Pultruded FRP grating is made of pultruded "I", "T" shaped profile as a bearing strip, with a solid pipe or bar as a connecting rod, made by a certain assembly process with a gap of the plate.
Name | Contect | Type |
|---|---|---|
Resin | 25% | OFR-25,IFR-25,VEFR-25 |
Fiberglass | 65% | E |
Filler | 8% | ATH,PR |
Others | 2% | --- |
Code | Resin type | Flame retardant property | Recommended usage occasions |
|---|---|---|---|
MP-5 | Phenolic type | Oxygen index can reach about 80 | Low toxicity and high flame retardant, fire safety is very important for the occasion |
VEFR-25 | Vinyl type | Oxygen index 28 or above | Acid, alkali and other corrosive harsh environment |
VEFR-10 | Vinyl type | Oxygen index 35 or above | Flame retardant requirements of high acid, alkali and good occasions |
IFR-25 | Meta benzene | Oxygen index 28 or above | A VEFR type economy, and excellent, moderate acid alkali and solvent |
IFGR-30 | Benzene food grade | Oxygen index 26 | Mainly used in meat products and food processing plants |
OFR-25 | Ortho type | Oxygen index 28 or above | General acid and alkali environment |
OCR | Ortho type | Oxygen index below 28 | OFR-25 economy, no flame retardant requirements |
The type selection of coarse glass fiber
Code | Coarse sand type | Recommended usage occasions |
E | Non alkali sand | For high strength requirements and high corrosion resistance of the occasion |
Selected filler type
Code | Filler type | Recommended usage occasions |
|---|---|---|
ATH | Aluminum hydroxide | Retardant, smoke suppression, corrosion-resistant occasions |
PR | No filler, pure resin | For high corrosion-resistant applications |




Standard Panel Size:
1220mm,915mm-wide 3050mm,6100mm-length
Bearing Bar: 25mm
Open Area: 25%
Approx Weight (With three-core shoots): 13.6kg/m²

Liner load(units:mm)
Spacing | kg/m | kg/m | kg/m | kg/m | kg/m | kg/m | Limit |
|---|---|---|---|---|---|---|---|
(mm) | 150 | 300 | 450 | 750 | 1500 | 3000 | Load |
| 450 | 0.25 | 0.51 | 0.76 | 1.27 | 2.79 | 5.59 | 4619 |
| 600 | 0.51 | 1.02 | 1.78 | 2.79 | 5.59 | 11.4 | 3472 |
| 900 | 1.78 | 3.56 | 5.59 | 9.14 | --- | --- | 2310 |
| 1200 | 2.03 | 4.32 | 8.38 | 12.7 | --- | --- | 1728 |

Uniform load(units:mm)
Spacing | kg/m² | kg/m² | kg/m² | kg/m² | kg/m² | kg/m² | Limit |
|---|---|---|---|---|---|---|---|
(mm) | 450 | 950 | 1450 | 2400 | 4850 | 9500 | Load |
| 450 | 0.25 | 0.51 | 0.76 | 1.27 | 2.54 | 5.08 | 10638 |
| 600 | 0.76 | 1.52 | 2.03 | 3.56 | 7.11 | --- | 8003 |
| 900 | 3.56 | 6.86 | 10.4 | --- | --- | --- | 5075 |
| 1200 | 10.7 | --- | --- | --- | --- | --- | 2830 |
The characteristics:
Fire Retardant
High Flame Resistance
Low Smoke and Toxic Fume Emissions
High Strength-to-Weight Ratio
Corrosion Resistant
Low Maintenance
Slip Resistant
Electrically & Thermally Non-Conductive
Easily Fabricated
Impact Resistant
UV resistance
Maintenance free
Installation and accessories

Application Scenarios
Pultruded Grating T-2510 is commonly used in platforms, walkways, trench covers and equipment operating surfaces that require both load-bearing capacity and corrosion resistance, and is particularly suitable for humid, acid-alkali or weight-reduction industrial environments. For suitability under specific working conditions, we recommend confirming with us based on load, span and media conditions.
Selection Guide
When selecting, key considerations include load-bearing direction, support span, service environment and flame-retardant requirements, and the corresponding corrosion resistance and fire protection grade should be chosen according to the resin system (such as orthophthalic, isophthalic, vinyl ester or phenolic type). You are welcome to contact us with working condition parameters, and our technical staff will assist in specification matching and selection recommendations.
Product Advantages
Assembled with pultruded "I" and "T" profiles as load-bearing bars and solid tubes or rods as connecting rods, it features light weight, high strength, corrosion resistance, easy cutting and installation, and low maintenance costs, and the surface can be treated for anti-slip. Compared with traditional metal grating, it has a longer service life in corrosive environments and is non-conductive and non-magnetic.
Inquiry Guide
To obtain detailed specifications, resin system options, load-bearing data and quotations for T-2510, you are welcome to contact us. We will provide targeted solutions and commercial terms according to your project requirements.
Operating Environment
- Pultruded FRP grating T-2510 is built for both indoor and outdoor service, where the pultruded I- and T-shaped bearing bars and solid pipe or bar connecting rods resist weather exposure without the corrosion problems of steel.
- It is suited to humid and wet areas, including wash-down zones and locations with frequent condensation, because the FRP profile does not rust or deteriorate under moisture.
- The grating performs in chemically aggressive settings where acids, alkalis and salts are present, making it a candidate for chemical processing, wastewater treatment and coastal installations.
- For very high temperatures or fire-safety-critical areas, specify the appropriate resin system: the phenolic MP-5 grade offers high flame retardant properties with an oxygen index of about 80 for low-toxicity, high-fire-safety environments, while vinyl ester VEFR-25 provides flame retardancy with an oxygen index of 28 or above.