拉挤格栅 I-6010
欢迎询价。
Genius FRP
Pultruded FRP grating is made of pultruded "I", "T" shaped profile as a bearing strip, with a solid pipe or bar as a connecting rod, made by a certain assembly process with a gap of the plate.
Name | Contect | Type |
Resin |
25% | OFR-25、IFR-25、VEFR-25 |
Fiberglass |
65% | E |
Filler | 8%
| ATH、PR |
Others |
2% | --- |
Code | Resin type | Flame retardant property | Recommended usage occasions |
MP-5 | Phenolic type | Oxygen index can reach about 80 | Low toxicity and high flame retardant, fire safety is very important for the occasion |
VEFR-25 | Vinyl type | Oxygen index 28 or above | Acid, alkali and other corrosive harsh environment |
VEFR-10 | Vinyl type | Oxygen index 35 or above | Flame retardant requirements of high acid, alkali and good occasions |
IFR-25 | Meta benzene | Oxygen index 28 or above | A VEFR type economy, and excellent, moderate acid alkali and solvent |
IFGR-30 | Benzene food grade | Oxygen index 26 | Mainly used in meat products and food processing plants |
OFR-25 | Ortho type | Oxygen index 28 or above | General acid and alkali environment |
OCR | Ortho type | Oxygen index below 28 | OFR-25 economy, no flame retardant requirements |
The type selection of coarse glass fiber
Code | Coarse sand type | Recommended usage occasions |
E | Non alkali sand | For high strength requirements and high corrosion resistance of the occasion |
Selected filler type
Code | Filler type | Recommended usage occasions |
ATH | Aluminum hydroxide | Retardant, smoke suppression, corrosion-resistant occasions |
PR | No filler, pure resin | For high corrosion-resistant applications |

Sand surface

Smooth surface

Antiskid groove surface

Standard Panel Size:
1220mm,915mm-wide 3050mm,6100mm-length
Bearing Bar: 25mm
Open Area: 60%
Approx Weight (With three-core shoots): 12.2kg/m²

Liner load(units:mm)
Spacing | kg/m | kg/m | kg/m | kg/m | kg/m | kg/m | Limit |
(mm) | 300 | 450 | 750 | 1500 | 3000 | 5950 | Load |
| 450 | 0.59 | 0.89 | 1.52 | 2.94 | 5.83 | 11 | 11067 |
| 600 | 1.41 | 2.12 | 3.52 | 5.59 | 14.2 | 27.6 | 8639 |
| 900 | 4.75 | 7.13 | 11.9 | 23.7 | --- | --- | 5750 |
| 1200 | 11.2 | 16.9 | 28.2 | --- | --- | --- | 4275 |

Uniform load(units:mm)
Spacing | kg/m² | kg/m² | kg/m² | kg/m² | kg/m² | kg/m² | Limit |
(mm) | 1000 | 1900 | 4000 | 7000 | 9500 | 19500 | Load |
| 450 | 1.23 | 2.36 | 4.95 | 8.67 | 11.9 | 22.2 | 48380 |
| 600 | 2.93 | 5.35 | 11.7 | --- | --- | --- | 28344 |
| 900 | 9.91 | 19.52 | --- | --- | --- | --- | 12559 |
| 1200 | 23.5 | --- | --- | --- | --- | --- | 6988 |
The characteristics:
Fire Retardant
High Flame Resistance
Low Smoke and Toxic Fume Emissions
High Strength-to-Weight Ratio
Corrosion Resistant
Low Maintenance
Slip Resistant
Electrically & Thermally Non-Conductive
Easily Fabricated
Impact Resistant
UV resistance
Maintenance free
Installation and accessories

应用场景
拉挤格栅 I-6010 适用于对承重与耐腐蚀同时有要求的平台、走道、地沟盖板及各类工业操作面。其以拉挤“I”型材作承力条、实心管或棒作连接杆的结构,便于在潮湿、化学介质或户外环境中保持稳定。具体场景适配与安装方式,欢迎联系我们结合工况确认。
选型指导
选型时请先明确使用环境的腐蚀介质与防火要求,再据此选择树脂体系,例如酚醛型适用于低毒高阻燃、防火安全要求高的场合,乙烯基型适用于一般耐腐蚀工况。同时需考虑格栅的承载方向、支撑跨距与安装固定方式。我们可协助您完成选型,欢迎提供工况参数获取建议。
产品优势
拉挤格栅 I-6010 采用玻璃纤维与树脂体系,按型材组装工艺成型,兼具轻质高强、耐腐蚀与便于切割安装的特点。表面可根据使用需求进行防滑处理,连接杆与承力条的组合结构有助于分散载荷。相比传统金属格栅,在耐化学腐蚀与绝缘方面具有优势。
询盘引导
如需获取拉挤格栅 I-6010 的详细规格、树脂类型选择、承载数据及商务条款,欢迎联系我们的销售团队。请提供您的应用环境、尺寸需求与数量,我们将为您提供针对性方案与报价。
简体中文