

Tread dimensions: depth, width and riser

Industrial stairs commonly use a tread depth of 240 to 300 mm and a riser height of 150 to 200 mm. Within one stair, every tread should have the same depth and height; large variations noticeably increase the risk of tripping.

Tread width follows the traffic: 600 mm for a single-person access stair, 800 to 900 mm for a normal walkway, and wider stairs need intermediate support. The grating tread should cover the clear distance between stringers and leave fixing allowance at both edges.

The final dimensions follow the project's building code and equipment requirements; the ranges here are common industrial practice, not code text. Renovation projects in particular should be measured before anything is ordered.

Open or closed risers

An open riser, with no riser plate, drains and clears debris well and keeps weight down, but small objects can fall between treads, so it is unsuitable where people or equipment pass underneath.

A closed riser adds a plate at the rear of each tread, which stops falling objects and reduces visual clutter below the stair. The plate can be FRP sheet or grating with an edge board, and its fixings should be independent of the tread panel.

Where liquids and dust are present, open risers are easier to keep clean; where dropped tools are a risk, closed risers are safer. The two approaches can be mixed by floor or area rather than applied to the whole stair.

Slip-resistant surfaces: gritted, sanded and nosing

Molded grating treads usually come with a gritted or sanded surface. Gritted gives good grip in wet and oily conditions with moderate cleaning effort; sanded gives the best slip resistance for outdoor, wash-down and oily workshops, but the rough surface holds dust.

The front edge of a tread is where slips start, so a nosing strip or edge binding should be added there. The binding also protects the cut edge of the grating, keeping glass fibres covered and reducing edge wear.

Slip performance should be compared on test data, not on how coarse the surface looks. Test methods are explained in FRP grating slip testing, and the full surface comparison is in FRP grating slip resistance; read the two together.

Connecting the tread to the stringers

Grating treads are normally fixed to the stringers with stainless bolts, with at least two fixing points at each end. Removable access treads can use M-clips, but clips are not suitable for impact loads.

Bolt holes become stress concentrations, so they should avoid the grating ribs, and the hole should be one to two millimetres larger than the bolt to allow for thermal movement. Use large washers so the bolt does not crush the grating surface.

Fixing selection is covered in FRP grating fixings, and installation should follow the manufacturer's torque, not the torque used for steel grating.

Renovating an old steel stair

There are two common approaches: remove the original treads and fit FRP grating treads, or cover the existing steel treads with FRP tread covers. The first is thorough and cures the corrosion; the second is quick and leaves the stringers untouched, but it raises the tread height.

A cover installation must account for the added height against the riser and headroom. After covering, add a nosing strip at the front edge, keep the edges tight against the original tread, and avoid pockets that hold water.

Before renovation, measure the stringer spacing, tread height and width, and the original connections, then order to the measured sizes. The tread span is the clear distance between stringers; deflection control is covered in FRP grating support spans, so measure before selecting.

Checking capacity and deflection

Stair treads are designed for a concentrated load, commonly 3 to 5 kN for industrial stairs, following the project code. The check places the concentrated load at mid-span, the worst position.

Deflection usually controls before strength does. Stair treads often use L/300 or a stricter limit; excessive deflection makes the stair feel soft underfoot and loosens the fixings faster.

Manufacturer load tables are usually written for uniform load, so a tread application needs a conversion or the concentrated-load column. How to read the table is covered in FRP grating load tables, and platform values should not be copied directly.

Joining up with handrails and guardrails

Handrails and guardrails on an FRP stair should be designed together with the treads. Post fixings should land on the stringers or on independent supports, never on the grating tread alone.

Handrail height, post spacing and railing loads follow the project code. The FRP handrail range is shown in FRP guardrail and handrail products, and using the same material as the treads avoids galvanic corrosion.

Use one material family for tread and railing fixings; mixing stainless and galvanized parts invites rust. Fasteners can also pit in chloride environments, so coastal projects should inspect them regularly.

Cutting, drilling and edge sealing on site

Cut grating treads with a fine-tooth or diamond blade, and wear a dust mask while cutting. Seal the cut face with resin edge sealant so moisture cannot travel along the fibres.

Drilled holes need the same sealing, and washers should spread the pressure around the hole. The process is described in FRP grating field fabrication; do not cut with an angle grinder at random.

Check the cut tread against the site. On renovation work the stringers are often not parallel, so measure each end separately instead of cutting to an average.

Acceptance and maintenance checklist

Five things to check at acceptance: tread depth and height are consistent, all fixing bolts are present and torqued to specification, the slip surface is intact, edge sealing is complete, and there is a thermal expansion gap between the tread and the railing.

In service, check quarterly for loose fixings, worn slip surfaces and cracks or split ribs in the tread. Chemical and coastal sites should shorten the interval.

FRP treads need no painting, but surface contamination reduces slip resistance, so wash-down water should drain freely. Replace corroded fixings promptly instead of waiting for them to work loose.