Pultruded Grating T-2510

Pultruded Grating T-2510

Price on request

Request a Quote


Please feel freely to contact with us for new price .

Genius FRP  

  Pultruded FRP grating is made of pultruded "I", "T" shaped profile as a bearing strip, with a solid pipe or bar as a connecting rod, made by a certain assembly process with a gap of the plate.  

Name

Contect

Type

Resin

25%

OFR-25,IFR-25,VEFR-25

Fiberglass

65%

E

Filler

8%

ATH,PR

Others

2%

---

Introduction of raw materials 
Resin type

Code

Resin type

Flame retardant property

Recommended usage occasions

MP-5

Phenolic type

Oxygen index can reach about 80

Low toxicity and high flame retardant, fire safety is very important for the occasion

VEFR-25

Vinyl type

Oxygen index 28 or above

Acid, alkali and other corrosive harsh environment

VEFR-10

Vinyl type

Oxygen index 35 or above

Flame retardant requirements of high acid, alkali and good occasions

IFR-25

Meta benzene

Oxygen index 28 or above

A VEFR type economy, and excellent, moderate acid alkali and solvent

IFGR-30

Benzene food grade

Oxygen index 26

Mainly used in meat products and food processing plants

OFR-25

Ortho type

Oxygen index 28 or above

General acid and alkali environment

OCR

Ortho type

Oxygen index below 28

OFR-25 economy, no flame retardant requirements

The type selection of coarse glass fiber   

Code

Coarse sand type

Recommended usage occasions

E

Non alkali sand

For high strength requirements and high corrosion resistance of the occasion

Selected filler type  

Code

Filler type

Recommended usage occasions

ATH

Aluminum hydroxide

Retardant, smoke suppression, corrosion-resistant occasions

PR

No filler, pure resin

For high corrosion-resistant applications

Software - Sample 1 for three columns

Sand surface
Software - Sample 2 for three columns

Smooth surface
Software - Sample 3 for three columns

Antiskid groove surface

T2510

Standard Panel Size:
1220mm,915mm-wide  3050mm,6100mm-length
Bearing Bar: 25mm
Open Area: 25%

Approx Weight (With three-core shoots): 13.6kg/m²
Liner load

Liner load(units:mm)

Spacing

kg/m

kg/m

kg/m

kg/m

kg/m

kg/m

Limit

(mm)

15030045075015003000

Load

4500.250.510.761.272.795.594619
6000.511.021.782.795.5911.43472
9001.783.565.599.14------2310
12002.034.328.3812.7------1728
Uniform load

Uniform load(units:mm)

Spacing

kg/m²

kg/m²

kg/m²

kg/m²

kg/m²

kg/m²

Limit

(mm)

4509501450240048509500

Load

4500.250.510.761.272.545.0810638
6000.761.522.033.567.11---8003
9003.566.8610.4---------5075
120010.7---------------2830

The characteristics:

  • Fire Retardant

  • High Flame Resistance

  • Low Smoke and Toxic Fume Emissions

  • High Strength-to-Weight Ratio

  • Corrosion Resistant

  • Low Maintenance

  • Slip Resistant

  • Electrically & Thermally Non-Conductive

  • Easily Fabricated

  • Impact Resistant 

  • UV resistance

  • Maintenance free

Installation and accessories  

Installation and accessories

Application Scenarios

Pultruded Grating T-2510 is commonly used in platforms, walkways, trench covers and equipment operating surfaces that require both load-bearing capacity and corrosion resistance, and is particularly suitable for humid, acid-alkali or weight-reduction industrial environments. For suitability under specific working conditions, we recommend confirming with us based on load, span and media conditions.

Selection Guide

When selecting, key considerations include load-bearing direction, support span, service environment and flame-retardant requirements, and the corresponding corrosion resistance and fire protection grade should be chosen according to the resin system (such as orthophthalic, isophthalic, vinyl ester or phenolic type). You are welcome to contact us with working condition parameters, and our technical staff will assist in specification matching and selection recommendations.

Product Advantages

Assembled with pultruded "I" and "T" profiles as load-bearing bars and solid tubes or rods as connecting rods, it features light weight, high strength, corrosion resistance, easy cutting and installation, and low maintenance costs, and the surface can be treated for anti-slip. Compared with traditional metal grating, it has a longer service life in corrosive environments and is non-conductive and non-magnetic.

Inquiry Guide

To obtain detailed specifications, resin system options, load-bearing data and quotations for T-2510, you are welcome to contact us. We will provide targeted solutions and commercial terms according to your project requirements.

Operating Environment

  • Pultruded FRP grating T-2510 is built for both indoor and outdoor service, where the pultruded I- and T-shaped bearing bars and solid pipe or bar connecting rods resist weather exposure without the corrosion problems of steel.
  • It is suited to humid and wet areas, including wash-down zones and locations with frequent condensation, because the FRP profile does not rust or deteriorate under moisture.
  • The grating performs in chemically aggressive settings where acids, alkalis and salts are present, making it a candidate for chemical processing, wastewater treatment and coastal installations.
  • For very high temperatures or fire-safety-critical areas, specify the appropriate resin system: the phenolic MP-5 grade offers high flame retardant properties with an oxygen index of about 80 for low-toxicity, high-fire-safety environments, while vinyl ester VEFR-25 provides flame retardancy with an oxygen index of 28 or above.