拉挤格栅 I-6020

拉挤格栅 I-6020

¥ 1.00 1.0 CNY

¥ 1.00

加入购物车


欢迎询价。

Genius FRP  

  Pultruded FRP grating is made of pultruded "I", "T" shaped profile as a bearing strip, with a solid pipe or bar as a connecting rod, made by a certain assembly process with a gap of the plate.  

Name

Contect

Type

Resin

25%

OFR-25、IFR-25、VEFR-25

Fiberglass

65%

E

Filler

8%

ATH、PR

Others

2%

---

Introduction of raw materials 
Resin type

Code

Resin type

Flame retardant property

Recommended usage occasions

MP-5

Phenolic type

Oxygen index can reach about 80

Low toxicity and high flame retardant, fire safety is very important for the occasion

VEFR-25

Vinyl type

Oxygen index 28 or above

Acid, alkali and other corrosive harsh environment

VEFR-10

Vinyl type

Oxygen index 35 or above

Flame retardant requirements of high acid, alkali and good occasions

IFR-25

Meta benzene

Oxygen index 28 or above

A VEFR type economy, and excellent, moderate acid alkali and solvent

IFGR-30

Benzene food grade

Oxygen index 26

Mainly used in meat products and food processing plants

OFR-25

Ortho type

Oxygen index 28 or above

General acid and alkali environment

OCR

Ortho type

Oxygen index below 28

OFR-25 economy, no flame retardant requirements

The type selection of coarse glass fiber  

Code

Coarse sand type

Recommended usage occasions

E

Non alkali sand

For high strength requirements and high corrosion resistance of the occasion

Selected filler type  

Code

Filler type

Recommended usage occasions

ATH

Aluminum hydroxide

Retardant, smoke suppression, corrosion-resistant occasions

PR

No filler, pure resin

For high corrosion-resistant applications

Software - Sample 1 for three columns

Sand surface
Software - Sample 2 for three columns

Smooth surface
Software - Sample 3 for three columns

Antiskid groove surface

I 6020

Standard Panel Size:
1220mm,915mm-wide  3050mm,6100mm-length
Bearing Bar: 50mm
Open Area: 60%

Approx Weight (With three-core shoots): 20.1kg/m²
Liner load

Liner load(units:mm)

Spacing

kg/m

kg/m

kg/m

kg/m

kg/m

kg/m

kg/m

(mm)

30075010001500200025003000
4500.090.230.30.460.610.760.92
6000.210.540.721.091.451.822.18
9000.731.842.463.694.926.157.38
12001.754.375.838.7511.714.5---
Uniform load

Uniform load(units:mm)

Spacing

kg/m²

kg/m²

kg/m²

kg/m²

kg/m²

kg/m²

kg/m²

(mm)

1000200030004000500070008000
4500.190.380.570.760.961.341.53
6000.450.911.361.822.273.193.64
9001.533.074.616.157.6910.712.4
12003.647.291114.6---------

The characteristics:

  • Fire Retardant

  • High Flame Resistance

  • Low Smoke and Toxic Fume Emissions

  • High Strength-to-Weight Ratio

  • Corrosion Resistant

  • Low Maintenance

  • Slip Resistant

  • Electrically & Thermally Non-Conductive

  • Easily Fabricated

  • Impact Resistant 

  • UV resistance

  • Maintenance free

Installation and accessories  

Installation and accessories

应用场景

拉挤格栅 I-6020 常用于对承载、耐腐蚀和通风格栅有要求的工业平台、走道、地沟盖板及化工、污水处理、海洋工程等环境。具体场景下的承载力、跨距与安装方式需结合工况确认,欢迎联系我们沟通选型。

选型指导

选型时可重点关注树脂体系、格栅高度、承载条间距与连接杆形式,以匹配耐腐蚀等级、防火要求及荷载条件。我们可根据您的使用环境与安装尺寸提供建议方案,欢迎联系我们获取详细规格与报价。

产品优势

采用拉挤 I 型承载条与连接杆组装,具有轻质高强、耐腐蚀、不导电、易切割安装等特点,适合替代部分金属格栅。不同树脂类型在阻燃与耐化学性上各有侧重,可按需选择。

询盘引导

如需了解拉挤格栅 I-6020 的规格参数、供货周期与商务条款,请提供使用环境、尺寸及数量等信息,欢迎联系我们获取详细规格与报价。